Abstract

Dissimilar metal joining has always been a challenging task because of the metallurgical incompatibility and difference in melting points of alloys being joined. Diffusion and mixing of alloying elements from dissimilar base metals at the weld often cause unwanted metallurgical changes resulting in unsuccessful welds or underperformance of the weldment. Solid-state dissimilar friction welds of Inconel 718 and F22 were prepared in this study with an Inconel 625 interlayer to address the carbon enrichment of Inconel 718 during the welding. Defect-free rotary friction welds were produced in this study. Microstructural and mechanical properties investigation of the weldments and base metals was carried out, and results were analysed. Intermixing zone was observed at the weld interface due to the softening of the metal at the interface and rotatory motion during the welding. The high temperatures and the plastic deformation of the intermixing zone and thermo-mechanically affected zone (TMAZ) resulted in the grain refinement of the weld region. The highest hardness was observed at the Inconel 718/F22 weld interface due to the plastic strain and the carbon diffusion. The tensile specimens failed in the F22 base metal for the weld prepared with and without the Inconel 625 interlayer. Inconel 718/F22 welds exhibited lower toughness values compared to the Inconel 718/F22 welds prepared with Inconel 625 interlayer.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Industrial Engineering, College of Engineering, King Saud University, Riyadh 11451, Saudi Arabia

Department of Metallurgical and Materials Engineering, National Institute of Technology Warangal, Warangal 506004, India

Funding

National Plan for Science, Technology and Innovation (MAARIFAH), King Abdulaziz City for Science and Technology, Kingdom of Saudi Arabia

References (24)

Show source-provided references
1. Effect of Tempering Heat Treatment on the CO2 Corrosion Resistance of Quench-Hardened Cr-Mo Low-Alloy Steels for Oil and Gas Applications10.1016/j.corsci.2019.03.036 ↗
2. Future Research Directions in the Machining of Inconel 71810.1016/j.jmatprotec.2021.117260 ↗
3. The Superplasticity Improvement of Inconel 718 through Grain Refinement by Large Reduction Cold Rolling and Two-Stage Annealing10.1016/j.msea.2021.141713 ↗
4. A Review of Mechanical Properties of Additively Manufactured Inconel 718
5. Nickel Based Superalloy Welding Practices for Industrial Gas Turbine Applications10.1179/136217104225017099 ↗
6. Ferretti, S., Valenzano, G., and Cugno, W. (2006, January 2–6). International Space Station External Active Thermal Control System Lines Manufacturing. Proceedings of the AIAA 57th International Astronautical Congress, Valencia, Spain.10.2514/6.IAC-06-B4.2.09 ↗
7. An Assessment of Microstructure, Mechanical Properties and Corrosion Resistance of Dissimilar Welds between Inconel 718 and 310S Austenitic Stainless Steel10.1016/j.ijpvp.2014.01.002 ↗
8. Effect of Hardfaced Interlayer Thickness and Low Hydrogen Ferritic Capping on Ballistic Performance of Shielded Metal Arc Welded Armour Steel Joints10.1016/S1006-706X(13)60220-4 ↗
9. Friction Welding of AA6061 to AISI 4340 Using Silver Interlayer10.1016/j.dt.2015.05.007 ↗
10. Role of Nickel as an Interlayer in Dissimilar Metal Friction Welding of Maraging Steel to Low Alloy Steel10.1016/j.jmatprotec.2011.08.005 ↗
11. The Microstructures and Mechanical Properties of Dissimilar Laser Welding of Copper and 316L Stainless Steel with Ni Interlayer10.1016/j.cryogenics.2021.103344 ↗
12. Analysis of Ni Interlayer Effects on Laser Beam Welding of Dissimilar Pure Mo Alloy to Stainless Steel10.1016/j.ijrmhm.2021.105654 ↗
13. Fiber Laser Welding of Ti-6Al-4V to Inconel 718 Bimetallic Structure via Cu/Ta Multi-Interlayer10.1016/j.vacuum.2021.110461 ↗
14. Effect of Process Parameters on Microstructure and Properties of Laser Welded Joints of Aluminum/Steel with Ni/Cu Interlayer10.1016/S1003-6326(21)65654-6 ↗
15. Dissimilar Metal Welds Used in AUSC Power Plant, Fabrication and Structural Integrity Issues10.1088/1757-899X/1017/1/012022 ↗
16. Continuous Drive Friction Welding of Inconel 718 and EN24 Dissimilar Metal Combination10.1179/174328408X369384 ↗
17. Joining of Inconel 718 and 316 Stainless Steel Using Electron Beam Melting Additive Manufacturing Technology10.1016/j.matdes.2016.01.041 ↗
18. The Relationship between Carbon Content, Microstructure, and Intergranular Liquation Cracking in Cast Nickel Alloy 71810.1007/BF02656823 ↗
19. Tempering Behavior of the Fusion Boundary Region of an F22/625 Weld Overlay
20. Characterization of the Interface of an Alloy 625 Overlay on Steels Using Nanoindentation10.1007/s11665-018-3444-1 ↗
21. Effect of Heat Treatment Parameters on the Microstructure and Properties of Inconel-625 Superalloy10.1007/s11665-017-2774-8 ↗
22. Rehman, A.U., Babu, N.K., Talari, M.K., Usmani, Y.S., and Al-Khalefah, H. (2021). Microstructure and Mechanical Properties of Dissimilar Friction Welding Ti-6Al-4V Alloy to Nitinol. Metals, 11.10.3390/met11010109 ↗
23. Reed, R.C., and Rae, C.M.F. (2014). Physical Metallurgy of the Nickel-Based Superalloys, Elsevier. [5th ed.].10.1016/B978-0-444-53770-6.00022-8 ↗
24. Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars10.5781/JWJ.2019.37.1.6 ↗