journal article·2021-06

Liquefaction-induced plasticity from entropy-boosted amorphous ceramics

Haidong Bian, Quanfeng He, Junhua Luan, Yu Bu, Yong Yang, Zhengtao Xu, Jian Lu, Yang Yang Li

Publisher page

Abstract

Ceramics are easy to break, and very few generic mechanisms are available for improving their mechanical properties, e.g., the 1975-discovered anti-fracture mechanism is strictly limited to zirconia and hafnia. Here we report a general mechanism for achieving high plasticity through liquefaction of ceramics. We further disclose the general material design strategies to achieve this difficult task through entropy-boosted amorphous ceramics (EBACs), enabling fracture-resistant properties that can withstand severe plastic deformation (e.g., over 95%, deformed to a thickness of a few nanometers) while maintaining high hardness and reduced modulus. The findings reported here open a new route to ductile ceramics and many applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · High Entropy Alloys Studies · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. The conflicts between strength and toughness10.1038/nmat3115 ↗
2. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
3. Toughness amplification in natural composites10.1016/j.jmps.2011.01.001 ↗
4. Layered nanocomposites inspired by the structure and mechanical properties of nacre10.1039/C1CS15106A ↗
5. Strong, tough and stiff bioinspired ceramics from brittle constituents10.1038/nmat3915 ↗
6. Fracture toughness and toughening mechanisms in graphene platelet reinforced Si3N4 composites10.1016/j.scriptamat.2012.02.009 ↗
7. Toughening in Graphene Ceramic Composites10.1021/nn200319d ↗
8. Contact-damage-resistant ceramic/single-wall carbon nanotubes and ceramic/graphite composites10.1038/nmat1161 ↗
9. CNT-reinforced ceramics and metals10.1016/S1369-7021(04)00508-5 ↗
10. Ceramic and metal matrix composites: Routes and properties10.1016/j.jmatprotec.2005.04.038 ↗
11. Effect of nano-metal particles on the fracture toughness of metal–ceramic composite10.1016/j.matdes.2012.08.065 ↗
12. The fracture toughness of Ni/Al2O3 laminates by digital image correlation I: Experimental crack opening displacement and R-curves10.1016/j.engfracmech.2005.09.005 ↗
13. Strong, tough and stiff bioinspired ceramics from brittle constituents10.1038/nmat3915 ↗
14. Synthetic nacre by predesigned matrix-directed mineralization10.1126/science.aaf8991 ↗
15. Crack-Interface Grain Bridging as a Fracture Resistance I, Mechanism in Ceramics: I, Experimental Study on Alumina10.1111/j.1151-2916.1987.tb04982.x ↗
16. Hardness and Fracture Toughness of Pressureless-Sintered Boron Carbide (B4C)10.1111/j.1151-2916.2002.tb00260.x ↗
17. Toughening of yttria-stabilised tetragonal zirconia ceramics10.1179/174328005X41113 ↗
18. Synthetic nacre by predesigned matrix-directed mineralization10.1126/science.aaf8991 ↗
19. Strong, lightweight, and recoverable three-dimensional ceramic nanolattices10.1126/science.1255908 ↗
20. Ceramic steel?10.1038/258703a0 ↗
21. Hafnia and hafnia-toughened ceramics10.1007/BF00541601 ↗
22. Transformation Toughening in ZrO2-Containing Ceramics10.1111/j.1151-2916.1987.tb04865.x ↗
23. Transformation Toughening in Zirconia-Containing Ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
24. Mechanics of Transformation-Toughening in Brittle Materials10.1111/j.1151-2916.1982.tb10426.x ↗
25. Highly ductile amorphous oxide at room temperature and high strain rate10.1126/science.aav1254 ↗
26. Anodic nanoporous SnO2 grown on Cu foils as superior binder-free Na-ion battery anodes10.1016/j.jpowsour.2015.12.118 ↗
27. TiO2 Nanotubes: Synthesis and Applications10.1002/anie.201001374 ↗
28. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
29. Mechanical and frictional behaviour of nano-porous anodised aluminium10.1016/j.matchemphys.2014.08.066 ↗
30. Spherical indentation of porous ceramics: Cracking and toughness10.1016/j.jeurceramsoc.2016.05.010 ↗
31. On the hardness and the inherent ductility of chromium carbide nanostructured coatings prepared by RF sputtering10.1016/j.jallcom.2008.07.220 ↗
32. Nanocrystalline TiN coatings with improved toughness deposited by pulsing the nitrogen flow rate10.1016/j.surfcoat.2012.04.040 ↗
33. Nanocrystalline carbide/amorphous carbon composites10.1063/1.365784 ↗
34. Magnetron sputtered hard a-C coatings of very high toughness10.1016/S0257-8972(02)00900-3 ↗
35. Kinking Nonlinear Elastic Solids, Nanoindentations, and Geology10.1103/PhysRevLett.92.255508 ↗
36. Deformation of anodic aluminum oxide nano-honeycombs during nanoindentation10.1016/j.actamat.2009.02.025 ↗
37. Observation of indentation-induced shear bands in a metal−organic framework glass10.1073/pnas.2000916117 ↗
38. Indentation fracture and toughness assessment for thin optical coatings on glass10.1088/0022-3727/40/18/S01 ↗
39. Nanostructured High-Entropy Alloys with Multiple Principal Elements: Novel Alloy Design Concepts and Outcomes10.1002/adem.200300567 ↗
40. Tuning element distribution, structure and properties by composition in high-entropy alloys10.1038/s41586-019-1617-1 ↗
41. A lightweight single-phase AlTiVCr compositionally complex alloy10.1016/j.actamat.2016.10.037 ↗
42. Full-Color Reflective Filters in a Large Area with a Wide-Band Tunable Absorber Deposited by One-Step Magnetron Sputtering10.1002/adom.201901626 ↗