Abstract

The effect of heat treatment on microstructural and mechanical properties of three different Al-Si alloys was investigated. Both sand and permanent molds were used to produce Al7Si, Al-12Si and Al-17Si alloy samples. Changes in microstructure, hardness, wear and surface roughness were evaluated. In T6 heat treatment, two different temperatures (425 degrees C and 500 degrees C) and three different durations (5, 15, and 30 h) were selected, and after quenching, aging was carried out at 190 degrees C for 16 h. It was found that increasing the heat treatment temperature and duration resulted in smaller silicon phases for all three alloys. This case positively affected the hardness, wear and surface roughness of the alloys. The best parameter for the morphology of Al7Si and Al-12Si alloys in sand casting samples was 500 degrees C solution temperature and 30 h. 425 degrees C solutionizing temperature was found to be insufficient for Si modification.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. S. Hegde, K.N. Prabhu, Modification of eutectic silicon in Al–Si alloys. J. Mater. Sci. 43(9), 3009–3027 (2008)10.1007/s10853-008-2505-5 ↗
2. M. Cabrini et al., Corrosion behavior of heat-treated AlSi10Mg manufactured by laser powder bed fusion. Materials. 11(7), 1051 (2018)10.3390/ma11071051 ↗
3. F. Kahraman, M. Kulekçi, Microstructure and eutectic morphology of Al-12.5°/O Si alloy refined with antimony. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi. 11(1), 10–14 (2007)
4. O.E. Sebaie et al., The effects of mischmetal, cooling rate and heat treatment on the eutectic Si particle characteristics of A319. 1, A356. 2 and A413. 1 Al-Si casting alloys. Mater. Sci. Eng. Struct. Materials: Prop. Microstruct. Process. 480(1–2), 342–355 (2008)10.1016/j.msea.2007.07.039 ↗
5. A. Vencl, I. Bobić, Z. Mišković, Effect of thixocasting and heat treatment on the tribological properties of hypoeutectic Al–Si alloy. Wear. 264(7–8), 616–623 (2008)10.1016/j.wear.2007.05.011 ↗
6. M. Haque, A. Sharif, Study on wear properties of aluminium–silicon piston alloy. J. Mater. Process. Technol. 118(1–3), 69–73 (2001)10.1016/S0924-0136(01)00869-X ↗
7. N. Raghukiran, R. Kumar, Effect of scandium addition on the microstructure, mechanical and wear properties of the spray formed hypereutectic aluminum–silicon alloys. Mater. Sci. Eng. A 641, 138–147 (2015)10.1016/j.msea.2015.06.027 ↗
8. M. Moustafa, F. Samuel, H. Doty, Effect of solution heat treatment and additives on the microstructure of Al-Si (A413. 1) automotive alloys. J. Mater. Sci. 38(22), 4507–4522 (2003)10.1023/A:1027333602276 ↗
9. M.O. Shabani, A. Mazahery, Microstructural prediction of cast A356 alloy as a function of cooling rate. JOM. 63(8), 132 (2011)10.1007/s11837-011-0127-x ↗
10. M. Uludağ, R. Çetin, D. Dispinar, Freezing range, melt quality, and hot tearing in Al-Si alloys. Metall. Mater. Trans. A 49(5), 1948–1961 (2018)10.1007/s11661-018-4512-8 ↗
11. H. Barhoumi et al., Study on the effect of pressure and cooling rate on the solidification Characteristics and mechanical properties of Al-11% Si cast alloy. 2019
12. R. Rana, R. Purohit, S. Das, Reviews on the influences of alloying elements on the microstructure and mechanical properties of aluminum alloys and aluminum alloy composites. Int. J. Sci. Res. Publications. 2(6), 1–7 (2012)
13. S. Gowri, F. Samuel, Effect of alloying elements on the solidification characteristics and microstructure of Al-Si-Cu-Mg-Fe 380 alloy. Metall. Mater. Trans. A 25(2), 437–448 (1994)10.1007/BF02647989 ↗
14. Q. Wang et al., Cast Aluminum Alloys (Google Patents, 2014)
15. Z. Li et al., Influence of Sr, Fe and Mn content and casting process on the microstructures and mechanical properties of AlSi7Cu3 alloy. Mater. Sci. Eng. A, Struct. Mater. Prop. Microstruct. Process. 689, 286–297 (2017)10.1016/j.msea.2017.02.041 ↗
16. H. Ye, An overview of the development of Al-Si-alloy based material for engine applications. J. Mater. Eng. Perform. 12(3), 288–297 (2003)10.1361/105994903770343132 ↗
17. J. Ding et al., Effect of solution treatment on microstructure and mechanical properties of A356. 2 aluminum alloy treated with Al–Sr–La master alloy. Adv. Eng. Mater. 20(6), 1701173 (2018)10.1002/adem.201701173 ↗
18. D. Manickam, S.K.V. SANTHANAM, Effect of solution heat treatment and artificial aging on compression behaviour of A356 alloy. Mater. Sci. 25(3), 281–285 (2019)
19. D. Zhang, L. Zheng, The quench sensitivity of cast Al-7 Wt Pct Si-0.4 Wt Pct Mg alloy. Metall. Mater. Trans. A 27(12), 3983–3991 (1996)10.1007/BF02595647 ↗
20. A.P. Rao et al., Effect of grain refinement on wear properties of al and al–7Si alloy. Wear. 257(1–2), 148–153 (2004)
21. V. Vijeesh, K.N. Prabhu, Review of microstructure evolution in hypereutectic Al–Si alloys and its effect on wear properties. Trans. Indian Inst. Met. 67(1), 1–18 (2014)
22. N. Saheb et al., Influence of Ti addition on wear properties of Al–Si eutectic alloys. Wear. 249(8), 656–662 (2001)10.1016/S0043-1648(01)00687-1 ↗
23. R. Sharma, D. Dwivedi, Influence of silicon (wt.%) and heat treatment on abrasive wear behaviour of cast Al–Si–Mg alloys. Mater. Sci. Engineering: A 408(1–2), 274–280 (2005)10.1016/j.msea.2005.08.013 ↗
24. Y. Alemdağ, M. Beder, Çözündürme ve Yaşlandırma İşleminin Al-7Si-4Zn-3Cu Alaşımının Sürtünme ve Aşınma Özelliklerine Etkisi. Uluslararası Muhendislik Arastirma ve Gelistirme Dergisi 11(2), 602–611 (2019)10.29137/umagd.531910 ↗
25. S. Kori, T. Chandrashekharaiah, Studies on the dry sliding wear behaviour of hypoeutectic and eutectic Al–Si alloys. Wear. 263(1–6), 745–755 (2007)10.1016/j.wear.2006.11.026 ↗
26. C.-Y. Yang et al., Effects of Sr and Sb modifiers on the sliding wear behavior of A357 alloy under varying pressure and speed conditions. Wear. 261(11–12), 1348–1358 (2006)10.1016/j.wear.2006.03.051 ↗
27. L. Lasa, J. Rodriguez-Ibabe, Effect of composition and processing route on the wear behaviour of Al–Si alloys. Scripta Mater. 46(6), 477–481 (2002)10.1016/S1359-6462(02)00020-9 ↗
28. M. Prabhudev et al., Influence of Cu addition on dry sliding wear behaviour of A356 alloy. Procedia Eng. 97, 1361–1367 (2014)10.1016/j.proeng.2014.12.417 ↗
29. G. Rajaram, S. Kumaran, T.S. Rao, High temperature tensile and wear behaviour of aluminum silicon alloy. Mater. Sci. Eng. A 528(1), 247–253 (2010)10.1016/j.msea.2010.09.020 ↗
30. A. Alpas, J. Zhang, Effect of SiC particulate reinforcement on the dry sliding Wear of aluminium-silicon alloys (A356). Wear. 155(1), 83–104 (1992)10.1016/0043-1648(92)90111-K ↗
31. A. Mandal, B. Murty, M. Chakraborty, Sliding wear behaviour of T6 treated A356–TiB2 in-situ composites. Wear. 266(7–8), 865–872 (2009)10.1016/j.wear.2008.12.011 ↗
32. S. Tjong, S. Wu, H. Liao, Wear behaviour of an Al–12% Si alloy reinforced with a low volume fraction of SiC particles. Compos. Sci. Technol. 57(12), 1551–1558 (1998)10.1016/S0266-3538(97)00074-2 ↗
33. A. Lakshmikanthan et al., Microstructure, mechanical and wear properties of the A357 composites reinforced with dual sized SiC particles. J. Alloys Compd. 786, 570–580 (2019)10.1016/j.jallcom.2019.01.382 ↗
34. M. Uludağ, A statistical assessment of casting quality-tribological properties of eutectic Al-12Si alloy: effect of Mg. J. Mater. Eng. Perform. (2020). https://doi.org/10.1007/s11665-020-05225-710.1007/s11665-020-05225-7 ↗
35. S. Nikanorov et al., Structural and mechanical properties of Al–Si alloys obtained by fast cooling of a levitated melt. Mater. Sci. Engineering: A 390(1–2), 63–69 (2005)10.1016/j.msea.2004.07.037 ↗
36. O. Uzun et al., Hardness and microstructural characteristics of rapidly solidified Al–8–16 wt.% Si alloys. J. Alloys Compd. 376(1–2), 149–157 (2004)10.1016/j.jallcom.2004.01.017 ↗
37. W. Kurz, D. Fisher, Fundamentals of Solidification; 1992 (Trans Tech Publications, 1989)
38. Q. Li et al., Mechanical properties and microstructural evolution of Yb-modified Al-20% Si alloy. J. Mater. Eng. Perform. 27(7), 3498–3507 (2018)10.1007/s11665-018-3456-x ↗
39. J. Wang et al., Grain refinement of Al–Si alloy (A356) by melt thermal treatment. J. Mater. Process. Technol. 141(1), 29–34 (2003)10.1016/S0924-0136(02)01007-5 ↗
40. M. Zuo et al., Effect of P and Sr complex modification on Si phase in hypereutectic Al–30Si alloys. Mater. Design. 47, 857–864 (2013)10.1016/j.matdes.2012.12.054 ↗
41. M. Haque, M. Maleque, Effect of process variables on structure and properties of aluminium–silicon piston alloy. J. Mater. Process. Technol. 77(1–3), 122–128 (1998)10.1016/S0924-0136(97)00409-3 ↗
42. M.A. Elahi, S. Shabestari, Effect of various melt and heat treatment conditions on impact toughness of A356 aluminum alloy. Trans. Nonferrous Met. Soc. China. 26(4), 956–965 (2016)10.1016/S1003-6326(16)64191-2 ↗
43. J. Yaokawa et al., Estimation of solid solution Si concentration in Al–Si alloy castings based on dimensional change during heat treatment. Mater. Trans., F–M2019823 (2019)10.2320/matertrans.F-M2019823 ↗
44. J. Wang et al., Effects of melt thermal treatment on hypoeutectic Al–Si alloys. Mater. Sci. Engineering: A 338(1–2), 101–107 (2002)10.1016/S0921-5093(02)00067-9 ↗
45. M.F. Ibrahim et al., Effect of Microalloying Elements on the Heat Treatment Response and Tensile Properties of Al-Si-Mg Alloys, in Solidification. IntechOpen, (2017)10.5772/intechopen.70665 ↗
46. M. Tash et al., Effect of metallurgical parameters on the hardness and microstructural characterization of as-cast and heat-treated 356 and 319 aluminum alloys. Mater. Sci. Engineering: A 443(1–2), 185–201 (2007)10.1016/j.msea.2006.08.054 ↗
47. F. Samuel, Incipient melting of Al5Mg8Si6Cu2 and Al2Cu intermetallics in unmodified and strontium-modified Al–Si–Cu–Mg (319) alloys during solution heat treatment. J. Mater. Sci. 33(9), 2283–2297 (1998)10.1023/A:1004383203476 ↗
48. A. Hekmat-Ardakan et al., Wear behaviour of hypereutectic Al–Si–Cu–Mg casting alloys with variable Mg contents. Wear. 269(9–10), 684–692 (2010)10.1016/j.wear.2010.07.007 ↗
49. Y. Birol, Microstructural evolution during annealing of a rapidly solidified Al–12Si alloy. J. Alloys Compd. 439(1–2), 81–86 (2007)10.1016/j.jallcom.2006.08.068 ↗
50. H. Lus, Murat et al., Wear properties of squeeze cast in situ Mg2Si–A380 alloy. Int. J. Cast Met. Res. 28(1), 59–64 (2015)10.1179/1743133614Y.0000000131 ↗
51. D. Dwivedi, Adhesive wear behaviour of cast aluminium–silicon alloys: overview. Materials & Design (1980–2015) 31(5), 2517–2531 (2010)10.1016/j.matdes.2009.11.038 ↗
52. D.K. Dwivedi, Wear behaviour of cast hypereutectic aluminium silicon alloys. Mater. Design. 27(7), 610–616 (2006)10.1016/j.matdes.2004.11.029 ↗
53. H. Saghafian et al., Effects of Iron, Manganese, and cooling rate on microstructure and dry sliding wear behavior of LM13 aluminum alloy. Tribol. Trans. 60(5), 888–901 (2017)10.1080/10402004.2016.1227513 ↗
54. J. Kang et al., Synergistic effects of Ce and Mg on the microstructure and tensile properties of Al-7Si-0.3 Mg-0.2 Fe alloy. J. Alloys Compd. 796, 267–278 (2019)10.1016/j.jallcom.2019.05.049 ↗
55. H. Hasirci, Effects of heat treatment parameters on the abrasive wear behaviours of the eutectic AlSi alloy. J. Polytechnic-Politeknik Dergisi. 18(1), 7–13 (2015)