Effects of Compressive Deformation on Wettability and Water Uptake Behavior of Poplar
Source abstract
Abstract
Abstract Wood compression is a method of increasing the density and stiffness of wood. Using heat (thermal compression) or impregnating wood with various resins can also increase its dimensional stability. Compressed wood can be used as a structural component in buildings, but it generally must be painted to improve its durability. The objective of this research was to investigate the surface wettability and water uptake behavior of compressed poplar wood with and without melamine-formaldehyde resin impregnation in order to be able to predict the behavior of resins or paints on surfaces of compressed wood. Samples of poplar wood were pressed both in the presence of resin and without resin at 180°C for 30 minutes under different pressures (0 to 8 MPa). Compression ratios were 10, 20, and 50 percent, depending on the pressure. Results indicate that the surface contact angle of the compressed wood, without resin, increased as the compression ratio increased. The water absorption of compressed wood, without resin, was much higher than that of the compressed wood with resin treatment. Also, the amount of absorbed water in the direction of the grain was greater than that in the perpendicular-to-grain direction for both compressed wood samples.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Tree Root and Stability Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Bekhta, P., S. Hiziroglu, and O. Shepelyuk. 2009. Properties of plywood manufactured from compressed veneer as building material. Mater. Design30(4):947–953.
2. Blomberg, J. and B. Persson. 2004. Plastic deformation in small clear pieces of Scots pine (Pinus sylvestris) during densification with the CaLignum process. J. Wood Sci. 50(4):307–314.
3. Garcia, R. A., A. Cloutier, and B. Riedl. 2006. Chemical modification and wetting of medium density fibreboard panels produced from fibres treated with maleated polypropylene wax. Wood Sci. Technol. 40(5):402–416.
4. Inoue, M., S. Ogata, S. Kawai, R. M. Rowell, and M. Morimoto. 1993. Fixation of compressed wood using melamine-formaldehyde resin. Wood Fiber Sci. 25(4):404–410.
5. Kutnar, A., F. A. Kamke, M. Petric, and M. Sernek. 2008. The influence of viscoelastic thermal compression on the chemistry and surface energetics of wood. Colloids Surf. A Physicochem. Eng. Aspects329:82–86.
6. Kutnar, A., F. A. Kamke, and M. Sernek. 2009. Density profile and morphology of viscoelastic thermal compressed wood. Wood Sci. Technol. 43(1):57–68.
7. Pétrissans, M., P. Gérardin, I. Elbakali, and M. Serraj. 2003. Wettability of heat-treated wood. Holzforschung57(3):301–307.
8. Ryu, J. Y., Y. Imamura, M. Takahashi, and H. Kajita. 1993. Effects of molecular weight and some other properties of resins on the biological resistance of phenolic resin treated wood. Mokuzai Gakkaishi39(4):486–492.
9. Sekino, N., M. Inoue, and M. Irle. 1997. Thickness swelling and internal bond strength in particleboard made from steam-pretreated particles. Mokuzai Gakkaishi43(12):1009–1015.
10. Shams, M. I., N. Kagemori, and H. Yano. 2006 a. Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin IV: Species dependency. J. Wood Sci. 52(2):179–183.
11. Shams, M. I., T. Morooka, and H. Yano. 2006 b. Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin V: Effects of steam pretreatment. J. Wood Sci. 52(5):389–394.
12. Shams, M. I. and H. Yano. 2004. Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin II: Effects of processing parameters. J. Wood Sci. 50:343–350.
13. Shams, M. I., H. Yano, and K. Endou. 2004. Compressive deformation of wood impregnated with low molecular weight phenol formaldehyde (PF) resin I. Effects of pressing pressure and pressure holding. J. Wood Sci. 50:337–342.
14. Tjeerdsma, B. F. and H. Militz. 2005. Chemical changes in hydrothermal treated wood: FTIR analysis of combined hydrothermal and dry heat-treated wood. Holz Roh- Werkst. 63:101–111.
15. Tze, W. T. and D. J. Gardner. 2001. Contact angle and IGC measurements for probing surface-chemical changes in the recycling of wood pulp fibers. J. Adhes. Sci. Technol. 15:223–241.
16. Yoshihara, H. and S. Tsunematsu. 2007 a. Bending and shear properties of compressed Sitka spruce. Wood Sci. Technol. 41(2):117–131.
17. Yoshihara, H. and S. Tsunematsu. 2007 b. Elastic properties of compressed spruce with respect to its cross section obtained under various compression ratios. Forest Prod. J. 57(4):98–100.
18. Zhang, Y., J. Jin, and S. Wang. 2007. Effects of resin and wax on the water uptake behaviour of wood strands. Wood Fiber Sci. 39(2):271–278.