Abstract

Abstract Apart from some strongly fluorescent wood species, the general fluorescence of wood has long been ignored. Recent studies suggest that each species has a distinct fluorescence, originating from both basic components and characteristic extractives. However, wood colour and fluorescence rapidly change upon exposure to sunlight. In this study, 288 samples of Acer pseudoplatanus, Quercus robur, Picea abies and Juglans nigra were irradiated with different bands of ultraviolet (UV) and visible (VIS) light. Photosensitivity was examined in regards of colour, infrared absorbance (FTIR), and fluorescence imaging. UV light caused strong yellowing in all examined species, mostly correlating with lignin degradation, carbonyl formation and the appearance of a broad banded fluorescence emission. VIS light above 420 nm, however, caused different, partly contradicting effects in colour and fluorescence, and did not affect lignin. J. nigra proved to be most sensitive towards VIS-induced yellowing and bleaching. The main new finding of this study is that the native long wave fluorescence of wood was strongly decreased by VIS-irradiation above 510 nm wavelength in all samples. This effect was not species-specific, probably originating from a cross-species wood component. The results have potential impacts on non-destructive image-based evaluation methods and wood identification.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood and Agarwood Research · Cultural Heritage Materials Analysis · Wood Treatment and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institut für Berufswissenschaften im Bauwesen, Leibniz Universität Hannover , Herrenhäuser Str. 8 , 30419 Hannover , Germany

References (56)

Show source-provided references
1. Antikainen, J., Hirvonen, T., Kinnunen, J., and Hauta-Kasari, M. (2012). Heartwood detection for Scotch pine by fluorescence image analysis. Holzforschung 66: 877–881, https://doi.org/10.1515/hf-2011-0131.10.1515/hf-2011-0131 ↗
2. Avella, T., Dechamps, R., and Bastin, M. (1988). Fluorescence study of 10,610 woody species from the Tervuren (Tw) Collection, Belgium. IAWA J. 9: 346–352, https://doi.org/10.1163/22941932-90001094.10.1163/22941932-90001094 ↗
3. Baur, S.I. and Easteal, A.J. (2014). ESR studies on the free radical generation in wood by irradiation with selected sources from UV to IR wavelength regions. Holzforschung 68: 775–780, https://doi.org/10.1515/hf-2013-0185.10.1515/hf-2013-0185 ↗
4. Beyer, M., Müller, M., Scheiding, W., and Emmler, R. (2012). Grundlegende Untersuchungen zum Verhalten von Oberflächen aus Thermoholz und dunklen nativen Hölzern bei Bestrahlung. Holztechnologie 53: 18–23.
5. Bianco, M.-A., Handaji, A., and Savolainen, H. (1998). Quantitative analysis of ellagic acid in hardwood samples. Sci. Total Environ. 222: 123–126, https://doi.org/10.1016/S0048-9697(98)00294-0.10.1016/S0048-9697(98)00294-0 ↗
6. Bonifazi, G., Calienno, L., Capobianco, G., Lo Monaco, A., Pelosi, C., Picchio, R., and Serranti, S. (2015). Modeling color and chemical changes on normal and red heart beech wood by reflectance spectrophotometry, Fourier transform infrared spectroscopy and hyperspectral imaging. Polym. Degrad. Stabil. 113: 10–21, https://doi.org/10.1016/j.polymdegradstab.2015.01.001.10.1016/j.polymdegradstab.2015.01.001 ↗
7. Burtin, P., Jay-Allemand, C., Charpentier, J.-P., and Janin, G. (1998). Natural wood colouring process in Juglans sp. (J. nigra, J. regia and hybrid J. nigra 23 × J. regia) depends on native phenolic compounds accumulated in the transition zone between sapwood and heartwood. Trees 12: 258–264, https://doi.org/10.1007/pl00009716.10.1007/PL00009716 ↗
8. Burtin, P., Jay-Allemand, C., Charpentier, J.-P., and Janin, G. (2000). Modifications of hybrid walnut (Juglans nigra 23 × Juglans regia) wood colour and phenolic composition under various steaming conditions. Holzforschung 54: 33–38, https://doi.org/10.1515/hf.2000.006.10.1515/HF.2000.006 ↗
9. Buschle-Diller, G. and Zeronian, S.H. (1993). Photodegradation of oxidized cotton cellulose. J. Appl. Polym. Sci. 47: 1319–1328, https://doi.org/10.1002/app.1993.070470802.10.1002/app.1993.070470802 ↗
10. Camorani, P., Badiali, M., Francomacaro, D., Gamassi, M., Piuri, V., Scotti, F., and Zanasi, M. (20082008). A classification method for wood types using fluorescence spectra. 2008 IEEE instrumentation and measurement technology conference. I2MTC 200810.1109/IMTC.2008.4547245 ↗
11. Victoria, BC, Canada, 12-15 May 2008. IEEE Service Center, Piscataway, NJ, pp. 1312-1315.
12. Castellan, A., Ruggiero, R., Frollini, E., Ramos, L.A., and Chirat, C. (2007). Studies on fluorescence of cellulosics. Holzforschung 61: 504–508, https://doi.org/10.1515/hf.2007.090.10.1515/HF.2007.090 ↗
13. Chang, S.-T., Wang, S.-Y., and Cheng, S.-S. (2000). Environmental effects on the color of sugi (Cryptomeria japonica D. Don) heartwood. J. Wood Sci. 46: 390–394, https://doi.org/10.1007/bf00776402.10.1007/BF00776402 ↗
14. Dehon, L., Macheix, J.J., and Durand, M. (2002). Involvement of peroxidases in the formation of the brown coloration of heartwood in Juglans nigra. J. Exp. Bot. 53: 303–311, https://doi.org/10.1093/jexbot/53.367.303.10.1093/jexbot/53.367.303 ↗
15. Derbyshire, H. and Miller, E.R. (1981). The photodegradation of wood during solar irradiation. Part 1-effects on the structural integrity of thin wood strips. Holz als Roh- Werkst. 39: 341–350, https://doi.org/10.1007/bf02608404.10.1007/BF02608404 ↗
16. Derbyshire, H., Miller, E.R., and Turkulin, H. (1997). Investigations into the photodegradation of wood using microtensile testing. Part 3: the influence of temperature on photodegradation rates. Holz als Roh- Werkst. 55: 287–292, https://doi.org/10.1007/s001070050229.10.1007/s001070050229 ↗
17. Desai, R.L. and Shields, J.A. (1969). Photochemical degradation of cellulose material. Makromol. Chem. 122: 134–144, https://doi.org/10.1002/macp.1969.021220111.10.1002/macp.1969.021220111 ↗
18. Ding, Q., Han, W., Li, X., Jiang, Y., and Zhao, C. (2020). New insights into the autofluorescence properties of cellulose/nanocellulose. Sci. Rep. 10: 21387, https://doi.org/10.1038/s41598-020-78480-2.10.1038/s41598-020-78480-2 ↗
19. Donaldson, L. (2020). Autofluorescence in plants. Molecules 25: 2393, https://doi.org/10.3390/molecules25102393.10.3390/molecules25102393 ↗
20. Evans, P.D. (2013). Weathering of wood and wood composites. In: Rowell, R.M. (Ed.), Handbook of wood chemistry and wood composites, Vol. 2. CRC Press, Boca Raton, Fla, pp. 151–216.
21. Evans, P.D., Urban, K., and Chowdhury, M.J.A. (2008). Surface checking of wood is increased by photodegradation caused by ultraviolet and visible light. Wood Sci. Technol. 42: 251, https://doi.org/10.1007/s00226-007-0175-0.10.1007/s00226-007-0175-0 ↗
22. Fengel, D. and Wegener, G. (2003). Wood: chemistry, ultrastructure, reactions. In: Reprint der Orig.-Ausg. Kessel Verlag, Remagen, pp. 345–370.
23. Firouzjaei, R.A., Minaei, S., and Beheshti, B. (2018). Sweet lemon mechanical damage detection using image processing technique and UV radiation. J. Food Meas. Char. 12: 1513–1518, https://doi.org/10.1007/s11694-018-9766-8.10.1007/s11694-018-9766-8 ↗
24. Goble, P.G., Lead, J., Baker, A., Reynolds, D.M., and Spencer, R.G.M. (2014). Aquatic organic matter fluorescence. Cambridge University Press, Cambridge, pp. 303–338.10.1017/CBO9781139045452 ↗
25. Grönroos, P., Bessonoff, M., Salminen, K., Paltakari, J., and Kulmala, S. (2018). Phosphorescence and fluorescence of fibrillar cellulose films. Nord. Pulp Pap Res. J. 33: 246–255.10.1515/npprj-2018-3030 ↗
26. Ho, K.-V., Roy, A., Foote, S., Vo, P.H., Lall, N., and Lin, C.-H. (2020). Profiling anticancer and antioxidant activities of phenolic compounds present in black walnuts (Juglans nigra) using a high-throughput screening approach. Molecules 25: 4516, https://doi.org/10.3390/molecules25194516.10.3390/molecules25194516 ↗
27. Hon, D.N.-S. and Minemura, N. (2001). Color and discoloration. In: Hon, D.N.-S. and Shiraishi, N. (Eds.), Wood and cellulosic chemistry, 2nd ed., rev. and expanded. ed. New York, NY: Dekker, pp. 385–442.10.1201/9781482269741 ↗
28. Kalkan, H., Güneş, A., Durmuş, E., and Kuşçu, A. (2014). Non-invasive detection of aflatoxin-contaminated figs using fluorescence and multispectral imaging. Food Addit. Contam. A 31: 1414–1421, https://doi.org/10.1080/19440049.2014.926398.10.1080/19440049.2014.926398 ↗
29. Kataoka, Y., Kiguchi, M., Williams, R.S., and Evans, P.D. (2007). Violet light causes photodegradation of wood beyond the zone affected by ultraviolet radiation. Holzforschung 61: 23–27, https://doi.org/10.1515/hf.2007.005.10.1515/HF.2007.005 ↗
30. Khalid, A., Zhang, L., Tetienne, J.-P., Abraham, A.N., Poddar, A., Shukla, R., Shen, W., and Tomljenovic-Hanic, S. (2019). Intrinsic fluorescence from cellulose nanofibers and nanoparticles at cell friendly wavelengths. APL Photonics 4: 20803, https://doi.org/10.1063/1.5079883.10.1063/1.5079883 ↗
31. Mao, L. and Ritcey, A.M. (1996). Excimer formation and excitation energy transfer in Langmuir-Blodgett films of cellulose derivatives containing carbazole. Thin Solid Films 284/285: 618–621, https://doi.org/10.1016/s0040-6090(95)08405-3.10.1016/S0040-6090(95)08405-3 ↗
32. Miller, R.B. (1976). Wood anatomy and identification of species of Juglans. Bot. Gaz. 137: 368–377, https://doi.org/10.1086/336886.10.1086/336886 ↗
33. Miller, R.B. and Wiemann, M.C. (2006). Separation of ‘Dalbergia nigra’ from ‘Dalbergia spruceana’. Forest Products Lab., Madison, WI, pp. 12.10.2737/FPL-RP-632 ↗
34. Mishra, G., Collings, D.A., and Altaner, C.M. (2018). Cell organelles and fluorescence of parenchyma cells in Eucalyptus bosistoana sapwood and heartwood investigated by microscopy. N. Z. J. For. Sci. 48: 13, https://doi.org/10.1186/s40490-018-0118-6.10.1186/s40490-018-0118-6 ↗
35. Mitsui, K. (2010). Acetylation of wood causes photobleaching. J. Photochem. Photobiol. B Biol. 101: 210–214, https://doi.org/10.1016/j.jphotobiol.2010.07.005.10.1016/j.jphotobiol.2010.07.005 ↗
36. Miyawaki, A. and Sakurai, H. (2020). Comprehensive approaches using luminescence to studies of cellular functions. In: Make life visible. Springer OpenSpringer, ImprintSingapore, pp. 115–124.10.1007/978-981-13-7908-6_11 ↗
37. Moya, R., Wiemann, M.C., and Olivares, C. (2013). Identification of endangered or threatened Costa Rican tree species by wood anatomy and fluorescence activity. Rev. Biol. Trop. 61: 1113–1156, https://doi.org/10.15517/rbt.v61i3.11909.10.15517/rbt.v61i3.11909 ↗
38. Müller, U., Rätzsch, M., Schwanninger, M., Steiner, M., and Zöbl, H. (2003). Yellowing and IR-changes of spruce wood as result of UV-irradiation. J. Photochem. Photobiol. B Biol. 69: 97–105.10.1016/S1011-1344(02)00412-8 ↗
39. Nagai, A., Miller, J.B., Du, J., Kos, P., Stefan, M.C., and Siegwart, D.J. (2015). Biocompatible organic charge transfer complex nanoparticles based on a semi-crystalline cellulose template. Chem. Commun. 51: 11868–11871, https://doi.org/10.1039/c5cc03822g.10.1039/C5CC03822G ↗
40. Ou, Y. and Huang, Q. (2003). Study on the photo degradation of pulp mold container. J. Appl. Polym. Sci. 87: 2052–2056, https://doi.org/10.1002/app.11392.10.1002/app.11392 ↗
41. Pandey, K.K. and Chandrashekar, N. (2006). Photostability of wood surfaces esterified by benzoyl chloride. J. Appl. Polym. Sci. 99: 2367–2374.10.1002/app.22685 ↗
42. Passauer, L., Prieto, J., Müller, M., Rössler, M., Schubert, J., and Beyer, M. (2015). Novel color stabilization concepts for decorative surfaces of native dark wood and thermally modified timber. Prog. Org. Coating 89: 314–322, https://doi.org/10.1016/j.porgcoat.2015.06.017.10.1016/j.porgcoat.2015.06.017 ↗
43. Pfanz, H., Aschan, G., Langenfeld-Heyser, R., Wittmann, C., and Loose, M. (2002). Ecology and ecophysiology of tree stems: corticular and wood photosynthesis. Naturwissenschaften 89: 147–162, https://doi.org/10.1007/s00114-002-0309-z.10.1007/s00114-002-0309-z ↗
44. Piuri, V. and Scotti, F. (2010). Design of an automatic wood types classification system by using fluorescence spectra. IEEE Trans. Syst. Man Cybern. C Appl. Rev. 40: 358–366, https://doi.org/10.1109/tsmcc.2009.2039479.10.1109/TSMCC.2009.2039479 ↗
45. Prieto, J. and Kiene, J. (2019). Holzbeschichtung: Chemie und Praxis, 2 nd, ed. Vincentz Network GmbH & Co, Hannover.10.1515/9783748601746 ↗
46. Rabek, J.F. (1996). Photodegradation of polymers: physical characteristics and applications, 1st ed. Berlin: Springer.10.1007/978-3-642-80090-0 ↗
47. Rapp, A.O. (2018). Methoden der optischen Bauforensik für die Schimmelpilzdetektion. In: Kraus-Johnsen, I. (Ed.), Schimmelpilz-Handbuch. Praxiswissen zu Schimmelpilzschäden in Gebäuden: Mikrobiologie + Gesundheit, Bautechnik + Arbeitsschutz, Versicherung, Bewertung + Recht. Bundesanzeiger Verlag, Köln, pp. 177–212.
48. Temiz, A., Terziev, N., Eikenes, M., and Hafren, J. (2007). Effect of accelerated weathering on surface chemistry of modified wood. Appl. Surf. Sci. 253: 5355–5362, https://doi.org/10.1016/j.apsusc.2006.12.005.10.1016/j.apsusc.2006.12.005 ↗
49. Tokutomi, H., Takeda, T., Hoshino, N., and Akutagawa, T. (2018). Molecular structure of the photo-oxidation product of ellagic acid in solution. ACS Omega 3: 11179–11183, https://doi.org/10.1021/acsomega.8b01716.10.1021/acsomega.8b01716 ↗
50. Tolvaj, L. and Faix, O. (1995). Artificial ageing of wood monitored by DRIFT spectroscopy and CIE lab color measurements. Holzforschung 49: 397–404, https://doi.org/10.1515/hfsg.1995.49.5.397.10.1515/hfsg.1995.49.5.397 ↗
51. Turkulin, H., Derbyshire, H., and Miller, E.R. (2004). Investigations into the photodegradation of wood using microtensile testing. Part 5-the influence of moisture on photodegradation rates. Holz als Roh- Werkst. 62: 307–312, https://doi.org/10.1007/s00107-004-0493-y.10.1007/s00107-004-0493-y ↗
52. Turkulin, H. and Živković, V. (2018). Microtensile testing of wood – influence of material properties, exposure and testing conditions on analysis of photodegradation. Drv. Ind. 69: 183–191, https://doi.org/10.5552/drind.2018.1757.10.5552/drind.2018.1757 ↗
53. Tylli, H., Forsskåhl, I., and Olkkonen, C. (1996). Photochromic behaviour of ozonated and photoirradiated cellulose studied by fluorescence spectroscopy. Cellulose 3: 203–215, https://doi.org/10.1007/bf02228802.10.1007/BF02228802 ↗
54. Wheeler, E., Baas, P., and Gasson, P.E. (1989). IAWA list of microscopic features for hardwood identification. IAWA J. 10: 219–332.10.1163/22941932-90000496 ↗
55. Ximenes, F.A. and Evans, P.D. (2006). Protection of wood using oxy-aluminium compounds. For. Prod. J. 56: 116–122.
56. Živković, V., Arnold, M., Radmanović, K., Richter, K., and Turkulin, H. (2014). Spectral sensitivity in the photodegradation of fir wood (Abies alba Mill.) surfaces: colour changes in natural weathering. Wood Sci. Technol. 48: 239–252.10.1007/s00226-013-0601-4 ↗