Steel pipes have been widely used in the water and petroleum industries where crack-like flaws have long been recognised as a major cause of their failures. This paper intends to develop a new method for determining the elasto-plastic J-integral of cracked pipes made of all types of steel. A solution to elasto-plastic J-integrals is derived for external longitudinal semi-elliptical surface cracks in pressurised steel pipes. A meshing technique is developed in the detailed three-dimensional finite element analysis that incorporates the mixed types of quadratic tetrahedron and hexahedron elements. The developed method is verified with detailed finite element results. It is found in the paper that the general trend of normalised fully plastic J-integral changes with the change of crack depths and aspect ratios, and the magnitude of normalised fully plastic J-integrals can be significantly affected by material properties and pipe dimensions. The developed method can provide a useful tool for the failure assessment of pressurized steel pipes, allowing for a wide range of pipe dimensions, crack geometries and material properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Structural Integrity and Reliability Analysis · Geotechnical Engineering and Underground Structures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. 6.14 Documentation
2. Anderson · 2017
3. R.B. Anderson, T.L. Sullivan, Fracture mechanics of through-cracked cylindrical pressure vessels (No. NASA-TN-D-3252). National aeronautics and space administration cleveland oh lewis research center, 1966.
4. Al Laham · 1998 · Vol. 3
5. J.T. Bloom, A procedure for the assessment of the structural integrity of nuclear pressure vessels, J. Pressure Vessel Technol. 105(1) (1983) 28-34.10.1115/1.3264235 ↗
6. Advances in J-integral estimation of circumferentially surface cracked pipes10.1111/j.1460-2695.2011.01558.x ↗
7. Improved J and COD estimation by GE/EPRI method in elastic to fully plastic transition zone10.1016/j.engfracmech.2006.03.012 ↗
8. EDF Energy, R6: Assessment of the integrity of structures containing defects, Revision 4, with amendments to Amendment 11, Gloucester, 2015.
9. Elasto and fully plastic J-integrals for mixed mode fracture induced by inclined surface cracks in plates under biaxial loading10.1016/j.engfracmech.2017.10.032 ↗
10. Prediction of Fracture Failure of Steel Pipes With Sharp Corrosion Pits Using Time-Dependent Reliability Method With Lognormal Process10.1115/1.4043010 ↗
11. The penny-shaped crack and the plane strain crack in an infinite body of power-law material10.1115/1.3157742 ↗
12. Plastic influence functions for calculating J-integral of complex-cracks in pipe10.1016/j.ijpvp.2016.07.003 ↗
13. Reference stress method for evaluation of failure assessment curve of cracked pipes in nuclear power plants10.1016/j.ijpvp.2009.11.002 ↗
14. J. Kiefner, W. Maxey, R. Eiber, A. Duffy, Failure stress levels of flaws in pressurised cylinders. In Progress in flaw growth and fracture toughness testing. ASTM International, 1973.10.1520/STP49657S ↗
15. Enhanced reference stress-based J and crack opening displacement estimation method for leak-before-break analysis and comparison with GE.EPRI method10.1046/j.1460-2695.2001.00388.x ↗
16. Quantification of pressure-induced hoop stress effect on fracture analysis of circumferential through-wall cracked pipes10.1016/S0013-7944(01)00132-1 ↗
17. Elastic–plastic J and COD estimates for axial through-wall cracked pipes10.1016/S0308-0161(02)00030-3 ↗
18. Approximate J estimates for tension-loaded plates with semi-elliptical surface cracks10.1016/S0013-7944(01)00146-1 ↗
19. Finite element based plastic limit loads for cylinders with part-through surface cracks under combined loading10.1016/S0308-0161(03)00106-6 ↗
20. Elastic–plastic fracture mechanics method for finite internal axial surface cracks in cylinders10.1016/S0013-7944(03)00159-0 ↗
21. Review of Quantita-tive Reliability Methods for Onshore Oil and Gas Pipe-lines
22. V.G.M.D. Kumar, M.D. German, C.F. Shih, Engineering approach for elasto-plastic fracture analysis (No. EPRI-NP--1931). General Electric Co., 1981.10.2172/6068291 ↗
23. V. Kumar, M.D. German, W.W. Wilkening, W.R. Andrews, H.G. deLorenzi, D.F. Mowbray, Advances in elastic-plastic fracture analysis. Final report (No. EPRI-NP-3607). General Electric Co., Schenectady, NY (USA). Corporate Research and Development Center, 1984.
24. J-integral and limit load analysis of semi-elliptical surface cracks in plates under combined tension and bending10.1016/j.ijpvp.2003.12.002 ↗
25. Stress intensity factors for high aspect ratio semi-elliptical internal surface cracks in pipes10.1016/j.ijpvp.2012.05.005 ↗
26. Failure Assessment for the High-Strength Pipelines with Constant-Depth Circumferential Surface Cracks10.1155/2018/2089514 ↗
27. Makar · 2001 · 303
28. Fracture response of pipelines subject to large plastic deformation under bending10.1016/j.ijpvp.2004.08.012 ↗
29. J.G. Park, D.S. Jeon, N.S. Huh, S.M. Lee, Y.J. Kim, Simple Calculations of J-Integral for Through-Wall Crack in Welded Pipes Based on Failure Assessment Diagram. In Pressure Vessels and Piping Conference (Vol. 58974, p. V06AT06A064). American Society of Mechanical Engineers, 2019, July.10.1115/PVP2019-93561 ↗
30. Stress-Intensity Factor Influence Coefficients for Internal and External Surface Cracks in Cylindrical Vessels
31. Review of triaxial crack border stress and energy behavior10.1016/0167-8442(89)90011-6 ↗
32. Limit analysis of flaws in pressurized pipes and cylindrical vessels. Part I: Axial defects10.1016/j.engfracmech.2006.04.031 ↗
33. New J and COD estimates for thin-walled pipes with axial through-wall cracks and high strain hardening exponents10.1016/j.tafmec.2017.03.001 ↗
34. Three-dimensional fully plastic solutions for semi-elliptical surface cracks10.1016/0308-0161(93)90073-3 ↗
35. Time dependent reliability analysis for cast iron pipes subjected to pitting corrosion10.1016/j.ijpvp.2019.103935 ↗
36. Degradation of mechanical property of corroded water pipes after long service10.1080/1573062X.2019.1687744 ↗
37. Evaluation of stress intensity factor for cast iron pipes with sharp corrosion pits10.1016/j.engfailanal.2017.06.026 ↗
38. Fully plastic J-integral solutions for surface cracked plates under biaxial loading10.1016/j.engfracmech.2005.12.014 ↗