Effect of silane and phosphate primers on the adhesive performance of atri-n-butylborane initiated luting agent bonded to zirconia
Source abstract
Abstract
The purpose of this study was to evaluate the effects of primers on the bond strength and durability of an acrylic resin luting agent bonded to zirconia. Disk specimens were fabricated from zirconia partially stabilized with yttrium oxide. The disks were primed with one of the following materials: Alloy Primer (AP), Ceramic Primer (CP), Liquid A of the Porcelain Liner M (PLM-A), Liquid B of Porcelain Liner M (PLM-B), Porcelain Liner M (PLM-A+PLM-B), Monobond Plus (MP), and mixture of AP and PLM-B. The specimens were bonded with a tri-n-butylborane (TBB)-initiated luting agent. The shear bond strengths were determined both before and after thermocycling. The results were statistically analyzed with a non-parametric procedure. The highest post-thermocycling bond strength was generated from the groups primed with MP, CP, and AP. It can be concluded that the application of three phosphate primers is recommended for bonding the zirconia with the TBB-initiated luting agent.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. 10.1067/mpr.2003.5010.1067/mpr.2003.50 ↗
2. 2) Al-Amleh B, Lyons K, Swain M. Clinical trials in zirconia: a systematic review. J Oral Rehabil 2010; 37: 641-652.10.1111/j.1365-2842.2010.02094.x ↗
3. 10.1016/S0142-9612(98)00010-610.1016/S0142-9612(98)00010-6 ↗
4. 10.1016/j.jdent.2009.06.00210.1016/j.jdent.2009.06.002 ↗
5. 5) Beuer F, Stimmelmayr M, Gernet W, Edelhoff D, Guh JF, Naumann M. Prospective study of zirconia-based restorations: 3-year clinical results. Quintessence Int 2010; 41: 631-637.
6. 10.1016/j.jdent.2012.02.01110.1016/j.jdent.2012.02.011 ↗
7. 10.1111/joor.1201810.1111/joor.12018 ↗
8. 8) Roediger M, Gersdorff N, Huels A, Rinke S. Prospective evaluation of zirconia posterior fixed partial dentures: four year clinical results. Int J Prosthodont 2010; 23: 141-148.
9. 9) Sax C, Hammerle CH, Sailer I. 10-year clinical outcomes of fixed dental prostheses with zirconia frameworks. Int J Comput Dent 2011; 14: 183-202.
10. 10.1111/j.1365-2842.2012.02311.x10.1111/j.1365-2842.2012.02311.x ↗
11. 10.11607/ijp.322910.11607/ijp.3229 ↗
12. 12) Vanlioglu BA, Ozkan Y, Evren B, Ozkan YK. Experimental custom-made zirconia abutments for narrow implants in esthetically demanding regions: a 5-year follow-up. Int J Oral Maxillofac Implants 2012; 27: 1239-1242.
13. 13) Lops D, Bressan E, Chiapasco M, Rossi A, Romeo E. Zirconia and titanium implant abutments for single-tooth implant prostheses after 5 years of function in posterior regions. Int J Oral Maxillofac Implants 2013; 28: 281-287.10.11607/jomi.2668 ↗
14. 14) Di Alberti L, Di Alberti C, Donini F, Lo Muzio L, Cadrobbi F, D’Agostino A, De Santis D, Bertossi D. Clinical and mechanical evaluation of screw-retained implant-supported zirconia restorations. A 36 months prospective clinical study. Minerva Stomatol 2013; 62: 25-32.
15. 15) Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000; 13: 131-135.
16. 10.1016/S0109-5641(98)00011-610.1016/S0109-5641(98)00011-6 ↗
17. 10.1016/j.prosdent.2004.02.00110.1016/j.prosdent.2004.02.001 ↗
18. 18) Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000; 2: 139-147.
19. 10.1007/s00784-008-0222-810.1007/s00784-008-0222-8 ↗
20. 10.1046/j.1365-2842.1999.00423.x10.1046/j.1365-2842.1999.00423.x ↗
21. 10.1046/j.1365-2842.2001.00627.x10.1046/j.1365-2842.2001.00627.x ↗
22. 22) Nogami T, Tanoue N, Atsuta M, Matsumura H. Effectiveness of two-liquid silane primers on bonding sintered feldspathic porcelain with a dual-cured composite luting agent. J Oral Rehabil 2004; 31: 770-774.10.1111/j.1365-2842.2004.01303.x ↗
23. 10.1016/j.dental.2005.11.03510.1016/j.dental.2005.11.035 ↗
24. 24) Piascik JR, Swift EJ, Thompson JY, Grego S, Stoner BR. Surface modification for enhanced silanation of zirconia ceramics. Dent Mater 2009; 25: 1116-1121.10.1016/j.dental.2009.03.008 ↗
25. 10.1016/j.dental.2005.02.00510.1016/j.dental.2005.02.005 ↗
26. 10.1016/S0300-5712(96)00023-110.1016/S0300-5712(96)00023-1 ↗