journal article·2002-03-01

Causes of different catalytic activities of metals in formation of single-wall carbon nanotubes

M. Yudasaka, Y. Kasuya, F. Kokai, K. Takahashi, M. Takizawa, S. Bandow, S. Iijima

Publisher page

Abstract

When single-wall carbon nanotubes (SWNTs) were formed by pulsed Nd:YAG laser ablation or arc discharge, the yield depended on the metal catalyst: NiCo> Ni∼NiFe≫Co∼Fe>Pd∼Pt. It appears that an effective catalyst for SWNT growth must satisfy three conditions: it must be a good graphitization catalyst, have low solubility in carbon, and have a stable crystallographic orientation on graphite. NiCo, Ni, and NiFe satisfy these three conditions. The poor catalytic activities of Co, Fe, Pd, and Pt for SWNT formation would be explained by the ineffectiveness of Pt and Pd as graphitization catalysts, crystallographic orientation instability of Co crystals on graphite, and high solubility of Fe in graphite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical and Alloy Processes · Advanced Materials Characterization Techniques · Chemical and Physical Properties of Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.