journal article·2023-05-31Open access

Laser Cavitation Peening: A Review

Hitoshi Soyama, Yuka Iga

Applied Sciences· Volume 13· Issue 11

Abstract

During submerged laser peening using a pulsed laser, a bubble that behaves like cavitation is generated after laser ablation (LA). The bubble is referred to as laser cavitation (LC). The amplitude of the shockwave in water generated by LA is larger than that of LC; however, the impact passing through the target metal during LC is larger than that of LA. LC impact can be utilized for peening at optimized conditions. Thus, submerged laser peening is referred to as “laser cavitation peening”, as the peening method using the cavitation impact is known as “cavitation peening”. The impact induced by a hemispherical bubble is more aggressive than that of a spherical bubble with a microjet. Laser cavitation peening can improve the fatigue strength of metallic materials by producing work-hardening and introducing compressive residual stress. Three-dimensional additively manufactured metals (3D metals) such as titanium alloy are attractive materials for aviation components and medical implants; however, the fatigue strength of as-built components is nearly half of that of bulk metals, and this is an obstacle for the applications of 3D metals. In the present study, published research papers are reviewed to identify the key factors of laser cavitation peening, with additional visualization of LC and data. Then, improvements in the fatigue strength of metallic materials, including 3D metals treated by laser cavitation peening, are summarized.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · Ultrasound and Cavitation Phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Finemechanics, Tohoku University, Sendai 980-8579, Japan

Institute of Fluid Science, Tohoku University, Sendai 980-8577, Japan

Funding

JSPS KAKENHI · Amada Foundation

References (73)

Show source-provided references
1. Mechanical surface treatments on titanium, aluminum and magnesium alloys10.1016/S0921-5093(98)01168-X ↗
2. Additively manufactured heterogeneously porous metallic bone with biostructural functions and bone-like mechanical properties10.1016/j.jmst.2020.05.056 ↗
3. Electron beam additive manufacturing of titanium components: Properties and performance10.1115/1.4025773 ↗
4. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
5. Sano, Y. (2020). Quarter century development of laser peening without coating. Metals, 10.10.3390/met10010152 ↗
6. A critical comparative review of cavitation peening and other surface peening methods10.1016/j.jmatprotec.2022.117586 ↗
7. The use of various peening methods to improve the fatigue strength of titanium alloy Ti6Al4V manufactured by electron beam melting10.3934/matersci.2018.5.1000 ↗
8. Laser peening: A tool for additive manufacturing post-processing
9. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
10. Kuji, C., and Soyama, H. (2023). Mechanical surface treatment of titanium alloy Ti6Al4V manufactured by direct metal laser sintering using laser cavitation. Metals, 13.10.3390/met13010181 ↗
11. Retardation of crack initiation and growth in austenitic stainless steels by laser peening without protective coating10.1016/j.msea.2005.11.017 ↗
12. Surface texturing by indirect laser shock surface patterning for manipulated friction coefficient10.1016/j.jmatprotec.2018.02.041 ↗
13. Femtosecond laser peening of friction stir welded 7075-T73 aluminum alloys10.1016/j.jmatprotec.2018.06.022 ↗
14. Influence of pulse duration on mechanical properties and dislocation density of dry laser peened aluminum alloy using ultrashort pulsed laser-driven shock wave10.1063/5.0083511 ↗
15. A mechanism for inducing compressive residual stresses on a surface by laser peening without coating10.3390/met10060816 ↗
16. Soyama, H. (2021). Laser cavitation peening and its application for improving the fatigue strength of welded parts. Metals, 11.10.3390/met11040531 ↗
17. Study on processing and strengthening mechanisms of mild steel subjected to laser cavitation peening10.1016/j.apsusc.2021.150242 ↗
18. Behavior of bubbles induced by the interaction of a laser pulse with a metal plate in water10.1007/s00339-004-3196-7 ↗
19. Key factors and applications of cavitation peening
20. Comparison between the improvements made to the fatigue strength of stainless steel by cavitation peening, water jet peening, shot peening and laser peening10.1016/j.jmatprotec.2019.01.030 ↗
21. Evaluation of the enhanced cavitation impact energy using a pvdf transducer with an acrylic resin backing10.1016/j.measurement.2011.03.027 ↗
22. Cavitation bubble oscillation period as a process diagnostic during the laser shock peening process10.1007/s00339-017-1209-6 ↗
23. Mechanical effect of laser-induced cavitation bubble of 2a02 alloy10.1016/j.optlastec.2018.02.039 ↗
24. Development of water jet peening technique for reactor internal components of nuclear power plant
25. Soyama, H. (2020). Cavitating jet: A review. Applied Sciences, 10.10.3390/app10207280 ↗
26. Collapse of an initially spherical vapour cavity in neighbourhood of a solid boundary10.1017/S0022112071001058 ↗
27. Experimental investigations of cavitation-bubble collapse in neighborhood of a solid boundary10.1017/S0022112075003448 ↗
28. Surface oscillations and jet development in pulsating bubbles10.1051/jphyscol:1979849 ↗
29. Brennen, C.E. (1995). Cavitation and Bubble Dynamics, Oxford University Press.10.1093/oso/9780195094091.001.0001 ↗
30. Ley, S.V., and Low, C.M.R. (1980). Ultrasound in Synthesis, Springer.
31. The acoustic pressure generated by the cavitation bubble expansion and collapse near a rigid wall10.1063/5.0043822 ↗
32. Numerical investigation of laser-induced cavitation bubble dynamics near a rigid surface based on three-dimensional fully compressible model10.1016/j.ijheatmasstransfer.2022.122853 ↗
33. The effect of surface geometry of solid wall on the collapse of a cavitation bubble10.1115/1.4053350 ↗
34. Cavitation bubble dynamics and microjet atomization near tissue-mimicking materials10.1063/5.0136577 ↗
35. Relationship between a non-spherical collapse of a bubble and a stress state inside a wall10.1063/5.0136355 ↗
36. Laser and shot peening effects on fatigue crack growth in friction stir welded 7075-T7351 aluminum alloy joints10.1016/j.ijfatigue.2006.05.007 ↗
37. Comparison of mechanisms of advanced mechanical surface treatments in nickel-based superalloy10.1016/j.msea.2013.04.021 ↗
38. Cavitation erosion by single laser-produced bubbles10.1017/S0022112098008738 ↗
39. Introduction of Compressive Residual Stress into Alloy Tool Steel by Submerged Laser Peening Utilizing Laser Cavitation Impact10.1299/jsmelem.2017.9.010 ↗
40. Development of a portable laser peening device and its effect on the fatigue properties of HT780 butt-welded joints10.1016/j.finmec.2022.100080 ↗
41. Estimation of aggressive intensity of a cavitating jet with multiple experimental methods10.1016/j.wear.2017.11.001 ↗
42. Effects of laser peening parameters on plastic deformation in aqueous glycerol solution as plasma confinement layer
43. Effect of impact induced by cavitation bubble on submerged laser peening
44. (2013). Test Strip, Holder, and Gage for Shot Peening. Standard No. J442_202205.
45. (2010). Procedures for Using Standard Shot Peening Almen Strip. Standard No. J443_201708.
46. Soyama, H. (2020). Cavitation peening: A review. Metals, 10.10.3390/met10020270 ↗
47. Comparison between impact induced by abrasion and bubble collapse impact on laser peening10.1299/jsmemecj.2016.G0400402 ↗
48. Soyama, H., Yahata, Y., and Saito, M. (2021, January 10–13). Aspect of bubbles in narrow tube imitating root canal induced by er: Yag laser. Proceedings of the 11th International Symposium on Cavitation, Virtual.
49. Sugimoto, Y., and Obata, S. (2021). Behavior of a sphere caused by pulsed laser induced bubble simulating stone crushing with TUL. Proc. 11th Inter. Sympo. Cavitation, 614–617.
50. Influences of focusing conditions on dynamics of laser ablation at a solid–liquid interface10.7567/APEX.6.122701 ↗
51. Soyama, H. (2020). Comparison between shot peening, cavitation peening and laser peening by observation of crack initiation and crack growth in stainless steel. Metals, 10.10.3390/met10010063 ↗
52. Cavitation bubble dynamics10.1016/S1350-4177(97)00009-6 ↗
53. Luminescence from spherically and aspherically collapsing laser induced bubbles10.1103/PhysRevLett.80.393 ↗
54. Bubble dynamics, shock waves and sonoluminescence10.1098/rsta.1999.0327 ↗
55. Luminescence intensity of vortex cavitation in a venturi tube changing with cavitation number10.1016/j.ultsonch.2020.105389 ↗
56. On the pressure developed in a liquid during the collapse of a spherical cavity10.1080/14786440808635681 ↗
57. Soyama, H., Kuji, C., Kuriyagawa, T., Chighizola, C.R., and Hill, M.R. (2021). Optimization of residual stress measurement conditions for a 2D method using X-ray diffraction and its application for stainless steel treated by laser cavitation peening. Materials, 14.10.3390/ma14112772 ↗
58. Soyama, H. (2018, January 17–22). Surface mechanics design by cavitation peening using submerged pulse laser. Proceedings of the Abstracts of 7th International Conference on Laser Peening and Related Phenomena, Singapore.
59. Introduction of compressive residual stress into stainless steel by bubble induced by submerged pulse laser
60. Improving effects of cavitation peening, using a pulsed laser or a cavitating jet, and shot peening on the fatigue properties of additively manufactured titanium alloy Ti6Al4V10.1016/j.surfcoat.2022.129047 ↗
61. Laser subtractive and laser powder bed fusion of metals: Review of process and production features10.1108/RPJ-03-2021-0055 ↗
62. Estimating the median fatigue limit for very small up-and-down quantal response tests and for S-N data with runouts
63. Depth-profiling of residual stress and microstructure for austenitic stainless steel surface treated by cavitation, shot and laser peening10.1016/j.msea.2021.141037 ↗
64. Soyama, H., and Takeo, F. (2020). Effect of various peening methods on the fatigue properties of titanium alloy Ti6Al4V manufactured by direct metal laser sintering and electron beam melting. Materials, 13.10.3390/ma13102216 ↗
65. Soyama, H., and Kuji, C. (2023, January 29–30). Comparison on fatigue strength of additive manufactured titanium alloy by various peening methods. Proceedings of the Annual Meeting Society Materials Science Japan, Tsukuba, Japan.
66. Soyama, H., Kuji, C., and Liao, Y. (2023). Comparison of the effects of submerged laser peening, cavitation peening and shot peening on the improvement of the fatigue strength of magnesium alloy AZ31. J. Magnes. Alloy., 11.10.1016/j.jma.2023.04.004 ↗
67. Deep rolling effect on fatigue behavior of austenitic stainless steels10.1016/j.ijfatigue.2016.10.008 ↗
68. Comparative study of the effects of surface mechanical attrition treatment and conventional shot peening on low cycle fatigue of a 316L stainless steel10.1016/j.surfcoat.2018.06.041 ↗
69. Effect of applied stress and temperature on residual stresses induced by peening surface treatments in alloy10.1007/s11665-018-3371-1 ↗
70. Improvement of AISI 304 austenitic stainless steel low-cycle fatigue life by initial and intermittent deep rolling10.1007/s00170-018-2955-0 ↗
71. Characterization of shot peening properties and modelling on the fatigue performance of 304 austenitic stainless steel10.1016/j.ijfatigue.2020.105621 ↗
72. Effect of compressive residual stress introduced by cavitation peening and shot peening on the improvement of fatigue strength of stainless steel10.1016/j.jmatprotec.2020.116877 ↗
73. Soyama, H. (2023). Abstracts of Quantum Beam Application for Sciences and Industries, Available online: https://qbasis2023.isir-sanken.jp/QBASIS2023/wp-content/uploads/2023/05/Q-BASIS-2023_Abstract_finalver.pdf.