journal article·2011Open access

Influence of silane heat treatment on bond strength of resin cement to a feldspathic ceramic

Rodrigo Furtado de CARVALHO, Maria Elizabeth Marques Nogueira MARTINS, José Renato Cavalcanti de QUEIROZ, Fabíola Pessoa Pereira LEITE, Mutlu ÖZCAN

Dental Materials Journal· Volume 30· Issue 3

Abstract

This study evaluated the influence of heat treatment (HT) of the silane on the microtensile bond strength of resin cement to a feldspathic ceramic. Ceramic (VITA VM7) and composite blocks (N=32) were divided into four groups (n=6 for bond test, n=2 for SEM) at random and subject to following sequence of conditioning: G1: HF 9.6%+Silane+Panavia F2.0, G2: HF 9.6%+Silane+HT+Panavia F2.0, G3: Silane+HT+Panavia F2.0, and G4: Silane+Panavia F2.0. HT was performed in an oven (100°C, 2 minutes). G1 (17.6±2.3 MPa) and G2 (19±3.2 MPa) showed significantly higher mean bond strength than those of G3 (9.1±2.8 MPa) and G4 (10.9±1.8 MPa). SEM analysis showed exclusively mixed failures. Silane HT did not increase the bond strength.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. 1) Gomes EA, Assunção WG, Rocha EP, Santos PH. Ceramic in dentistry: current situation. Cerâmica 2008; 54: 319-325.
2. 2) Della Bona A, Anusavice KJ. Microstructure, composition, and etching topography of dental ceramics. Int J Prosthodont 2002; 15: 159-167.
3. 3) Matinlinna JP, Lassila LV, Özcan M, Yli-Urpo A, Vallittu PK. An introduction to silanes and their clinical applications in dentistry. Int J Prosthodont 2004; 17: 155-164.
4. 10.1016/S0109-5641(03)00019-810.1016/S0109-5641(03)00019-8 ↗
5. 10.1016/S0022-3913(05)80076-910.1016/S0022-3913(05)80076-9 ↗
6. 10.1016/j.dental.2006.11.01110.1016/j.dental.2006.11.011 ↗
7. 7) Ayad MF, Fahmy NZ, Rosenstiel SF. Effect of surface treatment on roughness and bond strength of a heat-pressed ceramic. J Prosthet Dent 2008; 99: 123-130.10.1016/S0022-3913(08)60028-1 ↗
8. 8) Chen JH, Matsumura H, Atsuta M. Effect of different etching periods on the bond strength of a composite resin to a machinable porcelain. J Dent 1998; 28: 53-58.10.1016/S0300-5712(96)00078-4 ↗
9. 10.1046/j.1365-2842.2001.00626.x10.1046/j.1365-2842.2001.00626.x ↗
10. 10) Saraçoglu C, Cura C, Çötert HS. Effect of various surface treatment methods on the bond strength of the heat-pressed ceramic specimen. J Oral Rehabil 2004; 31: 790-797.10.1111/j.1365-2842.2004.01305.x ↗
11. 10.1016/j.prosdent.2004.12.00210.1016/j.prosdent.2004.12.002 ↗
12. 12) Matinlinna JP, Vallittu PK. Bonding of resin composites to etchable ceramics surface: An insight review of the chemical aspects on surface conditioning. J Oral Rehabil 2007; 34: 622-630.10.1111/j.1365-2842.2005.01569.x ↗
13. 10.1177/0022034597076006100110.1177/00220345970760061001 ↗
14. 10.1016/S0109-5641(01)00047-110.1016/S0109-5641(01)00047-1 ↗
15. 15) Filho AM, Vieira LC, Araújo E, Monteiro Júnior S. Effect of different ceramic surface treatments on resin microtensile bond strength. J Prosthodont 2004; 13: 28-35.10.1111/j.1532-849X.2004.04007.x ↗
16. 16) Fabianelli A, Pollington S, Papacchini F, Goracci C, Cantoro A, Ferrari M, van Noort R. The effect of different surface treatments on bond strength between leucite reinforced feldspathic ceramic and composite resin. J Dent 2010; 38: 39-43.10.1016/j.jdent.2009.08.010 ↗
17. 17) Edelhoff D, Özcan M. To what extent does the longevity of fixed dental prostheses depend on the function of the cement? Clin Oral Implants Res 2007; 18: 193-204.10.1111/j.1600-0501.2007.01442.x ↗
18. 10.1016/0109-5641(94)90067-110.1016/0109-5641(94)90067-1 ↗
19. 19) Van Noort R, Noroozi S, Howard IC, Cardew GE. A critique of bond strength measurements. J Dent Res 1989; 17: 61-67.10.1016/0300-5712(89)90131-0 ↗
20. 10.1177/0022034595074009140110.1177/00220345950740091401 ↗
21. 10.1016/0109-5641(92)90097-V10.1016/0109-5641(92)90097-V ↗
22. 10.1016/S0109-5641(98)00034-710.1016/S0109-5641(98)00034-7 ↗
23. 23) Pashley DH, Carvalho RM, Sano H, Nakajima M, Yoshiyama M, Shono Y, Fernandes CA, Tay F. The microtensile bond test: a review. J Adhes Dent 1999; 1: 290-309.
24. 24) Shono Y, Terashita M, Shimada J, Kozono Y, Carvalho RM, Russell CM, Pashley DH. Durability of resin-dentin bonds. J Adhes Dent 1999; 1: 211-218.
25. 25) Della Bona A, Anusavice, KJ, Shen C. Microtensile strength of composite bonded to hot-pressed ceramics. J Adhes Dent 2000; 2: 305-313.
26. 26) Moharamzadeh K, Hooshmand T, Keshvad A, van Noort R. Fracture toughness of a ceramic-resin interface. Dent Mater 2008; 24: 172-177.10.1016/j.dental.2007.04.002 ↗