journal article·2023-07-02Open access

Electrochemical corrosion behavior of plasma sprayed Cr2O3-25TiO2 composite coatings

School of Mechanical & Automotive Engineering, Qilu University of Technology (Shandong Academy of Sciences), Jinan, Shandong, 250353, PR China, Q. H. Song, F. S. Hao, Weihai Yinxing Prestressed Wire Products Co.,Ltd, Weihai, Shandong, 264200, PR China, Y. F. Zhang, School of Mechanical & Automotive Engineering, Qilu University of Technology (Shandong Academy of Sciences), Jinan, Shandong, 250353, PR China, Q. Li, School of Material Science & Engineering, Qilu University of Technology, Shandong Academy of Sciences, Jinan, Shandong, 250353, PR China, J. J. Li, School of Mechanical & Automotive Engineering, Qilu University of Technology (Shandong Academy of Sciences), Jinan, Shandong, 250353, PR China

Abstract

In this paper, Cr2O3-25TiO2 composite coatings were prepared on the surface of steel structure samples by atmospheric plasma spraying. The phase composition, microstructure, microhardness and long-term immersion corrosion behavior in 3.5 wt.% NaCl solution of Cr2O3-25TiO2 composite coatings were studied. The corrosion behavior of Cr2O3-25TiO2 composite coating was analyzed by potentiodynamic polarization and electrochemical impedance spectroscopy. The impedance data were fitted into an appropriate equivalent circuit to explain the electrochemical corrosion behavior of the coating at different stages. The results of scanning electron microscopy showed that the Cr2O3-25TiO2 composite coating was agglomerated, and the rhombohedral Cr2O3 powder was wrapped around the rhombohedral TiO2 powder. The coating melted completely without obvious defected. The XRD results showed that no phase transformation occurred in the Cr2O3-25TiO2 composite coating. The Cr2O3-25TiO2 coatings showed high corrosion resistance and good passivation behavior in the initial stage of corrosion. The coating itself did not corrode. With the extension of corrosion time, the corrosive medium had passed through the pores between the coatings, resulting in the contact between the corrosive medium and the matrix interface, resulting in the matrix corrosion damage. Corrosion products would deposit on the surface of the coating, blocking the pores between the coatings, and the corrosion rate would be reduced.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. [1] J. Guo, C. Shang, S. Yang, H. Guo, X. Wang, X. He, Materials & Design, 30(1), 129-134 (2009); https://doi.org/10.1016/j.matdes.2008.04.03810.1016/j.matdes.2008.04.038 ↗
2. [2] N.K. Mishra, S.B. Mishra, R. Kumar, Surface and Coatings Technology, 260, 23-27 (2014); https://doi.org/10.1016/j.surfcoat.2014.07.08910.1016/j.surfcoat.2014.07.089 ↗
3. [3] M. Nath, H.S. Tripathi, Ceramics International, 41(2), 3109-3115 (2015); https://doi.org/10.1016/j.ceramint.2014.10.15510.1016/j.ceramint.2014.10.155 ↗
4. [4] X. Wang, P. Ju, X. Lu, Y. Chen, F. Wang, Ceramics International, 48(3), 3615-3627 (2022); https://doi.org/10.1016/j.ceramint.2021.10.14210.1016/j.ceramint.2021.10.142 ↗
5. [5] V.P. Singh, A. Sil, R. Wear, 272(1), 149-158 (2011); https://doi.org/10.1016/j.wear.2011.08.00410.1016/j.wear.2011.08.004 ↗
6. [6] D. Chen, A. Huang, H. Gu, M. Zhang, Z. Shao, Ceramics International, 41(10), 14748-14753 (2015); https://doi.org/10.1016/j.ceramint.2015.07.20210.1016/j.ceramint.2015.07.202 ↗
7. [7] N.-n. Li, G.-l. Li, H.-d. Wang, J.-j. Kang, T.-s. Dong, H.-j. Wang, Materials & Design, 88, 906-914 (2015); https://doi.org/10.1016/j.matdes.2015.09.08510.1016/j.matdes.2015.09.085 ↗
8. [8] K.V. Sreenivas Rao, G.C. Tejaswini, K.G. Girisha, Materials Today: Proceedings, 5(11), 24068-24074 (2018); https://doi.org/10.1016/j.matpr.2018.10.20010.1016/j.matpr.2018.10.200 ↗
9. [9] A. Raj Sharma, R. Goyal, Materials Today: Proceedings, 48, 946-951 (2022); https://doi.org/10.1016/j.matpr.2021.05.67710.1016/j.matpr.2021.05.677 ↗
10. [10] P. Zamani, Z. Valefi, K. Jafarzadeh, Ceramics International, 48(2), 1574-1588 (2022); https://doi.org/10.1016/j.ceramint.2021.09.23710.1016/j.ceramint.2021.09.237 ↗
11. [11] J. Chen, J. Xiao, Y. Zhang, Y. Wei, B. Han, Y. Li, S. Zhang, N. Li, Corrosion Science, 163, (2020); https://doi.org/10.1016/j.corsci.2019.10825010.1016/j.corsci.2019.108250 ↗
12. [12] D.W.L. B.K. Kim, and G.H. Ha, Journal of Thermal Spray Technology, 10(1), 133-137 (2001); https://doi.org/10.1361/10599630177034960010.1361/105996301770349600 ↗
13. [13] P. Zamani, Z. Valefi, Surface and Coatings Technology, 316, 138-145 (2017); https://doi.org/10.1016/j.surfcoat.2017.03.02210.1016/j.surfcoat.2017.03.022 ↗
14. [14] E. Abedi Esfahani, H. Salimijazi, M.A. Golozar, J. Mostaghimi, L. Pershin, Journal of Thermal Spray Technology, 21(6), 1195-1202 (2012); https://doi.org/10.1007/s11666-012-9810-x10.1007/s11666-012-9810-x ↗
15. [15] C. Haixiang, K. Dejun, Materials Chemistry and Physics, 251, (2020); https://doi.org/10.1016/j.matchemphys.2020.12320010.1016/j.matchemphys.2020.123200 ↗
16. [16] S.M. Hashemi, N. Parvin, Z. Valefi, M. Alishahi, Ceramics International, 45(17), 21108-21119 (2019); https://doi.org/10.1016/j.ceramint.2019.07.08710.1016/j.ceramint.2019.07.087 ↗
17. [17] J. Zhang, Z. Wang, P. Lin, W. Lu, Z. Zhou, S. Jiang, Journal of Thermal Spray Technology, 20(3), 508-513 (2010); https://doi.org/10.1007/s11666-010-9528-610.1007/s11666-010-9528-6 ↗