journal article·2024-03

Rate-limiting mechanism of all-solid-state battery unravelled by low-temperature test-analysis flow

Pushun Lu, Yujing Wu, Dengxu Wu, Fengmei Song, Tenghuan Ma, Wenlin Yan, Xiang Zhu, Fuliang Guo, Jiaze Lu, Jian Peng, Liquan Chen, Hong Li, Fan Wu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Fundamentals and challenges of lithium ion batteries at temperatures between −40 and 60°C
2. Critical review on low-temperature li-ion/metal batteries10.1002/adma.202107899 ↗
3. Promoting rechargeable batteries operated at low temperature10.1021/acs.accounts.1c00420 ↗
4. Approaching practically accessible solid-state batteries: stability issues related to solid electrolytes and interfaces10.1021/acs.chemrev.9b00268 ↗
5. The role of Li-ion battery electrolyte reactivity in performance decline and self-discharge10.1016/S0378-7753(03)00149-6 ↗
6. In situ electrochemical-mass spectroscopic investigation of solid electrolyte interphase formation on the surface of a carbon electrode10.1016/j.electacta.2013.08.108 ↗
7. Thermal runaway caused fire and explosion of lithium ion battery10.1016/j.jpowsour.2012.02.038 ↗
8. Superior all-solid-state batteries enabled by a gas-phase-synthesized sulfide electrolyte with ultrahigh moisture stability and ionic conductivity10.1002/adma.202100921 ↗
9. 5V-class sulfurized spinel cathode stable in sulfide all-solid-state batteries10.1016/j.nanoen.2021.106589 ↗
10. Water-stable sulfide solid electrolyte membranes directly applicable in all-solid-state batteries enabled by superhydrophobic Li+-conducting protection layer10.1002/aenm.202102348 ↗
11. Long-life lithium-metal all-solid-state batteries and stable li plating enabled by in situ formation of Li3PS4 in the SEI layer10.1002/adma.202203281 ↗
12. Interfacial and cycle stability of sulfide all-solid-state batteries with Ni-rich layered oxide cathodes10.1016/j.nanoen.2022.107528 ↗
13. Stable Ni-rich layered oxide cathode for sulfide-based all-solid-state lithium battery10.1016/j.esci.2022.06.001 ↗
14. High-areal-capacity and long-cycle-life all-solid-state battery enabled by freeze drying technology10.1039/D3EE00420A ↗
15. High-safety, wide-temperature-range, low-external-pressure and dendrite-free lithium battery with sulfide solid electrolyte10.1016/j.ensm.2022.10.057 ↗
16. Solid state ionics – Selected topics and new directions10.1016/j.pmatsci.2022.100921 ↗
17. Doping strategy and mechanism for oxide and sulfide solid electrolytes with high ionic conductivity10.1039/D1TA10966A ↗
18. High Current Density and Long Cycle Life Enabled by Sulfide Solid Electrolyte and Dendrite-Free Liquid Lithium Anode10.1002/adfm.202105776 ↗
19. Fast charge storage kinetics by surface engineering for Ni-rich layered oxide cathodes10.1039/D3TA00890H ↗
20. Progress in solvent-free dry-film technology for batteries and supercapacitors10.1016/j.mattod.2022.04.008 ↗
21. Practical evaluation of energy densities for sulfide solid-state batteries10.1016/j.etran.2019.100010 ↗
22. Progress in thermal stability of all-solid-state-Li-ion-batteries10.1002/inf2.12224 ↗
23. Thermal stability between sulfide solid electrolytes and oxide cathode10.1021/acsnano.2c04905 ↗
24. LiNbO3-coated LiNi0.7Co0.1Mn0.2O2 and chlorine-rich argyrodite enabling high-performance solid-state batteries under different temperatures10.1016/j.ensm.2021.08.028 ↗
25. Impact of surface coating on the low temperature performance of a sulfide-based all-solid-state battery cathode10.5796/electrochemistry.21-00126 ↗
26. Chlorine-rich lithium argyrodite enabling solid-state batteries with capabilities of high voltage, high rate, low-temperature and ultralong cyclability10.1016/j.cej.2021.132896 ↗
27. Regulating Electronic Conductivity at Cathode Interface for Low-Temperature Halide-Based All-Solid-State Batteries
28. Carbon-free high-loading silicon anodes enabled by sulfide solid electrolytes10.1126/science.abg7217 ↗
29. Wide-Temperature, Long-Cycling, and High-Loading Pyrite All-Solid-State Batteries Enabled by Argyrodite Thioarsenate Superionic Conductor10.1002/adfm.202211211 ↗
30. Unlocking charge transfer limitations for extreme fast charging of Li-Ion Batteries
31. Tailoring electrolyte solvation for Li metal batteries cycled at ultra-low temperature10.1038/s41560-021-00783-z ↗
32. Lithium-ion battery structure that self-heats at low temperatures10.1038/nature16502 ↗
33. Lithium-sulfur battery diagnostics through distribution of relaxation times analysis10.1016/j.ensm.2022.06.016 ↗
34. Influence of the discretization methods on the distribution of relaxation times deconvolution: implementing radial basis functions with DRTtools10.1016/j.electacta.2015.09.097 ↗
35. The timescale identification decoupling complicated kinetic processes in lithium batteries10.1016/j.joule.2022.05.005 ↗
36. Highly stable halide-electrolyte-based all-solid-state li-se batteries10.1002/adma.202200856 ↗
37. Electrochemical impedance spectroscopy for all-solid-state batteries: theory, methods and future outlook10.1002/celc.202100108 ↗
38. Recent development of lithium argyrodite solid-state electrolytes for solid-state batteries: synthesis, structure, stability and dynamics10.1016/j.nanoen.2021.105858 ↗
39. Space–charge layer effect at interface between oxide cathode and sulfide electrolyte in all-solid-state lithium-ion battery10.1021/cm5016959 ↗
40. Interfacial observation between LiCoO2 electrode and Li2S−P2S5 solid electrolytes of all-solid-state lithium secondary batteries using transmission electron microscopy10.1021/cm901819c ↗
41. Interface Stability in Solid-State Batteries10.1021/acs.chemmater.5b04082 ↗
42. Deciphering Interfacial Chemical and Electrochemical Reactions of Sulfide-Based All-Solid-State Batteries10.1002/aenm.202100210 ↗
43. Realizing long-cycling all-solid-state Li-In||TiS2 batteries using Li6+xMxAs1-xS5I (M=Si, Sn) sulfide solid electrolytes10.1038/s41467-023-39686-w ↗
44. A rocking chair type all-solid-state lithium ion battery adopting Li2O–ZrO2 coated LiNi0.8Co0.15Al0.05O2 and a sulfide based electrolyte10.1016/j.jpowsour.2013.10.005 ↗