In situ Zn/ZnO mapping elucidating for “shape change” of zinc electrode
Source abstract
Abstract
For the use of the zinc anode in secondary batteries, it is necessary to solve the “shape change” deterioration issue in that zinc species agglomerate in the center of the electrode to fade the available capacity. The local chemical compositions of the zinc electrodes during “shape change” were precisely analyzed using the synchrotron X-ray diffraction mapping analysis of practical zinc-nickel cells in a non-destructive manner. The in situ Zn/ZnO mapping shows that metallic Zn deposition chiefly occurs in the periphery of ZnO while ZnO are left in the center of electrode like a hill on charging. On discharging, the ZnO hill grows to the perpendicular direction on the electrode while metallic zinc is oxidized and dissolved. These findings allow us to propose a mechanism for the shape change; thus dissolved zincate species are decomposed on the ZnO hill during discharging to be accumulated in the center of the electrode. It is suggested that suppressing zincate dissolution and non-uniform zinc deposition slow the growth rate of the ZnO hill to enhance the cyclability of zinc-based secondary batteries.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced battery technologies research · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Office of Society-Academia Collaboration for Innovation, Kyoto University 1 , Gokasho, Uji 611-0011, Japan
Graduate School of Human and Environmental Studies, Kyoto University 2 , Yoshida-nihonmatsu-cho, Sakyo-ku, Kyoto 606-8501, Japan
References (26)
Show source-provided references
1. High energy density metal-air batteries: A review10.1149/2.062310jes ↗
2. Rechargeable batteries with aqueous electrolytes10.1016/s0013-4686(00)00344-3 ↗
3. Rechargeable zinc batteries10.1016/0368-1874(84)87113-0 ↗
4. The secondary alkaline zinc electrode10.1149/1.2085653 ↗
5. Nickel/zinc batteries10.1016/0378-7753(94)01954-1 ↗
6. Modeling of an electrically rechargeable alkaline Zn-air battery10.1016/s0013-4686(02)00316-x ↗
7. Methods for the reduction of shape change and dendritic growth in zinc-based secondary cells10.1016/0378-7753(91)80117-g ↗
8. Visual observations of early shape changes in a zinc/nickel oxide cell10.1149/1.2048533 ↗
9. Effects of KOH concentration on the shape change and cycle life of Zn/NiOOH cells10.1149/1.2108327 ↗
10. Zinc electrode shape change: I. In situ monitoring10.1149/1.2085538 ↗
11. Zinc electrode shape change: II. Process and mechanism10.1149/1.2085582 ↗
12. Zinc electrode shape change in secondary cells10.1149/1.2404060 ↗
13. The effect of additives on current distribution in pasted zinc electrodes10.1149/1.2119488 ↗
14. Mathematical analysis of a Zn/NiOOH cell10.1149/1.2120009 ↗
15. Current density and ZnO precipitation-dissolution distributions in Zn-ZnO porous electrodes and their effect on material redistribution: A two-dimensional mathematical model10.1149/1.2086856 ↗
16. In situ microtomographic monitoring of discharging processes in alkaline cells10.1149/1.3294566 ↗
17. Visualization of charge distribution in a lithium battery electrode10.1021/jz100634n ↗
18. Transformation of leaf-like zinc dendrite in oxidation and reduction cycle10.1016/j.electacta.2015.03.076 ↗
19. The behavior of the zinc electrode in alkaline solutions V. Supersaturated zincate solutions10.1149/1.2127654 ↗
20. Effect of polyaniline coating on “shape change” phenomenon of porous zinc electrode10.1149/1.2008992 ↗
21. Study of alkaline solutions of zinc oxide10.1021/ja01652a041 ↗
22. 2009
23. Engineering analysis of shape change in zinc secondary electrodes: I. Theoretical10.1149/1.2132657 ↗
24. Engineering analysis of shape change in zinc secondary electrodes: II. Experimental10.1149/1.2132658 ↗
25. Supersaturated zincate solutions: A study of the decomposition kinetics10.1149/1.2086013 ↗
26. Preserving zinc electrode morphology in aqueous alkaline electrolytes mixed with highly concentrated organic solvent10.1149/2.0091602jes ↗