Effect of processing on structural features of anodic aluminum oxides
Source abstract
Abstract
Morphological features of the anodic aluminum oxide (AAO) templates fabricated by electrochemical oxidation under different processing conditions were investigated. The selection of the polishing parameters does not appear to be critical as long as the aluminum substrate is polished adequately prior to the anodization process. AAO layers with a highly ordered pore distribution are obtained after anodizing in 0.6 M oxalic acid at 20 °C under 40 V for 5 minutes suggesting that the desired pore features are attained once an oxide layer develops on the surface. While the pore features are not affected much, the thickness of the AAO template increases with increasing anodization treatment time. Pore features are better and the AAO growth rate is higher at 20 °C than at 5 °C; higher under 45 V than under 40 V; higher with 0.6 M than with 0.3 M oxalic acid.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Concrete Corrosion and Durability · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. H. Masuda, K. Fukuda, Science 268, 1466 (1995)10.1126/science.268.5216.1466 ↗
2. Q. Li, K. Wang, D. Xi, W. Dang, Z. Ren, Q. He, J. Bai, C. Gu, Q. Li, K. Wang, D. Xi, W. Dang, Z. Ren, Q. He, J. Bai, C. Gu, J. Nanosci. Nanotechnol. 10, 7447 (2010)10.1166/jnn.2010.2854 ↗
3. G. Xie, M. Song, K. Mitsuishi, K. Furuya, Appl. Surf. Sci. 241, 91 (2005)10.1016/j.apsusc.2004.09.023 ↗
4. A. Santos, L. Vojkuvka, J. Pallares, J. Ferré-Borrull, L.F. Marsal, Nanoscale Res. Lett. 4, 1021 (2009)10.1007/s11671-009-9351-5 ↗
5. Q. Wang, X. Sun, S. Luo, L. Sun, X. Wu, M. Cao, C. Hu, Cryst. Growth Des. 7, 2665 (2007)10.1021/cg0605178 ↗
6. R. Bertholdo, M.C. Assis, P. Hammer, S.H. Pulcinelli, C.V. Santilli, J. Eur. Ceram. Soc. 30, 181 (2010)10.1016/j.jeurceramsoc.2009.06.014 ↗
7. H.M. Chen, C.F. Hsin, R.-S. Liu, S.-F. Hu, H.-Y. Huang, J. Electrochem. Soc. 154, K11 (2007)
8. Y.-F. Liu, F.-H. Wang, D.-L. Guo, S.-Y. Huang, J.-P. Sang, X.-W. Zou, Appl. Phys. A 97, 677 (2009)10.1007/s00339-009-5289-9 ↗
9. R.E. Sabzi, K. Kant, D. Losic, Electrochim. Acta 55, 1829 (2010)10.1016/j.electacta.2009.10.075 ↗
10. A. Saedi, M. Ghorbani, Mater. Chem. Phys. 91, 417 (2005)10.1016/j.matchemphys.2004.12.001 ↗
11. G. Sharma, M.V. Pishko, C.A. Grimes, J. Mater. Sci. 42, 4738 (2007)10.1007/s10853-006-0769-1 ↗
12. H.-B. Xu, H.-Z. Chen, W.-J. Xu, M. Wang, Chem. Phys. Lett. 412, 294 (2005)10.1016/j.cplett.2005.07.006 ↗
13. Z.F. Zhou, Y.C. Zhou, Y. Pan, X.G. Wang, Mater. Lett. 62, 3419 (2008)10.1016/j.matlet.2008.02.071 ↗
14. K.H. Lee, Y.P. Huang, C.C. Wong, Electrochim. Acta 56, 2394 (2011)10.1016/j.electacta.2010.11.024 ↗
15. G.D. Sulka, W.J. Stepniowski, Electrochim. Acta 54, 3683 (2009)10.1016/j.electacta.2009.01.046 ↗
16. J.M. Montero-Moreno, M. Sarret, C. Müller, Surf. Coat. Technol. 201, 6352 (2007)10.1016/j.surfcoat.2006.12.003 ↗
17. S. Su, C. Li, F. Zhang, M. Yokoyama, Superlattices Microstruct. 44, 514 (2008)10.1016/j.spmi.2008.02.001 ↗
18. P. Ozer, B. Yuksel, Y. Birol, Appl. Surf. Sci. 258, 4544 (2012). doi: 10.1016/j.apsusc.2012.01.02510.1016/j.apsusc.2012.01.025 ↗
19. L. Zaraska, G.D. Sulka, M. Jaskuła, Surf. Coat. Technol. 205, 2432 (2010)10.1016/j.surfcoat.2010.09.038 ↗
20. G.D. Sulka, K.G. Parkola, Thin Solid Films 515, 338 (2006)10.1016/j.tsf.2005.12.094 ↗
21. A. Belwalkar, E. Grasing, W. Van Geertruyden, Z. Huang, W.Z. Misiolek, J. Membr. Sci. 319, 192 (2008)10.1016/j.memsci.2008.03.044 ↗
22. G.D. Sulka, S. Stroobants, V.V. Moshchalkov, G. Borghs, J.-P. Celisd, J. Electrochem. Soc. 151, B260 (2004)10.1149/1.1695384 ↗
23. Y. Wu, J. Cui, Y. Wang, G. Xu, X. Zhang, Adv. Mater. Res. 181–182, 707 (2011)
24. D.C. Leitao, C.T. Sousa, J. Ventura, F. Carpinteiro, J.G. Correia, M.M. Amado, J.B. Sousa, J.P. Araujo, Phys. Status Solidi C 11, 3488 (2008)10.1002/pssc.200779430 ↗
25. L. Zaraska, G.D. Sulka, J. Szeremeta, M. Jaskuła, Electrochim. Acta 55, 4377 (2010)10.1016/j.electacta.2009.12.054 ↗
26. J.M. Montero-Moreno, M. Sarret, C. Müller, Microporous Mesoporous Mater. 136, 68 (2010)10.1016/j.micromeso.2010.07.022 ↗
27. K. Lee, Y. Tang, M. Ouyang, Nano Lett. 8, 4624 (2008)10.1021/nl803271c ↗
28. J.M. Montero-Moreno, M. Sarret, C. Müller, J. Electrochem. Soc. 154, C169 (2007)
29. I. Vrublevsky, V. Parkoun, J. Schreckenbach, G. Marx, Appl. Surf. Sci. 227, 282 (2004)10.1016/j.apsusc.2003.12.003 ↗
30. N.N. Bwana, J. Nanopart. Res. 10, 313 (2008)10.1007/s11051-007-9253-3 ↗
31. M.K. McQuaig, A. Toro, W.V. Geertruyden, W.Z. Misiolek, J. Mater. Sci. 46, 243 (2011)10.1007/s10853-010-4966-6 ↗
32. G.D. Sulka, V. Moshchalkov, G. Borghs, J.-P. Celis, J. Appl. Electrochem. 37, 789 (2007)10.1007/s10800-007-9312-6 ↗
33. G.Q. Ding, W.Z. Shen, M.J. Zheng, Z.B. Zhou, Nanotechnology 17, 2590 (2006)10.1088/0957-4484/17/10/024 ↗
34. M. Almasi Kashi, A. Ramazani, J. Phys. D, Appl. Phys. 38, 2396 (2005)10.1088/0022-3727/38/14/015 ↗
35. T. Ono, Ch. Konoma, H. Miyashita, Y. Kanaori, M. Esashi, Jpn. J. Appl. Phys. Part 1 42, 3867 (2003)10.1143/JJAP.42.3867 ↗