Revealing the complex layered-mosaic structure of the cathode electrolyte interphase in Li-ion batteries
Source abstract
Abstract
Abstract Electrolyte decomposition on cathode surfaces is an irreversible reaction that creates a passivation layer known as the cathode electrolyte interphase (CEI). Since the CEI can lead to increased internal resistance, accelerated electrode decomposition, and loss of lithium inventory, a deeper comprehension is important for developing improved batteries. Although several models of the CEI have been proposed, the actual structure is unknown. Here we report three-dimensional tomography revealing the atomic-scale interface structure and micron-scale structure of a LiMn2O4 electrode. Atom probe tomography is employed to provide critical new information on CEI structure and composition: a complex layered-mosaic architecture is found consisting of inner homogeneous MnxOy and MnFx layers (~9nm- and ~4nm-thick) and an outer 3nm-thick mosaic structure containing a number of different inorganic and organic compounds. The results are used to develop a realistic quantitative model of the main electrochemical processes. This approach provides a new means to explore electrode systems including the effects of coatings and electrolyte additives.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Extraction and Separation Processes · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Issues and challenges facing rechargeable lithium batteries10.1038/35104644 ↗
2. Li-ion batteries: basics, progress, and challenges.10.1002/ese3.95 ↗
3. A comprehensive understanding of electrode thickness effects on the electrochemical performances of Li-ion battery cathodes10.1016/j.electacta.2012.03.161 ↗
4. Roles of surface chemistry on safety and electrochemistry in lithium ion batteries10.1021/ar200224h ↗
5. A consideration of lithium cell safety10.1016/S0378-7753(98)00240-7 ↗
6. The cathode-electrolyte interface in the Li-ion battery10.1016/j.electacta.2004.03.049 ↗
7. Surface Structure of LiMn[sub 2]O[sub 4] Electrodes10.1149/1.1432782 ↗
8. Interfaces Between Cathode and Electrolyte in Solid State Lithium Batteries: challenges and Perspectives10.3389/fchem.2018.00616 ↗
9. Study of the cathode-electrolyte interface of LiMn1.5 Ni 0.5 O4 synthesized by a sol-gel method for li-ion batteries.10.1149/1.3321710 ↗
10. Understanding the cathode electrolyte interface formation in aqueous electrolyte by scanning electrochemical microscopy10.1039/C9TA03199E ↗
11. Evolution of the LiFePO4 positive electrode interface along cycling monitored by MAS NMR10.1016/j.jpowsour.2012.08.099 ↗
12. Electrolytes and Interphases in Li-Ion Batteries and Beyond10.1021/cr500003w ↗
13. Effects of cathode electrolyte interfacial (CEI) layer on long term cycling of all-solid-state thin-film batteries10.1016/j.jpowsour.2016.05.098 ↗
14. Complementary analyses of aging in a commercial LiFePO4/graphite 26650 cell10.1016/j.electacta.2018.07.124 ↗
15. Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries
16. Electrode-Electrolyte Interface in Li-Ion Batteries: current Understanding and New Insights10.1021/acs.jpclett.5b01727 ↗
17. An, S.J. et al. The state of understanding of the lithium-ion-battery graphite solid electrolyte interphase (SEI) and its relationship to formation cycling. Carbon N. Y.105, 52–76 (2016).10.1016/j.carbon.2016.04.008 ↗
18. Review—SEI: past, Present and Future.10.1149/2.1441707jes ↗
19. Investigating the influence of high temperatures on the cycling stability of a LiNi 0.6 Co 0.2 Mn 0.2 O 2 cathode using an innovative electrolyte additive.10.1016/j.electacta.2017.03.155 ↗
20. Characterization of the Cathode Electrolyte Interface in Lithium Ion Batteries by Desorption Electrospray Ionization Mass Spectrometry10.1021/acs.analchem.6b01292 ↗
21. Electron microscopy investigations of changes in morphology and conductivity of LiFePO4/C electrodes10.1016/j.jpowsour.2015.12.119 ↗
22. Forming a Stable CEI Layer on LiNi 0.5 Mn 1.5 O 4 Cathode by the Synergy Effect of FEC and HDI10.1149/2.0211810jes ↗
23. High-voltage performance of LiCoO 2 /graphite batteries with methylene methanedisulfonate as electrolyte additive10.1016/j.jpowsour.2012.07.026 ↗
24. A TEM study of morphological and structural degradation phenomena in LiFePO4-CB cathodes10.1002/er.3575 ↗
25. Electrochemical Nature of the Cathode Interface for a Solid-State Lithium-Ion Battery: interface between LiCoO2 and Garnet-Li7La3Zr2O1210.1021/acs.chemmater.6b03870 ↗
26. Development of a new Electrochemical Impedance Spectroscopy Approach for Monitoring the Solid Electrolyte Interphase Formation10.1002/ente.201600132 ↗
27. Modeling of SEI Layer Growth and Electrochemical Impedance Spectroscopy Response using a Thermal-Electrochemical Model of Li-ion Batteries10.1149/06127.0043ecst ↗
28. On the Comparative Stability of Li and Na Metal Anode Interfaces in Conventional Alkyl Carbonate Electrolytes10.1149/2.0091513jes ↗
29. Devaraj, A. et al. Visualizing nanoscale 3D compositional fluctuation of lithium in advanced lithium-ion battery cathodes. (2015) doi:10.1038/ncomms9014.10.1038/ncomms9014 ↗
30. In Situ Atom Probe Deintercalation of Lithium-Manganese-Oxide10.1017/S1431927616012691 ↗
31. Vissers, D.R. et al. Understanding atomic scale phenomena within the surface layer of a long-term cycled 5 V spinel electrode. 297–306 (2016) doi:10.1016/j.nanoen.2015.11.031.10.1016/j.nanoen.2015.11.031 ↗
32. Dissolution, migration, and deposition of transition metal ions in Li-ion batteries exemplified by Mn-based cathodes-A critical review10.1039/C7EE03122J ↗
33. Understanding transition-metal dissolution behavior in LiNi 0.5 Mn 1.5 O 4 high-voltage spinel for lithium ion batteries.10.1021/jp405158m ↗
34. Separation of Charge Transfer and Contact Resistance in LiFePO4-Cathodes by Impedance Modeling10.1149/2.030207jes ↗
35. A Physically-Based Equivalent Circuit Model for the Impedance of a LiFePO 4 /Graphite 26650 Cylindrical Cell10.1149/2.1071709jes ↗
36. Low-voltage FIB/SEM Tomography for 3D Microstructure Evolution of LiFePO4/C Electrode10.1149/06918.0071ecst ↗
37. On porous electrodes.10.1016/0013-4686(64)85015-5 ↗
38. Theoretical and Experimental Analysis of Porous Electrodes for Lithium-Ion Batteries by Electrochemical Impedance Spectroscopy Using a Symmetric Cell10.1149/2.057207jes ↗
39. Modeling graphite anodes with serial and transmission line models10.1016/j.jpowsour.2015.02.038 ↗
40. The Impedance Response of a Porous Electrode Composed of Intercalation Particles10.1149/1.1393627 ↗
41. Effects of Nanoparticle Geometry and Size Distribution on Diffusion Impedance of Battery Electrodes10.1149/2.023301jes ↗
42. Current Collectors for Positive Electrodes of Lithium-Based Batteries10.1149/1.2039587 ↗
43. Analysis of the Interphase on Carbon Black Formed in High Voltage Batteries10.1149/2.0761507jes ↗
44. Li-Storage via Heterogeneous Reaction in Selected Binary Metal Fluorides and Oxides10.1149/1.1801451 ↗
45. Unraveling manganese dissolution/deposition mechanisms on the negative electrode in lithium ion batteries10.1039/c4cp00833b ↗
46. Graves, C. RAVDAV Data Analysis Software, Version 0.9.7. (2012).
47. E. Jones, E. Oliphant, P. Peterson, et al. Scipy: open Source Scientific Tools for Python. 2001http://www.scipy.org/.
48. The NumPy array: a structure for efficient numerical computation10.1109/MCSE.2011.37 ↗
49. A 2D graphics environment.10.1109/MCSE.2007.55 ↗
50. Contradicting geometrical concepts in pore size analysis attained with electron microscopy and mercury intrusion10.1111/j.1551-2916.2008.02736.x ↗
51. Mixtures of ionic liquid-Alkylcarbonates as electrolytes for safe lithium-ion batteries10.1016/j.jpowsour.2012.11.017 ↗
52. Comparative study on transport properties for LiFAP and LiPF6 in alkyl-carbonates as electrolytes through conductivity, viscosity and NMR self-diffusion measurements10.1016/j.electacta.2013.10.015 ↗
53. The Analysis of Electrode Impedances Complicated by the Presence of a Constant Phase Element10.1016/S0022-0728(84)80324-1 ↗
54. TauFactor: an open-source application for calculating tortuosity factors from tomographic data10.1016/j.softx.2016.09.002 ↗
55. Tutorial on the visualization of volumetric data using tomviz10.1017/S1551929517001213 ↗