Mechanical and in situ thermal-related behavior during directed energy deposition additive manufacturing of a high-performance Al alloy
Source abstract
Abstract
Abstract Directed energy deposition (DED) additive manufacturing (AM) can fabricate, repair, and join near-net-shaped components for high-performance engineering applications, including biomedical, energy, and transport sectors. The broader adoption of DED remains constrained by the limited number of alloys available that can be reliably manufactured without imperfections, hence limiting mechanical properties. Here, we designed an Al–Ni–Ce–Mn–Fe AM alloy that can achieve an ultra-fine microstructure (<5 μm), uniform distribution of intermetallics, low residual stress (<32 MPa), and superior mechanical properties in as-built DED components. Compared to DED AlSi10Mg in the as-built state using the same conditions, the yield increased by 70%, and the ultimate tensile strength by 50%. DED-AM involves rapid cooling and complex thermal conditions, which largely influence the property of the final components. Post-characterization cannot capture the time resolved thermal behavior, hence offer limited mechanism-based guide for alloy design. In this study, we develop a novel multimodal characterization methodology for correlative in situ X-ray imaging, X-ray diffraction, and infrared imaging, enabling quantification of the in situ thermal-related behavior, including phase evolution, temperature distribution, and stress accumulation during DED. We elucidated key mechanisms driving the structure refinement and stress development in this alloy. The insights gained into the interplay between alloy composition, thermal-related behavior, and performance under specific AM conditions inform next-generation material design tailored for AM technologies.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (80)
Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. Alloy design via additive manufacturing: advantages, challenges, applications and perspectives10.1016/j.mattod.2021.11.026 ↗
3. Alloy design for laser powder bed fusion additive manufacturing: a critical review10.1088/2631-7990/ad1657 ↗
4. Predictive tools for the cooling rate-dependent microstructure evolution of AISI 316L stainless steel in additive manufacturing10.1016/j.jmrt.2024.03.008 ↗
5. Reducing porosity in AlSi10Mg parts processed by selective laser melting10.1016/j.addma.2014.08.001 ↗
6. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗
7. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
8. Additive manufacturing of an ultrastrong, deformable Al alloy with nanoscale intermetallics10.1038/s41467-024-48693-4 ↗
9. SLM-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
10. Direct ageing of LPBF Al-1Fe-1Zr for high conductivity and mechanical performance10.1016/j.actamat.2023.119199 ↗
11. Correlative spatter and vapour depression dynamics during laser powder bed fusion of an Al-Fe-Zr alloy10.1088/2631-7990/ad4e1d ↗
12. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
13. Achieving ultrahigh fatigue resistance in AlSi10Mg alloy by additive manufacturing10.1038/s41563-023-01651-9 ↗
14. Study of the intrinsic mechanisms of nickel additive for grain refinement and strength enhancement of laser aided additively manufactured Ti–6Al–4V10.1088/2631-7990/ac6b61 ↗
15. Design of Al–Fe–Mn alloy for both high-temperature strength and sufficient processability of laser powder bed fusion10.1016/j.addma.2023.103524 ↗
16. Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion10.1016/j.addma.2023.103858 ↗
17. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
18. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
19. Pore evolution mechanisms during directed energy deposition additive manufacturing10.1038/s41467-024-45913-9 ↗
20. Magnetic modulation of keyhole instability during laser welding and additive manufacturing10.1126/science.ado8554 ↗
21. Crystal structure of a high-pressure/high-temperature phase of alumina by in situ X-ray diffraction10.1038/nmat1121 ↗
22. In situ observation of crystal rotation in Ni-based superalloy during additive manufacturing process10.1038/s41467-023-38727-8 ↗
23. Operando X-ray diffraction during laser 3D printing10.1016/j.mattod.2019.10.001 ↗
24. The kinetics of precipitation from supersaturated solid solutions10.1016/0022-3697(61)90054-3 ↗
25. Cerium in aluminum alloys10.1007/s10853-019-03892-z ↗
26. Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
27. A second-generation apparatus for in situ synchrotron characterisation of directed energy deposition additive manufacturing with multi-modal monitoring and external forces10.1016/j.matdes.2026.115495 ↗
28. I12: the joint engineering, environment and processing (JEEP) beamline at diamond light source10.1107/S1600577515003513 ↗
29. Emissivity characteristics of roughened aluminum alloy surfaces and assessment of multispectral radiation thermometry (MRT) emissivity models10.1016/j.ijheatmasstransfer.2004.04.025 ↗
30. Effect of surface oxidation on emissivity properties of pure aluminum in the near infrared region10.1088/2053-1591/aa7fc9 ↗
31. Data analysis WorkbeNch (DAWN)10.1107/S1600577515002283 ↗
32. Processing two-dimensional X-ray diffraction and small-angle scattering data in DAWN 210.1107/S1600576717004708 ↗
33. Estimation of the background in powder diffraction patterns through a robust smoothing procedure10.1107/S0021889800003617 ↗
34. Correlative synchrotron X-ray imaging and diffraction of directed energy deposition additive manufacturing10.1016/j.actamat.2021.116777 ↗
35. Time-resolved synchrotron diffractometry of phase transformations in high strength nickel-based superalloys10.1016/j.actamat.2015.04.046 ↗
36. Least squares
37. The magnetic structures of Ce3Al11: a single crystal study10.1016/0304-8853(95)00051-8 ↗
38. Crystallographic, electronic and magnetic studies of Ce4Ni6Al23: a new ternary intermetallic compound in the cerium–nickel–aluminum phase diagram10.1016/S0022-4596(02)00167-6 ↗
39. Structure and physical properties of single crystal PrCr2Al20 and CeM2Al20 (M=V, Cr): a comparison of compounds adopting the CeCr2Al20 structure type10.1016/j.jssc.2012.06.035 ↗
40. The Fe–Ni–Al phase diagram in the Al-rich (>50at.% Al) corner10.1016/j.intermet.2007.04.012 ↗
41. Understanding the residual stress distribution through the thickness of atmosphere plasma sprayed (APS) thermal barrier coatings (TBCs) by high energy synchrotron XRD; digital image correlation (DIC) and image based modelling10.1016/j.actamat.2017.03.044 ↗
42. Modeling of lattice parameter in the Ni-Al system10.1007/s11661-006-0211-y ↗
43. Stress analysis of polycrystalline thin films and surface regions by X-ray diffraction10.1107/S0021889804029516 ↗
44. In-Situ synchrotron investigation of elastic and tensile properties of oxide dispersion strengthened EUROFER97 steel for advanced fusion reactors10.1016/j.actamat.2024.119876 ↗
45. The variation of the elastic constants of crystalline aluminum with temperature between 63°K and 773°K10.1103/PhysRev.91.816 ↗
46. Indentation plastometry of welds10.1002/adem.202101645 ↗
47. Use of hardness, PIP and tensile testing to obtain stress-strain relationships for metals10.1016/j.mechmat.2023.104846 ↗
48. Profilometry-based indentation plastometry to obtain stress-strain curves from anisotropic superalloy components made by additive manufacturing10.1016/j.mtla.2021.101017 ↗
49. Indentation plastometry for study of anisotropy and inhomogeneity in maraging steel produced by laser powder bed fusion10.1002/srin.202200881 ↗
50. Laser-directed energy deposition of ZrH2 particles reinforced Al7075 alloy: cracks elimination and strength enhancement10.1016/j.addma.2023.103877 ↗
51. Microstructure and mechanical properties of AlSi10Mg alloy built by laser powder bed fusion/direct energy deposition hybrid laser additive manufacturing10.1016/j.addma.2022.103160 ↗
52. Microstructure evolution and mechanical properties of laser additive manufacturing of high strength Al-Cu-Mg alloy10.1016/j.optlastec.2018.11.008 ↗
53. Effects of laser rescanning on microstructure and mechanical properties of Al-10Si-1Mg alloy produced by laser-directed energy deposition10.1016/j.mtcomm.2023.106979 ↗
54. Mechanical properties of AlSi10Mg alloy fabricated by laser melting deposition and improvements via heat treatment10.1016/j.ijleo.2018.10.112 ↗
55. Microstructure and mechanical properties of laser metal deposited AlSi10Mg alloys10.1080/02670836.2019.1674022 ↗
56. Microstructure and mechanical properties of laser DED produced crack-free Al 7075 alloy: effect of process parameters and heat treatment10.1016/j.msea.2022.144075 ↗
57. The influence of laser direct energy deposition processing parameters on Al7075 alloy and Zr-modified Al7075 alloy10.1007/s00170-024-14503-w ↗
58. Microstructure and property enhancement of 7075 aluminium alloy via laser metal deposition augmented by in-situ ultrasonic vibration10.1080/17452759.2023.2301482 ↗
59. Microstructure and mechanical properties of a combination interface between direct energy deposition and selective laser melted Al-Mg-Sc-Zr alloy10.3390/met11050801 ↗
60. Microstructure and mechanical properties of TiC-reinforced Al–Mg–Sc–Zr composites additively manufactured by laser direct energy deposition10.1007/s40195-021-01309-y ↗
61. Effect of laser additive manufacturing on the microstructure and mechanical properties of TiB2 reinforced Al-Cu matrix composite10.1016/j.msea.2022.142950 ↗
62. Significant strength enhancement of FeCrNiMox medium-entropy alloys via hard intermetallic particles dispersion strengthening10.1016/j.matchar.2023.112877 ↗
63. Evolution of eutectic microstructure and strength in an Al-Ce-Ni-Mn-Sc-Zr alloy fabricated by laser powder-bed fusion10.1016/j.addma.2025.104903 ↗
64. Ductile CoCrFeNiMox high entropy alloys strengthened by hard intermetallic phases10.1016/j.actamat.2016.06.063 ↗
65. Microstructure and mechanical properties of cast, eutectic Al-Ce-Ni-Mn-Sc-Zr alloys with multiple strengthening mechanisms10.1016/j.actamat.2024.120006 ↗
66. Cerium-based, intermetallic-strengthened aluminum casting alloy: high-volume co-product development10.1007/s11837-016-1943-9 ↗
67. Primary solidification of ternary compounds in Al-rich Al–Ce–Mn alloys10.1016/j.jallcom.2020.156048 ↗
68. Solidification kinetics of an Al-Ce alloy with additions of Ni and Mn10.3390/met13050955 ↗
69. Design and characterization of hierarchically-strengthened, cast Al-Ce-Ni-Mn-Sc-Zr alloys for high-temperature applications10.1007/978-3-031-50308-5_32 ↗
70. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing10.1016/j.actamat.2016.03.063 ↗
71. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation10.1016/j.addma.2016.05.014 ↗
72. In process monitoring of the thermal profile during solidification in laser directed energy deposition of aluminium10.1016/j.addlet.2022.100084 ↗
73. Investigations of the processing–structure–performance relationships of an additively manufactured AlSi10Mg alloy via directed energy deposition10.1016/j.jallcom.2023.169050 ↗
74. The effect of process parameters on residual stress evolution and distortion in the laser powder bed fusion of Ti-6Al-4V10.1016/j.addma.2019.05.015 ↗
75. Effect of substrate yield strength and grain size on the residual stress of direct energy deposition additive manufacturing measured by neutron diffraction10.1016/j.msea.2022.143632 ↗
76. Solidification microstructure and residual stress correlations in direct energy deposited type 316L stainless steel10.1016/j.matdes.2021.109782 ↗
77. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
78. Residual stress in laser-based directed energy deposition of aluminum alloy 2024: simulation and validation10.1007/s00170-021-07988-2 ↗
79. Control of residual stress and distortion in aluminium wire + arc additive manufacture with rolling10.1016/j.addma.2018.06.015 ↗
80. Design of hot-tearing resistant and thermally stable aluminium alloys for advanced casting technologies10.1016/j.matdes.2025.115152 ↗