Abstract One of the failure modes of ductile structural elements undergoing repeated thermal loading is incremental collapse caused by strain accumulation. Another failure mode typical for such loading is the stable growth of long cracks, with the crack being able to achieve the size of thermal tension zone movement. The impact of general incremental deformation accumulation on cyclic crack growth under repeated thermal actions is studied in this paper. The computational interpretation of the experiment shows that the static damage resulted from overall incremental deformation accumulation exceeds the fatigue one caused by reversed plasticity. This fact proves that under severe thermal ratchetting a crack can be driven mostly by a quasistatic opening produced by the strain accumulated within a body rather than by fatigue.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · High Temperature Alloys and Creep · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Gokhfeld · 1980
2. Shakedown analysis of defective pressure vessels by a kinematic approach10.1007/s004190050254 ↗
3. A method for the evaluation of a ratchet limit and the amplitude of plastic strain for bodies subjected to cyclic loading10.1016/S0997-7538(01)01162-7 ↗
4. Thermal ratchetting deformation of a 316L stainless steel cylindrical structure under an axial moving temperature distribution10.1016/S0308-0161(02)00136-9 ↗
5. Modes of long crack growth under non-stationary temperature fields10.1016/j.nucengdes.2011.10.003 ↗
6. Crack growth under moving temperature field by the example of circumferential crack in steel cylinder specimen10.1115/1.2937743 ↗
7. Plastic limit loads of defective pipes under combined internal pressure and axial tension10.1016/S0020-7403(02)00025-5 ↗
8. Limit analysis of cracked structures by mathematical programming and finite element technique10.1007/s004660050455 ↗
9. Ratchetting limits for cracked bodies subjected to cyclic loads and temperatures10.1016/j.engfracmech.2004.12.003 ↗
10. Simulation of ratcheting and low cycle fatigue10.1016/j.ijpvp.2004.01.002 ↗
11. Timoshenko · 1959
12. ABAQUS User’s manual, version 6.2, 2001.
13. A two parameter driving force for fatigue crack growth analysis10.1016/j.ijfatigue.2005.07.002 ↗
14. Singular and non-singular approaches for predicting fatigue crack growth behavior10.1016/j.ijfatigue.2005.07.018 ↗
15. Mathematical modeling of the damage accumulation and crack propagation processes under low cycle loading
16. Mahutov · 1981
17. Singular behavior at the end of a tensile crack in a hardening material10.1016/0022-5096(68)90014-8 ↗
18. Plane strain deformation near a crack tip in a power law hardening material10.1016/0022-5096(68)90013-6 ↗