Correction: Graphene‐Confined Sn Nanosheets with Enhanced Lithium Storage Capability
Source abstract
Abstract
Also, the sentences “The first discharge and charge steps (Figure S6) deliver a specific discharge capacity of 1380 mAh g−1 for G/Sn/G, 1013 mAh g−1 for G-Sn@C, and 1572 mAh g−1 for G-Sn electrodes, with initial Coulombic efficiencies of 66.5%, 65.6%, and 64.8%, respectively.” on page 3541 should be “The first discharge and charge steps (Figure S6) deliver a specific discharge capacity of 1380 mAh g−1 for G/Sn/G, 1013 mAh g−1 for G-Sn@C, and 1637 mAh g−1 for G-Sn electrodes, with initial Coulombic efficiencies of 66.5%, 65.6%, and 61%, respectively.” The corresponding first discharge and charge curves (Figure S6) and the thermal gravimetric analysis data (Figure S2) for the control sample (G-Sn) are shown in the Supporting Information for this correction which is available from the Wiley Online Library or from the author. The arguments and conclusions of the original article are not affected. The authors apologize for any inconvenience caused.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Technologies Research · Graphene research and applications · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.