Failure analysis of oil refinery heater treater’s fractured fire tube
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Bakhtiari · Fitness for Service Assessment of a Pressure Vessel Subjected to Fire Damage in a Refinery Unit. · 2017 · 80 · 444
2. Zangeneh · Thermal/stress Analysis of a Failed Fire-Tube Heater Treater. · 2020 · 116 · 104762
3. Improving the Efficiency of Oil Treating and Refining Processes (Review)10.1134/S0965544120110092 ↗
4. Lei · Failure Analysis of Weld Cracking in a Thick-Walled 2.25 Cr-1Mo Steel Pressure Vessel. · 2014 · 23 · 1231
5. Effect of tempering time on mechanical and fracture behavior of SA 387 Gr
6. Performance degradation detection of 12CrMoV steel by magneto-acoustic compound inspection method10.1016/j.ndteint.2021.102525 ↗
7. Nondestructive evaluation of macro segregation in creep strength enhanced 9Cr–1Mo–V–Nb steel10.1016/j.scriptamat.2020.07.039 ↗
8. Comparative study on girth weld-induced residual stresses between austenitic and duplex stainless steel pipe welds10.1016/j.applthermaleng.2013.11.001 ↗
9. Zhang · Welding Residual Stress in a Large Diameter Nuclear Reactor Pressure Vessel Nozzle. · 2013 · 135
10. Pramanick · Failure Investigation of Super Heater Tubes of Coal Fired Power Plant. · 2017 · 9 · 17
11. Failure analysis: Sulfur stress corrosion cracking of S30432 stainless steel in the final super-heater10.1016/j.engfailanal.2020.104859 ↗
12. N. Parnian Failure analysis of austenitic stainless steel tubes in a gas fired steam heater. Materials & Design (1980-2015), 2012. 36 788 795 10.1016/j.matdes.2011.12.027.10.1016/j.matdes.2011.12.027 ↗
13. Advanced approach of reactor pressure vessel in-service inspection
14. Structural features of cast refractory alloy HP40NbTi high-temperature oxidation. Part 2
15. A. Assefinejad et al. Failure Investigation of Water Wall Tubes in a Drum Boiler of a Thermal Power Plant. 118 2020 104869 10.1016/j.engfailanal.2020.104869.10.1016/j.engfailanal.2020.104869 ↗
16. Experimental in-situ metallographic investigations of industrial hydrocarbon processed fired heater tubes10.1051/metal/2018062 ↗
17. M. Xu et al. Fractal and Probability Analysis of Creep Crack Growth Behavior in 2.25 Cr–1.6 W Steel Incorporating Residual Stresses. 359 2015 73 81 10.1016/j.apsusc.2015.10.063.10.1016/j.apsusc.2015.10.063 ↗
18. S. Paddea et al. Residual Stress Distributions in a P91 Steel-Pipe Girth Weld before and after Post Weld Heat Treatment. 534 2012 663 672 10.1016/j.msea.2011.12.024.10.1016/j.msea.2011.12.024 ↗
19. Rampat · Creep Embrittlement in Aged HP-Mod Alloy Reformer Tubes. · 2019 · 100 · 147
20. Hosseini · Failure Analysis of Boiler Tube at a Petrochemical Plant. · 2019 · 106 · 104146
21. On the elemental impact factor, a method to determine an alloy’s compositional influences upon phase stability and metallurgical material properties10.3390/ma13245747 ↗
22. Tachibana · Material and Fabrication of the HTTR Reactor Pressure Vessel. · 1997 · 305
23. A review of factors affecting the structural integrity of weldments in heavy wall reactor vessels10.1179/cmq.1989.28.1.75 ↗
24. Canale, L.d.C.F., G.E. Totten, and R.A. Mesquita, Failure analysis of heat treated steel components. 2008: ASM international, https://books.google.com/books.10.31399/asm.tb.fahtsc.9781627082846 ↗
25. Ibrahim, S.E.J.J.o.F.A. and Prevention, Impact of Short Operational Cycles on Cladding Materials in Coke Drums. 2023: p. 1-8, , https://doi.org/10.1007/s11668-023-01609-8.10.1007/s11668-023-01609-8 ↗
26. Zangeneh, S., et al., Failure Analysis of A213 TP347H Superheater Outlet Tube in A 320-MW Power Plant. 2022: p. 1-11, https://doi.org/10.1007/s11668-022-01474-x.10.1007/s11668-022-01474-x ↗
27. Pour saeidi, E., M. Aieneravaie, and M.M. Arhani, Failure Analysis of a 9–12% Cr Steel Superheater Tube. v,131: p.061401, 2009, https://doi.org/10.1115/1.3147982.10.1115/1.3147982 ↗
28. Failure analysis of a reheater tube dissimilar metal weld failure in a 500 MW power plant10.1016/j.engfailanal.2020.104851 ↗
29. Premature failure of superheater tubes in a fertilizer plant10.1016/j.engfailanal.2020.105152 ↗
30. Failure analysis of superheater tubes in an air quenching cooler waste heat boiler10.1016/j.engfailanal.2021.105869 ↗
31. Zhang · The Effect of Joint Configuration on Residual Stress and Distortion of the 304 Stainless Steel Multi-Pass Welded Joints. · 2022 · 30 · 103070
32. Siefert, J., J.J.I.J.o.P.V. Parker, and Piping, Evaluation of the creep cavitation behavior in Grade 91 steels. 2016. 138: p. 31-44 , https://doi.org/10.1016/j.ijpvp.2016.02.018.10.1016/j.ijpvp.2016.02.018 ↗
33. S.P. Rajan et al. An Investigation on SA 213-Tube to SA 387-Tube Plate Using Friction Welding Process. 30 2016 337 344 10.1007/s12206-015-1238-z.10.1007/s12206-015-1238-z ↗
34. A.C.S. Silva et al. Applied Methodology for Qualification of Welding Procedures of Industrial Pipes According to ASME B 31.3 and ASME SECTION IX. p 2019 24 10.1590/0104-9224/SI24.23.
35. Boiler, A. and P.V.J.A. Code, New York, section IX. 1968 p.115-116, https://www.asme.org/shop/certification‐accreditation.
36. Fuentes · Premature Fracture in Automobile Leaf Springs. · 2009 · 16 · 648
37. Francis · Welding Residual Stresses in Ferritic Power Plant Steels. · 2007 · 23 · 1009
38. Temper embrittlement and corrosion behaviour of martensitic stainless steel 420
39. Role of carbides in tempered martensite embrittlement10.1179/mst.1989.5.2.138 ↗
40. A review of underlying reasons for intergranular cracking for a variety of failure modes and materials and examples of case histories10.1016/j.engfailanal.2019.02.027 ↗
41. Microstructural analysis of candidate steels pre-selected for new advanced reactor systems10.1016/j.jnucmat.2007.01.068 ↗
42. Effect of prior-austenite grain refinement on microstructure, mechanical properties and thermal embrittlement of 9Cr-1Mo-0.1 C steel10.1016/j.jnucmat.2017.07.019 ↗
43. Imgram · Pressure Vessel, Piping, and Welding Needs for Coal Conversion Systems. · 1985 · 7 · 212
44. Wang · Fatigue Performance of Friction Stir Welded Weathering Mild Steels Joined below A1 Temperature. · 2022 · 156 · 106667
45. ISO 15156/NACE MR0175 - A new international standard for metallic materials for use in oil and gas production in sour environments
46. N.-E. Titouche et al., Direct drive friction welding effect on mechanical and electrochemical characteristics of titanium stabilized austenitic stainless steel (AISI 321) research reactor thick tube. 2019. 41: p. 273-283, https://doi.org/10.1016/j.jmapro.2019.03.016.10.1016/j.jmapro.2019.03.016 ↗
47. Ahmadi · Failure Analysis of Cracked 2.25 Cr–1.0 Mo Steel Tubes of an Oil Refinery Boiler. · 2020 · 110 · 104435
48. Herbirowo, S., Hakim, L., & Adjiantoro, B. (2018). Microstructure and mechanical characteristics of hot forged lateritic steels. In MATEC Web of Conferences (Vol. 204, p. 05007), https://doi.org/10.1051/matecconf/201820405007.10.1051/matecconf/201820405007 ↗
49. Moitra · A Toughness Study of the Weld Heat-Affected Zone of a 9Cr–1Mo Steel. · 2002 · 48 · 55
50. The effect of material heterogeneity and temperature on impact toughness and fracture resistance of sa-387 gr
51. Čamagić, I., et al., Influence of temperature and exploitation period on the behaviour of a welded joint subjected to impact loading. 2016. 16(3): p. 179-185, https://hdl.handle.net/21.15107/rcub_machinery_2384.
52. Strain controlled vs stress controlled hydrogen induced fracture in a quenched and tempered steel10.1007/BF02642339 ↗
53. Chaudhuri · High Temperature Boiler Tube Failures: Case Studies. · 1997 · 107
54. Precipitation–segregation mechanism for high temperature temper embrittlement of steels revealed by Auger electron spectroscopy and internal friction measurements10.1179/mst.1990.6.2.124 ↗
55. Temper embrittlement of supermartensitic stainless steel and non-destructive inspection by magnetic Barkhausen noise10.1016/j.engfailanal.2019.02.034 ↗
56. The influence of phosphorus on the temper embrittlement and hydrogen embrittlement of some dual-phase steels10.1016/j.msea.2022.143379 ↗
57. Temper embrittlement of Ni-Cr steel by antimony I. Embrittlement at low carbon concentration10.1007/BF02644044 ↗
58. The effects of composition and microstructure on temper embrittlement in 2 1/4 Cr-1 Mo
59. The role of reverse temper embrittlement on some low and high temperature crack extension processes in low carbon, low alloy steels: A review10.1016/0308-0161(92)90121-U ↗