Chemical and Molecular Variations in Commercial Epoxide Photoresists for X-ray Lithography
Source abstract
Abstract
The quality of high aspect ratio microstructures fabricated by deep X-ray lithography is highly dependent on the photoresist material used and the process parameters applied. Even with photoresists more suitable to this process, it is common to face defects in the final optical components, such as in case of X-ray gratings. The gratings need to be fabricated with critical dimensions on a sub-micrometer and micrometer scale, with periods of few micrometers and heights of hundreds of micrometers to be used in X-ray imaging techniques such as Talbot–Lau Interferometry. During the fabrication process, these features lead to challenges such as mechanical stability, homogeneity, and defect-free grating patterns. Usually, an epoxy-based negative photoresist is used in X-ray lithography, which needs to account for the shrinkage that takes place during polymer crosslinking in order to avoid defects in the final pattern. Nowadays, photoresist material still lacks certain suitable properties (chemical and mechanical) to fabricate gratings of high quality and with acceptable reproducibility. This work presents the results of TGA, FTIR, and MALDI-TOF analysis made on photoresists commercially available and suitable for X-ray lithography. The photoresists presented different profiles regarding the solvent content and oligomers composition, and in the case of some samples, there were high amounts of non-epoxidized oligomers.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Photolithography Techniques · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Karlsruhe Institute of Technology (KIT), Institute of Microstructure Technology, Hermann-von-Helmholtz-Platz 1, 76344 Eggenstein-Leopoldshafen, Germany
Chemistry Department, Federal University of Paraná, Rua Coronel Francisco Heráclito dos Santos, 100, Jardim das Américas, 81531-980 Curitiba, PR, Brazil
References (44)
Show source-provided references
1. Characterization method for new resist formulations for HAR patterns made by X-ray lithography10.1007/s00542-013-2055-x ↗
2. A comparative study of different thick photoresists for MEMS applications10.1007/s10854-005-4977-2 ↗
3. Key issues in fabricating microstructures with high aspect ratios by using deep X-ray lithography10.1016/j.mee.2004.02.004 ↗
4. Characterizing and smoothing of striated sidewall morphology on UV-exposed thick SU-8 structures for micromachining millimeter wave circuits10.1088/0960-1317/20/3/035007 ↗
5. Fabrication and investigation of in-plane compliant SU8 structures for MEMS and their application to micro valves and micro grippers10.1016/S0924-4247(01)00829-9 ↗
6. Freeze-Drying Process to Avoid Resist Pattern Collapse10.1143/JJAP.32.5813 ↗
7. Influences of pretreatment and hard baking on the mechanical reliability of SU-8 microstructures10.1088/0960-1317/23/10/105016 ↗
8. Lithographically fabricated SU8 composite structures for wettability control10.1016/j.surfcoat.2013.12.038 ↗
9. Mechanism of Resist Pattern Collapse during Development Process10.1143/JJAP.32.6059 ↗
10. SU8 resist for low-cost X-ray patterning of high-resolution, high-aspect-ratio MEMS10.1016/S0026-2692(01)00109-4 ↗
11. Supercritical Drying for Nanostructure Fabrication10.2494/photopolymer.15.381 ↗
12. Supercritical resist dryer10.1116/1.591276 ↗
13. (2017, September 17). Micro-chem–SU-8 3000–Data Sheet. Available online: http://microchem.com/pdf/SU-8%203000%20Data%20Sheet.pdf.
14. Suspension of nanoparticles in SU-8: Processing and characterization of nanocomposite polymers10.1016/j.mejo.2007.05.012 ↗
15. SU-8 nanocomposite coatings with improved tribological performance for MEMS10.1016/j.surfcoat.2006.03.041 ↗
16. A new SU-8 process to integrate buried waveguides and sealed microchannels for a Lab-on-a-Chip10.1016/j.snb.2005.05.011 ↗
17. Application of SU8 polymer in waveguide interferometer ammonia sensor
18. Bimodal Layers of the Polymer SU8 as Refractometer10.1016/j.proeng.2012.09.149 ↗
19. SU-8 MEMS Fabry-Perot pressure sensor10.1016/j.sna.2007.04.047 ↗
20. Advanced photoresist technologies for microsystems10.1088/0960-1317/11/4/312 ↗
21. Gelorme, J.D., Cox, R.J., and Gutierrez, S.A. (1989). Photoresist Composition and Printed Circuit Boards and Packages Made Therewith. (4,882,245), U.S. Patent.
22. Polymeric optical waveguides using direct ultraviolet photolithography process10.1007/s00339-003-2248-8 ↗
23. Triarylsulfonium salts as photoinitiators of free radical and cationic polymerization10.1002/pol.1979.130171203 ↗
24. Radiation curing of epoxies
25. Cationic electron-beam curing of a high-functionality epoxy: Effect of post-curing on glass transition and conversion10.1002/pi.1383 ↗
26. Polymerization optimization of SU-8 photoresist and its applications in microfluidic systems and MEMS10.1088/0960-1317/11/1/304 ↗
27. Characterization of the polymerization of SU-8 photoresist and its applications in micro-electro-mechanical systems (MEMS)10.1016/S0142-9418(01)00005-8 ↗
28. Effect of filler behavior on nanocomposite SU8 photoresist for moving micro-parts10.1016/j.mee.2006.01.068 ↗
29. Yeh, W.-M. (2013). Pattern Collapse in Lithographic Nanostructures: Quantifying Photoresist Nanostructure Behavior and Novel Methods for Collapse Mitigation. [Ph.D. Dissertation, Georgia Institute of Technology].
30. Photolithographic fabrication of arbitrarily shaped SU-8 microparticles without sacrificial release layers10.1088/0960-1317/21/2/027003 ↗
31. Relationship between aspect ratio and narrowing of reflowed photoresist structures10.7567/JJAP.54.06FM01 ↗
32. A simulation model on photoresist SU-8 thickness after development under partial exposure with reflection effect10.7567/JJAP.53.036505 ↗
33. Synthesis of a cross-linked triazine phosphine polymer and its effect on fire retardancy, thermal degradation and moisture resistance of epoxy resins10.1016/j.polymdegradstab.2015.04.027 ↗
34. Fabrication of porous material for micro component application by direct X-ray lithography and sintering10.1016/j.mee.2012.05.016 ↗
35. Matrix-Assisted Laser Desorption Ionization Mass Spectrometry of Synthetic Polymers10.1002/masy.201250317 ↗
36. MALDI−TOF Investigation of Polymer Degradation. Pyrolysis of Poly(bisphenol A carbonate)10.1021/ma9912148 ↗
37. Mass spectrometry of synthetic polymers by UV-matrix-assisted laser desorption/ionization10.1021/ac00046a036 ↗
38. Matrix-assisted laser desorption/ionization mass spectrometry of synthetic polymers. 4. Coupling of size exclusion chromatography and MALDI-TOF using a spray-deposition interface10.1016/S0032-3861(99)00646-1 ↗
39. Synthesis–structure–performance relationship of cocondensed phenol–urea–formaldehyde resins by MALDI-ToF and 13C NMR10.1002/app.28735 ↗
40. MALDI of synthetic polymers—An update10.1016/S1387-3806(02)00971-5 ↗
41. Matrix-assisted laser desorption/ionization mass spectrometry of synthetic polymers. VI. Analysis of phenol–urea–formaldehyde cocondensates10.1002/app.12989 ↗
42. Evaluation of matrix-assisted laser desorption ionization mass spectrometry for polymer characterization10.1016/1044-0305(95)00589-7 ↗
43. MALDI-TOF, 13C NMR and FT-MIR analysis and strength characterization of glycidyl ether tannin epoxy resins10.1016/j.indcrop.2015.11.067 ↗
44. Phenol–urea–formaldehyde resin co-polymer synthesis and its influence on Elaeis palm trunk plywood mechanical performance evaluated by 13C NMR and MALDI-TOF mass spectrometry10.1016/j.ijadhadh.2015.09.002 ↗