Mechanical Properties and Explosive Spalling Behavior of Steel-Fiber-Reinforced Concrete Exposed to High Temperature—A Review

Peng Zhang, Luoyi Kang, Juan Wang, Jinjun Guo, Shaowei Hu, Yifeng Ling

Applied Sciences· Volume 10· Issue 7

Abstract

Steel-fiber-reinforced concrete (SFRC) is being increasingly applied to various buildings and civil infrastructure as an advanced cementitious composite. In recent years, the requirements for SFRC in the construction industry have increased. Additionally, the fire resistance of SFRC has attracted attention; therefore, numerous investigations regarding the residual properties of SFRC have been conducted. This paper critically reviews the mechanical properties of SFRC subjected to elevated temperatures, including its residual compressive strength, flexural strength, tensile strength, elastic properties, fracture properties, and stress–strain relationships. The residual mechanical performance of SFRC and the action mechanism of steel fibers are reviewed in detail. Moreover, factors affecting the explosive spalling of concrete at high temperatures as well as the effect of steel fibers on the microstructure of heated concrete are discussed. It is demonstrated that, in general, SFRC exhibits better residual mechanical properties when exposed to elevated temperatures than plain concrete and can prevent the risk of explosive spalling more effectively. The purpose of this literature review is to provide an exhaustive insight into the feasibility of SFRC as a refractory building material; additionally, future research needs are identified.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Fire effects on concrete materials · Innovative concrete reinforcement materials · Structural Load-Bearing Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Water Conservancy Engineering, Zhengzhou University, Zhengzhou 450001, China

College of Civil Engineering, Chongqing University, Chongqing 400045, China

Department of Civil, Construction and Environmental Engineering, Iowa State University, Ames, IA 50011, USA

Funding

National Natural Science Foundation of China · CRSRI Open Research Program of China · Open Projects Funds of Dike Safety and Disaster Prevention Engineering Technology Research Center of Chinese Ministry of Water Resources of China · Program for Innovative Research Team (in Science and Technology) in University of Henan Province of China

References (100+)

Show source-provided references
1. Experimental investigation on flexural toughness of hybrid fiber reinforced concrete (HFRC) containing metakaolin and pumice10.1016/j.conbuildmat.2013.10.087 ↗
2. Performance of fly ash based geopolymer mortars in sulphate solution10.25103/jestr.031.07 ↗
3. Valorisation of glass wastes for the development of geopolymer composites–Durability, thermal and microstructural properties: A review10.1016/j.conbuildmat.2019.06.169 ↗
4. Valorisation of glass waste for development of geopolymer composites-Mechanical properties and rheological characteristics: A review10.1016/j.conbuildmat.2019.06.041 ↗
5. Noumowe, A.N., Clastres, P., Debicki, G., and Costaz, J.L. (1995, January 2–4). High performance concrete for severe thermal conditions. Proceedings of the International Conference on Concrete under Severe Conditions, CONSEC’95, Sapporo, Japan.
6. Effects of elevated temperatures on properties of concrete10.1016/j.firesaf.2007.01.003 ↗
7. Effect of elevated temperatures on the mechanical properties of concrete10.1016/j.prostr.2019.05.047 ↗
8. Effect of the high temperatures on the microstructure and compressive strength of high strength fibre concretes10.1016/j.conbuildmat.2018.12.074 ↗
9. Physicochemical, mineralogical, and morphological characteristics of concrete exposed to elevated temperatures10.1016/S0008-8846(01)00736-0 ↗
10. Mechanical properties of high-strength concrete after fire10.1016/j.cemconres.2003.11.007 ↗
11. Explosive spalling and residual mechanical properties of fiber-toughened high-performance concrete subjected to high temperatures10.1016/j.cemconres.2005.12.014 ↗
12. Pore structures, permeabilities, and compressive strengths of concrete at temperatures up to 800 °C
13. Fracture behaviour of steel fibre reinforced recycled aggregate concrete after exposure to elevated temperatures10.1016/j.conbuildmat.2016.10.072 ↗
14. Mechanical properties of concrete at high temperature—A review10.1016/j.conbuildmat.2015.05.131 ↗
15. Literature review of study on mechanism of explosive spalling in concrete at elevated temperatures
16. Bažant, Z.P., Kaplan, M.F., and Bazant, Z.P. (1996). Concrete at High Temperatures: Material Properties and Mathematical Models, Longman-Addison-Wesley.
17. Spalling and pore pressure in HPC at high temperatures10.1016/S0008-8846(00)00384-7 ↗
18. High-temperature behaviour of HPC with polypropylene fibres: From spalling to microstructure10.1016/S0008-8846(01)00596-8 ↗
19. Prevention and control of cracking by use of short random fibers
20. Shear behaviour of steel fibre reinforced self-consolidating concrete beams based on the modified compression field theory10.1016/j.compstruct.2012.02.025 ↗
21. An orthotropic material model for steel fibre reinforced concrete based on the orientation distribution of fibres10.1016/j.compstruct.2014.11.018 ↗
22. Anchorage effects of various steel fibre architectures for concrete reinforcement10.1007/s40069-016-0148-5 ↗
23. Predicting the pullout response of inclined hooked steel fibers10.1016/j.cemconres.2010.05.005 ↗
24. Effect of the fiber geometry on the pullout response of mechanically deformed steel fibers10.1016/j.cemconres.2012.10.014 ↗
25. Influence of high temperature on the mechanical properties of hybrid fibre reinforced normal and high strength concrete10.1016/j.conbuildmat.2017.10.129 ↗
26. Effect of aggregate size and inclusion of polypropylene and steel fibers on explosive spalling and pore pressure in ultra-high-performance concrete (UHPC) at elevated temperature10.1016/j.cemconcomp.2019.02.016 ↗
27. Compressive and tensile properties of reactive powder concrete with steel fibres at elevated temperatures10.1016/j.conbuildmat.2012.12.066 ↗
28. Splitting strength of GGBFS concrete incorporating with steel fiber and polypropylene fiber after exposure to elevated temperatures10.1016/j.firesaf.2012.07.009 ↗
29. Influence of moisture states of natural and recycled aggregates on the slump and compressive strength of concrete10.1016/S0008-8846(03)00186-8 ↗
30. Compressive behavior of fiber reinforced high-performance concrete subjected to elevated temperatures10.1016/j.cemconres.2004.02.011 ↗
31. Steel fibre reinforced concrete at elevated temperatures10.1016/0262-5075(84)90006-X ↗
32. Effect of elevated temperature on splitting tensile strength of fibre concrete10.1016/0262-5075(89)90090-0 ↗
33. Effect of high temperatures on high performance steel fibre reinforced concrete10.1016/j.cemconres.2006.03.024 ↗
34. Test methods for mechanical properties of concrete at high temperatures, Recommendations, Part 3: Compressive strength for service and accident conditions10.1007/BF02473077 ↗
35. Test methods for mechanical properties of concrete at high temperatures recommendations–Part 4: Tensile strength for service and accident conditions
36. Ismail, R., Zakwan, F.A.A., Petrus, C., Marzuki, N.A., Hashim, N.H., and Mustafa, M.F. (2014). Compressive behavior of steel fiber reinforced concrete after exposed to high temperatures. CIEC 2013, Springer.10.1007/978-981-4585-02-6_63 ↗
37. Coupling effects of silica fume and steel-fiber on the compressive behaviour of recycled aggregate concrete after exposure to elevated temperature10.1016/j.conbuildmat.2018.07.035 ↗
38. The experimental study on mechanical property of steel fiber reinforced high strength concrete after high temperature
39. Impact of steel fibre dosage on mechanical properties of concrete under high temperature
40. Experimental research for the effect of high temperature on the mechanical properties of steel fiber-reinforced concrete10.1016/j.conbuildmat.2014.11.005 ↗
41. Mechanical properties of steel fibre reinforced geopolymer concretes at elevated temperatures10.1016/j.conbuildmat.2016.03.158 ↗
42. Compressive behavior of steel fiber reinforced recycled aggregate concrete after exposure to elevated temperatures10.1016/j.conbuildmat.2014.08.012 ↗
43. Mechanical properties of steel fiber reinforced reactive powder concrete following exposure to high temperature reaching 800 °C10.1016/j.nucengdes.2011.04.008 ↗
44. Experimental study on dynamic compressive behavior of steel fiber reinforced concrete at elevated temperatures10.1016/j.conbuildmat.2019.03.138 ↗
45. Mehta, P.K. (1986). Concrete: Structure, Properties and Materials, Prentice-Hall Inc.
46. Effect of fire on concrete and concrete structures10.1002/pse.51 ↗
47. Effect of fibre type and geometry on maximum pore pressures in fibre-reinforced high strength concrete at elevated temperatures10.1016/j.cemconres.2011.11.014 ↗
48. Compressive behaviour of hybrid fiber-reinforced reactive powder concrete after high temperature10.1016/j.matdes.2012.05.026 ↗
49. Effect of Cu-Zn coated steel fibers on high temperature resistance of reactive powder concrete10.1016/j.cemconres.2018.12.008 ↗
50. Pore pressure development in hybrid fibre-reinforced high strength concrete at elevated temperatures10.1016/j.cemconres.2011.07.001 ↗
51. Effect of heating and cooling regimes on residual strength and microstructure of normal strength and high-performance concrete10.1016/S0008-8846(99)00264-1 ↗
52. Crack propagation behavior of cermets and cemented carbides under repeated thermal shocks by the improved quench test10.1023/A:1004575519293 ↗
53. Postfiring stress-strain hysteresis of concrete subjected to various heating and cooling regimes10.1002/fam.785 ↗
54. Totten, G.E. (2006). Steel Heat Treatment Handbook, CRC Press.10.1201/NOF0849384530 ↗
55. Effects of heating followed by water quenching on strength and microstructure of ultra-high performance concrete10.1016/j.conbuildmat.2019.02.123 ↗
56. Mechanical properties of steel-polypropylene fibre reinforced concrete under elevated temperature10.1016/j.proeng.2015.11.146 ↗
57. The effect of different fibres on the flexural behaviour of concrete exposed to normal and elevated temperatures10.1016/j.conbuildmat.2016.10.089 ↗
58. Influence of steel and/or polypropylene fibres on the behaviour of concrete at high temperature: Spalling, transfer and mechanical properties10.1016/j.conbuildmat.2016.11.120 ↗
59. Heat exposure tests on various types of fibre mortar10.1080/19648189.2011.9693360 ↗
60. Contribution of cocktail of polypropylene and steel fibres in improving the behaviour of high strength concrete subjected to high temperature10.1016/j.conbuildmat.2010.11.064 ↗
61. British Standard Institute (2004). Eurocode 2: Design of Concrete Structure–Part 1. 2: General Rules–Structural Fire Design, British Standard Institute. BS EN. 1992-1-2:2004.
62. Study on high-performance concrete at high temperatures in China (2004–2016)-An updated overview10.1016/j.firesaf.2017.10.007 ↗
63. Evaluation of mechanical properties of steel-fibre-reinforced concrete exposed to high temperatures by double-punch test10.1016/j.conbuildmat.2015.01.042 ↗
64. Mindess, S., Young, J.F., and Darwin, D. (2003). Concrete, Pearson Education, Pearson Education.
65. High temperature mechanical properties of high-strength fly ash concrete with and without fibers
66. Effect of short fibers on residual permeability and mechanical properties of hybrid fibre reinforced high strength concrete after heat exposition10.1016/j.cemconres.2006.05.006 ↗
67. High temperature resistance of normal strength and autoclaved high strength mortars incorporated polypropylene and steel fibers10.1016/j.conbuildmat.2006.11.003 ↗
68. Mechanical properties of fiber reinforcedconcrete after high temperature
69. Residual strength of hybrid-fiber-reinforced high-strength concrete after exposure to high temperatures10.1016/j.cemconres.2003.11.010 ↗
70. Compressive behaviour of concrete structures incorporating recycled concrete aggregates, rubber crumb and reinforced with steel fibre, subjected to elevated temperatures10.1016/j.jclepro.2014.02.036 ↗
71. Thermal and mechanical properties of fiber reinforced high performance self-consolidating concrete at elevated temperatures10.1016/j.cemconres.2011.06.012 ↗
72. Fracture behaviors of a new steel fiber reinforced recycled aggregate concrete with crumb rubber10.1016/j.conbuildmat.2013.11.075 ↗
73. Residual fracture energy of cement paste, mortar and concrete subject to high temperature10.1016/j.tafmec.2005.11.007 ↗
74. Residual fracture energy of high-performance and normal concrete subject to high temperatures10.1007/BF02480828 ↗
75. The effect of testing conditions (hot and residual) on fracture toughness of fiber reinforced high-strength concrete subjected to high temperatures10.1016/j.cemconres.2013.04.003 ↗
76. Study on residual behaviour and flexural toughness of fibre cocktail reinforced self compacting high performance concrete after exposure to high temperature
77. Analysis of the mechanical and fracture behavior of heated ultra-high-performance fiber-reinforced concrete by X-ray computed tomography10.1016/j.cemconres.2019.02.015 ↗
78. Compressive stress–strain relationship of steel fiber-reinforced reactive powder concrete after exposure to elevated temperatures10.1016/j.conbuildmat.2012.05.031 ↗
79. Mechanical properties of steel fibre reinforced concrete exposed at high temperatures10.1617/s11527-009-9504-0 ↗
80. Influence of steel fibers on strain-softening of high-strength concrete
81. Stress–strain curves for steel-fiber reinforced concrete under compression10.1016/S0958-9465(99)00021-9 ↗
82. Effect of damage on permeability and hygro-thermal behaviour of HPCs at elevated temperatures: Part 1. Experimental results10.12989/cac.2005.2.3.189 ↗
83. Residual strength and pore structure of high-strength concrete and normal strength concrete after exposure to high temperatures10.1016/S0958-9465(98)00034-1 ↗
84. The use of thermal analysis in assessing the effect of temperature on a cement paste10.1016/j.cemconres.2004.06.015 ↗
85. Dehydration and rehydration processes of cement paste exposed to high temperature environments10.1023/B:JMSC.0000025827.65956.18 ↗
86. Composition and microstructural changes of cement pastes upon heating, as studied by neutron diffraction10.1016/S0008-8846(03)00229-1 ↗
87. Behaviour of cement concrete at high temperature
88. Lim, S. (2015). Effects of Elevated Temperature Exposure on Cement-Based Composite Materials. [Ph.D. Thesis, University of Illinois at Urbana-Champaign].
89. Measurement and prediction of pore pressures in saturated cement mortar subjected to radiant heating
90. Analysis of the effect of heating and re-curing on the microstructure of high-strength concrete using X-ray CT10.1016/j.conbuildmat.2013.11.007 ↗
91. The behaviour ofconcrete structures in fire10.2298/TSCI0702037F ↗
92. Study of mechanisms of explosive spalling in high-strength concrete at high temperatures using acoustic emission10.1016/j.conbuildmat.2012.06.070 ↗
93. An experimental method for assessing the spalling sensitivity of concrete mixture submitted to high temperature10.1016/j.cemconcomp.2012.04.002 ↗
94. Naus, D. (2006). The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review.10.2172/974590 ↗
95. Evolution of the bond strength between reinforcing steel and fibre reinforced concrete after high temperature exposure10.1016/j.conbuildmat.2018.05.065 ↗
96. Danish investigations on silica fume concretes at elevated temperatures
97. Performance of thermally damaged fibre reinforced concretes10.1016/j.conbuildmat.2008.08.009 ↗
98. Felicetti, R. (2007, January 8–9). Assessment of the equivalent thermal diffusivity for fire analysis of concrete structures. Proceedings of the Fib Task Group 4.3 Workshop Fire Design of Concrete Structures, Coimbra, Portugal.
99. Effects of hybrid fiber on HPC properties under hightemperature
100. Mechanical properties and microstructure of ultra-lightweight cement composites with fly ash cenospheres after exposure to high temperatures10.1016/j.conbuildmat.2018.01.009 ↗