journal article·2019-10

Effect of double stage solution treatment on the volume fraction of massive phase (αm) as a new method to obtain a fine lamellar α/β in Ti–6Al–4V alloy

Ghozali Suprobo, Nokeun Park, Eung Ryul Baek

Intermetallics· Volume 113
Publisher page

Abstract

Abstract This study investigated the effect of double stage solution treatment (DSST) on the behavior of the massive phase (αm) transformation in a Ti–6Al–4V alloy. αm Phase transformation has been reported to occur by introducing a cooling rate between 20 °C/s and 410 °C/s before reaching the martensite start temperature (Ms). A featureless αm morphology is observed with optical microscopy (OM) because the α and β phases cannot be clearly distinguished. Higher magnification images with scanning electron microscopy (SEM) show that αm has a sub-lamellar morphology with two distinguishable regions: the clear region and the white-dot region. The volume fraction of αm was evaluated after DSST with a first annealing above the β-transus temperature, followed by a second annealing above Ms with varying holding times. The solution treatment at 850 °C for 1800 s yielded the highest fraction of αm (22.4%), which was confirmed with OM and further supported by the phase maps in the electron backscatter diffraction results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Investigation of the grain size effect on mechanical properties of Ti-6Al-4V alloy with equiaxed and bimodal microstructures10.1088/1757-899X/219/1/012013 ↗
2. Effect of microstructural morphology on the mechanical properties of titanium alloys10.1088/1742-6596/240/1/012022 ↗
3. Microstructure-Tensile properties correlation for the Ti-6Al-4V titanium alloy10.1007/s11665-015-1437-x ↗
4. The effect of microstructure on the mechanical properties of two-phase titanium alloys10.1016/S0261-3069(97)00087-3 ↗
5. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
6. Effect of microstructural factors on fatigue and fatigue crack propagation behaviors of mill-annealed Ti-6Al-4V alloy10.3365/KJMM.2018.56.12.845 ↗
7. High temperature deformation behavior of Ti-6Al-4V alloy with an equiaxed microstructure: a neural networks analysis10.3365/met.mat.2008.04.213 ↗
8. The role of modeling in the development of advanced processes for metallic aerospace alloys10.1007/BF03027423 ↗
9. The effect of heat treatment on microstructure and mechanical behaviors of laser direct energy deposited Ti-6Al-4V plate10.5781/JWJ.2018.36.5.10 ↗
10. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
11. Microstructural evolution of massively transformed γ-tial during isothermal aging10.1016/S1359-6462(96)00416-2 ↗
12. On the existence of the β→αm transformation in the alloy systems Ti-Ag, Ti-Au, and Ti-Si10.1007/BF02646561 ↗
13. G. Suprobo, A. A. Ammar, N. Park, E.R. Baek, and S. Kim, Thermal Decomposition of Massive Phase to Fine Lamellar α/β in Ti-6Al-4V Additively Manufactured Alloy by Directed Energy Deposition, Metals and Materials International. accepted. doi: 10.1007/s12540-019-00304-4.10.1007/s12540-019-00304-4 ↗
14. Cahn · 1996
15. Effect of single and duplex stage heat treatment on the microstructure and mechanical properties of cast Ti-6Al-4V alloy10.1007/s13632-013-0103-7 ↗
16. Effect of microstructure on the fatigue properties of Ti-6Al-4V titanium alloys10.1016/j.matdes.2012.10.059 ↗
17. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: bimodal vs. lamellar structures
18. Massive transformation in Ti-6Al-4V additively manufactured by selective electron beam melting10.1016/j.actamat.2015.11.011 ↗
19. The impact of diffusion on synthesis of high-strength titanium alloys from elemental powder blends10.4028/www.scientific.net/KEM.436.113 ↗
20. Vander Voort · 2009 · vol. 9
21. Characterization and decompositional crystallography of the massive phase grains in an additively-manufactured Ti-6Al-4V alloy10.1016/j.matchar.2017.01.012 ↗
22. Quenching-rate determination for standard steel tensile specimens10.1007/BF00543613 ↗
23. Influence of cooling rate and aging on the lamellar microstructure and fractography of TC21 titanium alloy10.1007/s13632-012-0055-3 ↗
24. Effect of heat treatment on microstructures and mechanical properties in a full lamellar PM TiAl alloy10.1590/S1516-14392012005000059 ↗
25. Prediction of the martensite start temperature for β titanium alloys as a function of composition10.1016/j.scriptamat.2008.12.034 ↗
26. Application of solidification theory to titanium alloys
27. Holt · 1977
28. Formation of α- Widmanstatten structure: effects of grain size and cooling rate on the Widnmanstatten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
29. Bainite formation kinetics in steels and the dynamic nature of the autocatalytic nucleation process10.1016/j.scriptamat.2017.06.051 ↗
30. Formation characteristics of the α/β interface phase in Ti-6Ai-4v10.1007/BF02817630 ↗
31. The effect of Al and V on microstructure and transfomiation of β phase during solution treatments of cast Ti-6Al-4V alloy
32. Phase transformation dynamics during welding of Ti – 6Al – 4V Phase transformation dynamics during welding of Ti – 6Al – 4V10.1063/1.1737476 ↗
33. The effect of initial structure on phase transformation in continuous heating of a TA15 titanium alloy10.3390/met7060200 ↗
34. Crystallography of α phase precipitated on dislocations and deformation twin boundaries in a β titanium alloy10.2320/matertrans1989.33.585 ↗
35. Lütjering · 2007 · 283