journal article·2013-03

Improved Coating Performance on Wood Treated with Carbon-Based Preservatives and an Ultraviolet/Visible Light Protective Precoat

Rod Stirling, Paul I. Morris

Forest Products Journal· Volume 63· Issue 3-4
Publisher page

Abstract

Abstract Transparent and semitransparent coatings applied to wood products often fail due to photochemical degradation and colonization by black stain fungi. Longer-lasting coatings are needed to enhance the competitiveness of wood products used in appearance applications. We hypothesized that shell treatment with carbon-based wood preservatives combined with a protective precoat containing organic ultraviolet (UV) absorbers and hindered amine light stabilizers would control black stain fungi and provide enhanced coating service life. After 3 years of field exposure at Maple Ridge, British Columbia, and Saucier, Mississippi, samples were evaluated for degree of black stain, coating degradation, and substrate damage. Heartwood substrate, preservative treatment, and use of protective precoats were associated with better stain resistance and enhanced coating performance. Use of preservative treatments and UV protective precoats is recommended to enhance the service life of high-quality transparent and semitransparent finishes. However, further work is needed to enhance the performance of transparent and semitransparent coatings to meet consumer demands for low maintenance.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Forest ecology and management · Forest Biomass Utilization and Management

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. American Society for Testing and Materials (ASTM). 1986. Standard method for evaluating degree of flaking (scaling) of exterior paints. ASTM D772‐86. ASTM, West Conshohocken, Pennsylvania.
2. American Society for Testing and Materials (ASTM). 1988a. Standard method for evaluating degree of cracking of exterior paints. ASTM D661‐88. ASTM, West Conshohocken, Pennsylvania.
3. American Society for Testing and Materials (ASTM). 1988b. Standard method for evaluating degree of surface disfigurement of paint films by microbial (fungal and algal) growth or dirt accumulation. ASTM D3274‐88. ASTM, West Conshohocken, Pennsylvania.
4. American Society for Testing and Materials (ASTM). 1993a. Standard method for evaluating degree of checking of exterior paints. ASTM D660‐93. ASTM, West Conshohocken, Pennsylvania.
5. American Society for Testing and Materials (ASTM). 1993b. Standard method for evaluating degree of erosion of exterior paints. ASTM D662‐93. ASTM, West Conshohocken, Pennsylvania.
6. Blanchard, V. and P. Blanchet. 2011. Color stability for wood products during use: Effects of inorganic nanoparticles. BioResources6(2):1219–1229.
7. Blanchard, V. and R. Stirling. 2013. Technical note: Plasma pretreatment enhanced field performance of exterior wood coatings. Wood Fiber Sci. 45(2):228–231.
8. Butler, M. and A. Day. 1998. Fungal melanins: A review. Can. J. Microbiol. 44(12):1115–1136.
9. Clausen, C. A. 2010. Biodeterioration of wood. In:Wood Handbook—Wood as an Engineering Material. General Technical Report FPL-GTR-190. USDA Forest Service, Forest Products Laboratory, Madison, Wisconsin. pp. 14‐1–14‐16.
10. Duncan, C. G. 1963. Role of microorganisms in weathering of wood and degradation of exterior finishes. Off. Dig. J. Paint Technol. Eng. 35(465):1003–1012.
11. Evans, P. D. 2009. Review of the weathering and photostability of modified wood. Wood Mater. Sci. Eng. 4(1–2):2–13.
12. Evans, P. D., S. K. Gibson, I. Cullis, C. Liu, and G. Sèbe. 2013. Photo stabilization of wood using low molecular weight phenol formaldehyde resin and hindered amine light stabilizer. Polym. Degrad. Stab. 98(1):158–168.
13. Feist, W. C. 1984. The role of water repellents and chemicals in controlling mildew on wood exposed outdoors. Research Note FPL-0247. USDA Forest Service, Forest Products Laboratory, Madison, Wisconsin. 15 pp.
14. Feist, W. C. 1988 a. Weathering performance of finished southern pine plywood siding. Forest Prod J. 38:22–28.
15. Feist, W. C. 1988 b. Role of pigment concentration in the weathering of semitransparent stains. Forest Prod. J. 38:41–44.
16. Forsthuber, B. and G. Grüll. 2010. The effects of HALS in the prevention of photo-degradation of acrylic clear topcoats and wooden surfaces. Polym. Degrad. Stab. 95:746–755.
17. Forsthuber, B., C. Schaller, and G. Grüll. 2013. Evaluation of the photo stabilising efficacy of clear coatings comprising organic UV absorbers and mineral UV screeners on wood surfaces. Wood Sci. Technol. 47:281–297.
18. French, D. W. 1977. Preservative stains as exterior wood finishes. IRG/WP/77‐389. International Research Group on Wood Preservation, Stockholm. 12 pp.
19. George, B., E. Suttie, A. Merlin, and X. Deglise. 2005. Photodegradation and photostabilization of wood—The state of the art. Polym. Degrad. Stab. 88:268–274.
20. Gobakken, L. R. and K. M. Jenssen. 2007. Growth and succession of mould on commercial paint systems in two field sites. IRG/WP/07‐30421. International Research Group on Wood Protection, Stockholm. 12 pp.
21. Hayoz, P., W. Peter, and D. Rogez. 2003. A new innovative stabilization method for the protection of natural wood. Prog. Organic Coat. 48:297–309.
22. Hennon, P., B. Woodward, and P. Lebow. 2007. Deterioration of wood from live and dead Alaska yellow-cedar in contact with soil. Forest Prod. J. 57(6):23–30.
23. Kataoka, Y., M. Kiguchi, R. S. Williams, and P. D. Evans. 2007. Violet light causes photodegradation of wood beyond the zone affected by ultraviolet light. Holzforschung61(1):23–27.
24. Kiguchi, M., Y. Karaoke, P. D. Evans, Y. Kadegaru, and Y. Imamura. 2001. Pretreatments of wood surfaces for improving weatherability of clear finishing. IRG/WP/01‐40196. International Research Group on Wood Preservation, Stockholm. 11 pp.
25. Knopf, F. W., J. Sell, and W. C. Feist. 1994. Comparative weathering tests of North American and European exterior wood finishes. Forest Prod. J. 44(10):33–41.
26. Liu, C., A. Ahniyaz, and P. D. Evans. 2010. Preliminary observations of the photostabilization of wood surfaces with cerium oxide nanoparticles. IRG/WP 10‐40504. International Research Group on Wood Protection, Stockholm. 8 pp.
27. Morris, P. I., J. Ingram, P. Laks, and G. Larkin. 2011. Field tests of naturally durable species. Forest Prod. J. 61(5):344–351.
28. Morris, P. I. and S. M. McFarling. 2006. Enhancing the performance of transparent coatings by UV protective pretreatments. IRG/WP/06‐30399. International Research Group on Wood Protection, Stockholm. 12 pp.
29. Nejad, M. and P. Cooper. 2011. Exterior wood coatings. Part 1: Performance of semitransparent stains on preservative-treated wood. J. Coat. Technol. Res. 8:449–458.
30. Ross, A. and W. C. Feist. 1993. The effects of CCA-treated wood on the performance of surface finishes. Am. Paint Coat. J. 78:41–54.
31. Rothstein, E. C. 1967. Compatibility and reactivity of UV absorbers in clear wood coatings. J. Paint Technol. 39(513):621–628.
32. Sandberg, K. 2008. Degradation of Norway spruce (Picea abies) heartwood and sapwood during 5.5 years' above-ground exposure. Wood Mater. Sci. Eng. 3(3–4):83–93.
33. Schaller, C. and D. Rogez. 2007. New approaches in wood coating stabilization. J. Coat. Technol. Res. 4(4):401–409.
34. Schaller, C., D. Rogez, and A. Braig. 2008. Hydroxyphenyl-s-triazines: Advanced multipurpose UV-absorbers for coatings. J. Coat. Technol. Res. 5(1):25–31.
35. Schauwecker, C. F., A. G. MacDonald, and J. J. Morrell. 2012. Performance of wood treated with prospective organic surface protectants upon outdoor exposure: FTIR spectroscopic analysis of weathered surfaces. Holzforschung67(2):227–235.
36. Schoeman, M. W. and D. J. Dickinson. 1996. Aureobasidium pullulans can utilize simple aromatic compounds as a sole source of carbon in liquid culture. Lett. Appl. Microbiol. 22:129–131.
37. Schoeman, M. W. and J. D. Lloyd. 1999. The role of boron-based additives in exterior wood coatings. Surf. Coat. Int. 82(3):124–126.
38. Seifert, K. 1964. Changes of the chemical wood components by the blue rot Pullularia pullulans (de Bary) Berkhout (=Aureobasidium pullulans (de Bary) Arnaud). Holz Roh- Werkst. 22(11):405–409.
39. Sell, J. and O. Wälchli. 1974. Investigations on weathered wood surfaces. Part VI. Mold prevention of fungicidal additives added to impregnating paints. Holz Roh- Werkst. 32:463–465.
40. Sharpe, P. R. and D. J. Dickinson. 1993. Blue stain in service on wood surfaces. Part 3. The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings. IRG/WP/93v10035. International Research Group on Wood Preservation, Stockholm. 10 pp.
41. Stirling, R. and P. I. Morris. 2013. Performance of coatings on wood treated with carbon-based preservatives. IRG/WP 13‐40638. International Research Group on Wood Protection, Stockholm. 11 pp.
42. Stirling, R., A. Uzunovic, and P. I. Morris. 2011. Control of black stain fungi with biocides in semitransparent wood coatings. Forest Prod. J. 61 (5):359–364.