Self-assembly of corrosion inhibitors-intercalated layered double hydroxides (LDHs) in cementitious systems
Source abstract
Abstract
This work investigates the self-assembly of corrosion inhibitor-intercalated layered double hydroxides (LDHs) in cementitious systems. The impacts of inorganic and organic corrosion inhibitors (i.e., sodium nitrite, sodium benzoate, and sodium molybdate) on the intercalation chemistry and chloride-induced transformation of LDHs in ordinary Portland cement (OPC) and limestone calcined clay cement (LC 3) pastes are revealed. The results show that direct admixing of inorganic or organic inhibitors results in spontaneous formation of inhibitors-intercalated LDHs (i.e., NO 2-AFm, C 6H 5COO-AFm, and MoO 4-AFm), regardless of binder chemistry. The sequestrated anodic inhibitors in cementitious systems are released upon exposure to chloride, accompanied by simultaneous formation of Friedel`s salts (Cl-AFm). The incorporation of anodic inhibitors has little influence on the chloride binding capacity of OPC and LC 3 pastes, but impacts their chloride resistance via pore structure modification. This research advances our understanding of the physicochemical roles of admixed anodic inhibitors in cementitious systems.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Layered Double Hydroxides Synthesis and Applications · Magnesium Oxide Properties and Applications · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Influence of limestone on the hydration of ternary slag cements10.1016/j.cemconres.2017.05.013 ↗
2. Aligizaki · 2014
3. Cement substitution by a combination of metakaolin and limestone10.1016/j.cemconres.2012.09.006 ↗
4. The anion exchange properties of AFm (hydrocalumite-group) minerals defined from solubility experiments and crystallographic information10.1016/j.cemconres.2020.106270 ↗
5. Investigation of the calcined kaolinite content on the hydration of Limestone Calcined Clay Cement (LC3)10.1016/j.cemconres.2018.02.016 ↗
6. Calcium nitrite corrosion inhibitor in Portland cement: influence of nitrite on chloride binding and mineralogy10.1111/j.1551-2916.2010.04362.x ↗
7. Influence of calcium nitrate and nitrite on the constitution of AFm and AFt cement hydrates10.1680/adcr.10.00002 ↗
8. The relationship between the sorption of organic compounds on cement and the retardation of hydration10.1016/0008-8846(86)90116-X ↗
9. Friedel’s salt, Ca2Al (OH) 6 (Cl, OH)· 2H2O: its solid solutions and their role in chloride binding10.1016/S0008-8846(98)00162-8 ↗
10. Limestone calcined clay cement as a low-carbon solution to meet expanding cement demand in emerging economies10.1016/j.deveng.2017.06.001 ↗
11. Multifunctional inhibition based on layered double hydroxides to comprehensively control corrosion of carbon steel in concrete10.1016/j.corsci.2017.06.026 ↗
12. Hydrotalcite-type anionic clays: Preparation, properties and applications10.1016/0920-5861(91)80068-K ↗
13. Sequestration and release of nitrite and nitrate in alkali-activated slag: a route toward smart corrosion control10.1016/j.cemconres.2021.106398 ↗
14. Chloride binding of synthetic Ca-Al-NO3 LDHs in hardened cement paste10.1016/j.conbuildmat.2015.05.047 ↗
15. Impact of admixtures on the hydration kinetics of Portland cement10.1016/j.cemconres.2011.03.005 ↗
16. Effect of corrosion inhibiting admixtures on concrete properties10.1016/j.conbuildmat.2004.04.001 ↗
17. Mechanical properties and durability performance of concretes with Limestone Calcined Clay Cement (LC3)10.1016/j.cemconres.2018.02.005 ↗
18. Second pilot production of limestone calcined clay cement in India: the experience
19. Hydration of a belite-calcium sulfoaluminate-ferrite cement: Aether TM
20. Infrared and Raman spectral studies in cement and concrete10.1016/0008-8846(80)90005-8 ↗
21. Thermodynamic properties and thermal behavior of Friedel’s salt10.1016/j.tca.2013.07.030 ↗
22. ATR-FTIR and XPS study on the structure of complexes formed upon the adsorption of simple organic acids on aluminum hydroxide10.1016/S1001-0742(07)60073-4 ↗
23. Preparation and characterization of nanocontainers of corrosion inhibitor based on layered double hydroxides10.1016/j.clay.2012.07.004 ↗
24. Determining cement composition by Fourier transform infrared spectroscopy10.1016/1065-7355(94)00031-X ↗
25. Cement hydration and microstructure formation in the presence of water-soluble polymers10.1016/j.cemconres.2008.10.003 ↗
26. The influence of limestone and Al2O3 content in the slag on the performance of the composite cements10.1016/j.proeng.2015.06.164 ↗
27. Uptake and retention of molybdenum in cementitious systems10.1016/j.apgeochem.2020.104630 ↗
28. Effect of MgO, Mg-Al-NO3 LDH and calcined LDH-CO3 on chloride resistance of alkali activated fly ash and slag blends10.1016/j.conbuildmat.2020.118865 ↗
29. Effect of alkalis on fresh C–S–H gels. FTIR analysis10.1016/j.cemconres.2009.01.003 ↗
30. Influence of limestone on the hydration of Portland cements10.1016/j.cemconres.2008.01.002 ↗
31. Removal of chloride ion from aqueous solution by ZnAl-NO3 layered double hydroxides as anion-exchanger10.1016/j.jhazmat.2008.04.114 ↗
32. Limitations of the hydrotalcite formation in Portland composite cement pastes containing dolomite and metakaolin10.1016/j.cemconres.2017.11.007 ↗
33. Performance of Limestone Calcined Clay Cement (LC 3) with various kaolinite contents with respect to chloride transport10.1617/s11527-018-1255-3 ↗
34. Thermodynamic and crystallographic model for anion uptake by hydrated calcium aluminate (AFm): an example of molybdenum10.1038/s41598-018-26211-z ↗
35. The AFm phase in Portland cement10.1016/j.cemconres.2006.10.010 ↗
36. Crystal structure of Kuzel’s salt 3CaO•Al2O 3•1/2CaSO4•1/2CaCl2•11H 2O determined by synchrotron powder diffraction10.1016/j.cemconres.2011.01.015 ↗
37. Relationship between free chloride and total chloride contents in concrete10.1016/S0008-8846(03)00065-6 ↗
38. Nedyalkova · 2017
39. Chloride diffusion in limestone flash calcined clay cement concrete
40. Study of the hydration mechanism and formation of new hydrates applying organic additives to the aluminate phase of cement
41. Mineralogy and crystal chemistry of calcium aluminate cement
42. Hybrid derivatives of layered double hydroxides10.1016/S0169-1317(00)00025-9 ↗
43. Relationship between the particle size and dosage of LDHs and concrete resistance against chloride ingress10.1016/j.cemconres.2018.01.005 ↗
44. Layered double hydroxide-like materials: nanocomposites for use in concrete10.1016/j.cemconres.2004.05.012 ↗
45. Thermal behaviour of the nitrated AFm phase Ca4Al2 (OH) 12 (NO3) 2• 4H2O and structure determination of the intermediate hydrate Ca4Al2 (OH) 12 (NO3) 2• 2H2O10.1016/S0008-8846(99)00251-3 ↗
46. Effect of admixture on cement hydration kinetics by synchrotron XRD and isothermal calorimetry
47. Calcined clay limestone cements (LC3)10.1016/j.cemconres.2017.08.017 ↗
48. Scrivener · 2018
49. Durability of Portland cement blends including calcined clay and limestone: interactions with sulfate, chloride and carbonate ions
50. Corrosion inhibitors for steel in concrete: State-of-the-art report10.1016/j.conbuildmat.2006.10.013 ↗
51. Tailoring hybrid layered double hydroxides for the development of innovative applications10.1002/adfm.201703868 ↗
52. Taylor · 1997
53. Assessment of sodium molybdate as an accelerator of cement hydration and setting10.1680/adcr.1989.2.7.89 ↗
54. Electrical resistivity of partially-saturated alkali-activated slag containing sodium nitrite admixture10.1016/j.cemconcomp.2021.104053 ↗
55. On the use of limestone calcined clay cement (LC3) in high-strength strain-hardening cement-based composites (HS-SHCC)10.1016/j.cemconres.2021.106421 ↗
56. The dynamics of capillary flow10.1103/PhysRev.17.273 ↗
57. Study of the system CaO–Al2O3–H2O at temperatures of 21 and 90 C10.6028/jres.030.027 ↗
58. Chloride removal and corrosion inhibitions of nitrate, nitrite-intercalated Mg–Al layered double hydroxides on steel in saturated calcium hydroxide solution10.1016/j.clay.2018.07.023 ↗
59. Laboratory investigation of the influence of two types of modified hydrotalcites on chloride ingress into cement mortar10.1016/j.cemconcomp.2014.12.016 ↗
60. The effect of two types of modified Mg-Al hydrotalcites on reinforcement corrosion in cement mortar10.1016/j.cemconres.2017.06.004 ↗
61. Characterization and adaptability of layered double hydroxides in cement paste10.1016/j.clay.2021.106197 ↗
62. Autogenous formation and smart behaviors of nitrite- and nitrate-intercalated layered double hydroxides (LDHs) in Portland cement-metakaolin-dolomite blends10.1016/j.cemconres.2020.106267 ↗
63. Influence of nitrate corrosion inhibitors on phase stability of alkali-activated slag against chloride binding and natural carbonation10.1061/(ASCE)MT.1943-5533.0002830 ↗
64. Chloride ingress profiles and binding capacity of mortar in cyclic drying-wetting salt fog environments10.1016/j.conbuildmat.2016.10.059 ↗
65. A review of the mechanisms of set-retardation in Portland cement pastes containing organic admixtures10.1016/0008-8846(72)90057-9 ↗
66. Structure of calcium silicate hydrate (C-S-H): Near-, Mid-, and Far-infrared spectroscopy10.1111/j.1151-2916.1999.tb01826.x ↗
67. The reaction between metakaolin and limestone and its effect in porosity refinement and mechanical properties10.1016/j.cemconres.2020.106307 ↗