Numerical Optimization of Laser Powder Bed Fusion Process Parameters for High-Precision Manufacturing of Pure Molybdenum
Source abstract
Abstract
This study presents a comprehensive numerical investigation of the Laser Powder Bed Fusion (LPBF) process for pure molybdenum, focusing on high-precision modeling and process optimization. The powder spreading behavior is simulated using the Discrete Element Method (DEM), while molten pool dynamics are analyzed through Computational Fluid Dynamics (CFD). Optimization of process parameters is performed using FLOW-3D Release 7 software in conjunction with the HEEDS-SHERPA algorithm. A total of 247 simulations are conducted to assess the effects of four critical parameters: laser power (50–400 W), scanning speed (80–300 mm/s), laser spot diameter (40–100 µm), and powder layer thickness (50–100 µm). The optimal parameter set—350 W laser power, 120 mm/s scanning speed, 50 µm spot diameter, and 50 µm layer thickness—results in an 80% laser absorption rate, a 60% reduction in micro-porosity, and over a 30% enhancement in both molten pool volume and surface area. Utilizing a fine 10 µm mesh resolution enables detailed insights into temperature gradients and phase transition behavior. The findings highlight that optimized parameter selection significantly improves the structural integrity of Mo-based components while minimizing manufacturing defects, thus offering valuable guidance for advancing industrial-scale additive manufacturing of refractory metals.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Vocational School of Technical Sciences, Akdeniz University, 07070 Antalya, Türkiye
Department of Mechanical Engineering, Gazi University, 06570 Ankara, Türkiye
Additive Manufacturing Technologies Application and Research Center, Gazi University, 06980 Ankara, Türkiye
Funding
Scientific and Technological Research Council of Türkiye (TUBITAK)
References (22)
Show source-provided references
1. Mo–Si–B alloys: Developing a revolutionary turbine-engine material10.1557/mrs2003.191 ↗
2. Investigation of the selective laser melting process with molybdenum powder
3. Yan, A., Atif, A.M., Wang, X., Lan, T., and Wang, Z. (2021). The microstructure and cracking behaviors of pure molybdenum fabricated by selective laser melting. Materials, 15.10.3390/ma15186230 ↗
4. Laser additive manufacturing of metallic components: Materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
5. Maamoun, A.H., Xue, Y.F., Elbestawi, M.A., and Veldhuis, S.C. (2018). Effect of selective laser melting process parameters on the quality of Al alloy parts: Powder characterization, density, surface roughness, and dimensional accuracy. Materials, 11.10.20944/preprints201811.0025.v1 ↗
6. Molybdenum and tungsten manufactured by selective laser melting: Analysis of defect structure and solidification mechanisms10.1016/j.ijrmhm.2019.104999 ↗
7. Densification and crack suppression in selective laser melting of pure molybdenum10.1016/j.matdes.2017.04.094 ↗
8. Balling phenomena in selective laser melted tungsten
9. The effect of powder oxidation on defect formation in laser additive manufacturing10.1016/j.actamat.2018.12.027 ↗
10. Crack suppression in additively manufactured tungsten by introducing secondary-phase nanoparticles into the matrix10.1016/j.ijrmhm.2018.11.013 ↗
11. Fully dense and crack free molybdenum manufactured by Selective Laser Melting through alloying with carbon10.1016/j.ijrmhm.2019.105000 ↗
12. Selective laser melting of high-performance pure tungsten: Parameter design, densification behavior and mechanical properties10.1080/14686996.2018.1455154 ↗
13. Microstructure, compressive performance and wear resistance of pure molybdenum additively manufactured via laser powder bed fusion10.1016/j.ijrmhm.2024.106740 ↗
14. Pure molybdenum manufactured by Laser Powder Bed Fusion: Thermal and mechanical characterization at room and high temperature
15. Yakang, K., Wang, C., Chen, X., Qu, Y., Yu, J., Ju, H., and Yilei, X. (2023). Review of Research Progress on Mo–Si–B Alloys. Materials, 16.10.3390/ma16155495 ↗
16. Synthesis and stabilization of a new phase regime in a Mo–Si–B based alloy by laser-based additive manufacturing10.1016/j.actamat.2018.03.037 ↗
17. Influence of TiC contents on the microstructure, mechanical properties, and oxidation behavior of Mo–10Si–8B alloys10.1016/j.intermet.2023.108122 ↗
18. Guo, Z., Wang, L., Wang, C., Ding, X., and Liu, J. (2021). Heat transfer, molten pool flow micro-simulation, and experimental research on molybdenum alloys fabricated via selective laser melting. Materials, 14.10.3390/ma14010075 ↗
19. Powder-bed-fusion additive manufacturing of molybdenum: Process simulation, optimization, and property prediction
20. Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
21. Laser powder bed fusion additive manufacturing of metals; physics, computational, and materials challenges10.1063/1.4937809 ↗
22. Chen, H.-Y., Lin, C.-C., Horng, M.-H., Chang, L.-K., Hsu, J.-H., Chang, T.-W., Hung, J.-C., Lee, R.-M., and Tsai, M.-C. (2022). Deep learning applied to defect detection in powder spreading process of magnetic material additive manufacturing. Materials, 15.10.3390/ma15165662 ↗