The interlayer properties of the CRTS III slab track during construction directly affect its long-term service condition. This article introduces time-varying coefficients that characterize the early properties of the interface between track slab and SCC to improve the bilinear CZM. Based on this, an interlayer property evolution model of the CRTS III slab track during construction is established. The evolution mechanism of interlayer properties under complex loads and the influence mechanism of key parameters on them are revealed. The results show that after SCC pouring, the interlayer damage at the corner of the slab becomes a sensitive area due to the combined effects of SCC shrinkage and temperature gradients. Interlayer damage initially manifests at the corner of the slab before progressively spreading toward the center of the slab, influencing the composite performance and force transmission characteristics of the track structure. The interlayer bonding property, shrinkage performance of SCC, and construction temperature substantially affect interlayer damage evolution. To reduce the risk of damage, mineral admixtures and expansion agents can be added as additives to improve the bonding property and minimize shrinkage of SCC. Insulation measures should be taken for SCC during low-temperature construction, and SCC pouring construction below 0 °C and above 30 °C should be avoided.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Railway Engineering and Dynamics · Tunneling and Rock Mechanics · Geotechnical Engineering and Underground Structures

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Civil Engineering, Beijing Jiaotong University, Beijing 100044, China

Zhejiang Institute of Intelligent Transportation, Zhejiang CICO, Hangzhou 310020, China

China Railway Engineering Design and Consulting Group Co., Ltd., Beijing 100055, China

Anhui Xingyu Track Equipment Co., Ltd., Bengbu 233000, China

Funding

Fundamental Research Funds for the Central Universities · 111 Project · Science and Technology Research and Development Project of China State Railway Group Co., Ltd. · Research Program of the Shandong Department of Transportation

References (41)

Show source-provided references
1. Evaluation index of CRTS III prefabricated slab track cracking condition based on interval AHP10.1142/S0219455421400137 ↗
2. Effects of the subgrade differential arch on damage characteristics of CRTS III slab track and vehicle dynamic response10.1016/j.conbuildmat.2022.126982 ↗
3. Study on the Evolution Characteristics of Temperature Field in CRTS III Ballastless Track Slab
4. Influence of bubble defects on the bonding performance of the interlayer interface of the CRTS III slab ballastless track structure10.1016/j.conbuildmat.2021.125003 ↗
5. Early warping deformation of high-speed railway CRTS III track slabs10.1016/j.engstruct.2023.116651 ↗
6. Improvement in early-age cracking performance of concrete with hybrid steel-macropolypropylene fiber blends10.1016/j.matpr.2022.04.554 ↗
7. Autogenous deformation and coefficient of thermal expansion of early-age concrete: Initial outcomes of a study using a newly-developed Temperature Stress Testing Machine10.1016/j.cemconcomp.2021.103997 ↗
8. Cause Analysis of Interlayer Seams of CRTS III Slab Ballastless Track
9. Research on the Early Temperature Field of Self-compacting Concrete of Ballastless Track and its lnfluence
10. Cai, X., Zhang, Q., Zhang, Y., Wang, Q., Luo, B., Yang, G., and Lau, A. (2021). Deformation law and control limit of CRTSIII slab track under subgrade frost heave. Appl. Sci., 11.10.3390/app11083520 ↗
11. Two-stage identification of interlayer contact loss for CRTS III prefabricated slab track based on multi-index fusion10.1631/jzus.A2300010 ↗
12. Zhu, K., Wu, B., Zeng, Z., and Liu, B. (2016, January 1–3). Reason Analysis of the Gap between CRTS Slab and Self Compacting Concrete. Proceedings of the International Conference on Education, Management, Computer and Society, Shenyang, China.10.2991/emcs-16.2016.152 ↗
13. Experimental study on the interface fatigue between track slab and self-compacting concrete for CRTS III slab track10.1016/j.engfailanal.2023.107302 ↗
14. Full-scale fatigue test of unit-plate ballastless track laid on long-span cable-stayed bridge10.1016/j.conbuildmat.2020.118601 ↗
15. Evolution mechanism of interlayer fatigue properties of CRTS III slab track10.1016/j.conbuildmat.2022.129459 ↗
16. Effect of daily changing temperature on the curling behavior and interface stress of slab track in construction stage10.1016/j.conbuildmat.2018.06.224 ↗
17. Arching mechanism of the slab joints in CRTSII slab track under high temperature conditions10.1016/j.engfailanal.2019.01.076 ↗
18. Study on the interlayer debonding and its effects on the mechanical properties of CRTS II slab track based on viscoelastic theory10.1016/j.conbuildmat.2019.07.089 ↗
19. Interface damage and arching mechanism of CRTS II slab track under temperature load10.1016/j.conbuildmat.2021.123258 ↗
20. Determination of the interfacial properties of longitudinal continuous slab track via a field test and ANN-based approaches10.1016/j.engstruct.2021.113039 ↗
21. Thermal evolution of CRTS II slab track under various environmental temperatures: Experimental study10.1016/j.conbuildmat.2022.126699 ↗
22. Time-variant reliability of interlayer damage of CRTS-II slab track by combining the second-order fourth-moment and outcrossing method10.1016/j.conbuildmat.2023.132790 ↗
23. Corrosion effects on the capacity and ductility of concrete half-joint bridges10.1016/j.conbuildmat.2022.129555 ↗
24. Normal statistical fracture analysis of Roller-compacted concrete on the basis of non-linear elastic fracture mechanics10.1016/j.compstruct.2023.117543 ↗
25. Temperature field and thermal effect analysis of CRTS III ballastless track structure under the outdoor natural environment10.1016/j.conbuildmat.2022.129383 ↗
26. Temperature field and thermal effects of the longitudinal connected slab track based on the measurement data and thermal-fluid-structure coupling analysis10.1016/j.conbuildmat.2022.128121 ↗
27. Real-time temperature field and thermal deformation of slab track on cable-stayed bridge10.1016/j.csite.2023.103582 ↗
28. Composite shear stud strength at early concrete ages10.1061/(ASCE)0733-9445(2004)130:6(952) ↗
29. Experimental research on fracture properties of adjerence for new to old concrete
30. Drying shrinkage of early-age concrete for twin-block slab track10.1016/j.conbuildmat.2020.118237 ↗
31. Debonding analysis and identification of the interface between sleeper and track slab for twin-block slab tracks10.1142/S0219455421400113 ↗
32. Wet/dry influence on behaviors of closed-cell polymeric cross-linked foams under static, dynamic and impact loads10.1016/j.conbuildmat.2018.08.052 ↗
33. Application of rubber mats in transition zone between two different slab tracks in high-speed railway10.1016/j.conbuildmat.2020.118219 ↗
34. An accurate method for fast assessment of under slab mats (USM) performance in ballastless track structures10.1016/j.conbuildmat.2021.123953 ↗
35. (2017). Code for Thermal Design of Civil Building (Standard No. GB 50176-2016).
36. Study of the thermal behaviour of a production unit of concrete structural components10.1016/S1359-4311(03)00161-3 ↗
37. Tan, Y., Li, H., Xie, Y., and Yi, Z. (2014, January 5–8). Research on Deformation Properties of Scc Used In High Speed Railway Slab Ballastless Track of CRTSb. Proceedings of the 3rd International Symposium on Design, Performance and Use of Self-Consolidating Concrete, Xiamen, China.
38. Self-compacting concretes with supplementary cementitious materials: Shrinkage and cracking tendency10.1061/(ASCE)MT.1943-5533.0001852 ↗
39. Mechanical property and damage evolution of concrete interface of ballastless track in high-speed railway: Experiment and simulation10.1016/j.conbuildmat.2018.07.163 ↗
40. Shrinkage of self-compacting concrete. A comparative analysis10.1016/j.jobe.2016.12.002 ↗
41. Shrinkage behavior of self-compacting concrete10.1631/jzus.A1100340 ↗