Application of Alumina Coping to Porcelain Laminate Veneered Crown: Part 1 Masking Ability for Discolored Teeth

Mitsunobu OKAMURA, Ker-Kong CHEN, Hiroshi KAKIGAWA, Yoshio KOZONO

Dental Materials Journal· Volume 23· Issue 2

Abstract

A densely sintered high-purity alumina has been successfully utilized as a coping for all-ceramic crown. In order to apply the alumina coping to the porcelain laminate veneer restoration for the discolored teeth, the present study evaluated its masking ability when it was thinner than the proposed thickness for the crown. Colorimetric examination was performed on white and black backgrounds for the 0.7 mm thick porcelain laminate veneer with 0.40 or 0.25 mm thick alumina coping and 0.7 mm thick porcelain without coping. With the presence of the coping, the porcelain appeared significantly lighter. Judging from the calculated color differences delta E and the literature, it was suggested that the masking ability of the alumina coping would be sufficient with a 0.25 mm thickness for the porcelain laminate veneer for heavily discolored teeth.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.