journal article·2014Open access

Hybrid effects of zirconia nanoparticles with aluminum borate whiskers on mechanical properties of denture base resin PMMA

Xiu-Yin ZHANG, Xin-Jing ZHANG, Zhuo-Li HUANG, Bang-Shang ZHU, Rong-Rong CHEN

Dental Materials Journal· Volume 33· Issue 1

Abstract

The aim of this study was to investigate the hybrid effects of ZrO₂ nanoparticles (nano-ZrO₂) and aluminum borate whiskers (ABWs) on flexural strength and surface hardness of denture base resin, polymethyl methacrylate (PMMA). Both nano-ZrO₂ and ABWs were modified by silane coupling agent (Z6030) before being mixed with PMMA. Various amounts of silanized nano-ZrO₂ and ABWs were mixed with PMMA to prepare ZrO₂-ABW/PMMA composites. Flexural strength and surface hardness were evaluated using three- point bending test and Vickers hardness test respectively. Fractured surfaces were also observed by scanning electron microscopy (SEM). The mechanical behaviors of silanized ZrO₂-ABW/PMMA composites were significantly improved. Flexural strength reached a maximum value of 108.01 ± 5.54 MPa when 2 wt% of nano-ZrO₂ was mixed with ABWs at a ZrO₂/ABW ratio of 1:2, amounting to an increase of 52% when compared with pure PMMA. Surface hardness achieved a maximum value of 22.50 ± 0.86 MPa when 3 wt% of nano-ZrO₂ was mixed with ABWs at the same ZrO₂/ABW ratio, which was an increase of 27% when compared with pure PMMA.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. 1) Frankilin P, Wood DJ, Bubb NL. Reinforcement of poly (methyl methacrylate) denture base with glass flake. Dent Mater 2005; 21: 365-370.10.1016/j.dental.2004.07.002 ↗
2. 2) Kanie T, Fujii K, Arikawa H, Inoue K. Flexural properties and impact strength of denture base polymer reinforced with woven glass fibers. Dent Mater 2000; 16: 150-158.10.1016/S0109-5641(99)00097-4 ↗
3. 3) Qian C, Zhang XY, Zhu BS, Lin KL, Chang J, Zhang XJ. The effect of CaSiO3 nano-particles reinforced denture polymethyl methacrylate. Adv Compos Lett 2011; 20: 13-20.10.1177/096369351102000102 ↗
4. 4) Nakamura M, Takahashi H, Hayakawa I. Reinforcement of denture base resin with short-rod glass fiber. Dent Mater J 2007; 26: 733-738.10.4012/dmj.26.733 ↗
5. 5) Atai M, Pahlavan A, Moin N. Nano-porous thermally sintered nano silica as novel fillers for dental composites. Dent Mater 2012; 28: 133-145.10.1016/j.dental.2011.10.015 ↗
6. 6) Wang QQ, Wang X, Li XJ, Cai YB, Wer QF. Surface modification of PMMA/O-MMT composite microfibers by TiO2 coating. Appl Surf Sci 2011; 258: 98-102.10.1016/j.apsusc.2011.08.013 ↗
7. 7) Gao Y, Gao XP, Zhou YF, Yan DY. Preparation of poly (methyl methacrylate) grafted titanate nanotubes by in situ atom transfer radical polymerization. Nanotechnology 2008; 19: 495604.10.1088/0957-4484/19/49/495604 ↗
8. 8) Xu HHK, Quinn JB, Giuseppetti AA, Eichmiller FC, Parry EE, Schumacher GE. Three-body wear of dental resin composites reinforced with silica-fused whiskers. Dent Mater 2004; 20: 220-227.10.1016/S0109-5641(03)00096-4 ↗
9. 9) Jouault N, Dalmas F, Boue F, Jestin J. Multiscale characterization of filler dispersion and origins of mechanical reinforcement in model nanocomposites. Polymer 2012; 53: 761-775.10.1016/j.polymer.2011.12.001 ↗
10. 10) Sorrentino L, Berardini F, Capozzoli MR, Amitrano S, Iannace S.Nano/micro ternary composites based on PP, nanoclay, and CaCO3. J Appl Polym Sci 2009; 113: 3360-3367.10.1002/app.30241 ↗
11. 11) Brown GM, Ellyin F. Mechanical properties and multiscale characterization of nanofiber-alumina/epoxy nanocomposites. J Appl Polym Sci 2011; 119: 1459-1468.10.1002/app.32662 ↗
12. 12) Luo ZX, Yang WS, Peng AD, Zeng Y, Yao JN. The fabrication of TiO2 nanorods from TiO2 nanoparticles by organic protection assisted template method. Nanotechnology 2009; 20: 345601.10.1088/0957-4484/20/34/345601 ↗
13. 13) Wang XF, Huang ZM, Chen LS. Comparison study on transparent composites with different patterns of nanofiber reinforcement. Fiber Polym 2011; 12: 359-365.10.1007/s12221-011-0359-y ↗
14. 14) Mu MF, Osswald S, Gogotsi Y, Winey KI. An in situ Raman spectroscopy study of stress transfer between carbon nanotubes and polymer. Nanotechnology 2009; 20: 335703.10.1088/0957-4484/20/33/335703 ↗
15. 15) Lin GM, Xie GY, Sui GX, Yang R. Hybrid effect of nanoparticles with carbon fibers on the mechanical and wear properties of polymer composite. Composites Part B: Engineering 2012; 43: 44-49.10.1016/j.compositesb.2011.04.029 ↗
16. 16) Koroglu A, Ozdemir T, Usanmaz A. Comparative study of the mechanical properties of fiber-reinforced denture base resin. J Appl Polym Sci 2009; 113: 716-720.10.1002/app.30123 ↗
17. 17) Shumsky VF, Getmanchuk IP, Lipatov YS. Effect of a filler on the rheological and mechanical properties of the liquid crystalline polyester-poly(methyl methacrylate) blends. J Appl Polym Sci 2000; 76: 993-999.10.1002/(SICI)1097-4628(20000516)76:7<993::AID-APP2>3.0.CO;2-9 ↗
18. 18) Zhang XJ, Zhang XY, Zhu BS, Lin KL, Chang J. Mechanical and thermal properties of denture PMMA reinforced with silanized aluminum borate whiskers. Dent Mater J 2012; 31: 903-908.10.4012/dmj.2012-016 ↗
19. 19) Sung YM, Shin YK, Ryu JJ. Preparation of hydroxyapatite/zirconia bioceramic nanocomposites for orthopaedic and dental prosthesis applications. Nanotechnology 2007; 18: 065602.10.1088/0957-4484/18/6/065602 ↗
20. 20) Ellakwa AE, Morsy MA, El-Sheikh AM. Effect of aluminum oxide addition on the flexural strength and thermal diffusivity of heat-polymerized acrylic resin. J Prosthodont 2008; 17: 439-444.10.1111/j.1532-849X.2008.00318.x ↗
21. 21) Pallav P, De Gee AJ, Davidson CL, Erickson RL, Glasspoole EA. The influence of admixing microfiller to small-particle composite resin on wear, tensile strength, hardness, and surface roughness. J Dent Res 1989; 68: 489-490.10.1177/00220345890680031101 ↗
22. 22) ISO 20795-1:2008. Dentistry —Base polymer— Part 1: Denture base polymers.
23. 23) Medina R, Haupert F, Schlarb AK. Improvement of tensile properties and toughness of an epoxy resin by nanozirconium dioxide reinforcement. J Mater Sci 2008; 43: 3245-3252.10.1007/s10853-008-2547-8 ↗
24. 24) Alhareb AO, Ahmad ZA. Effect of Al2O3/ZrO2 hybrid on the fracture toughness and flexural properties of PMMA denture base. Adv Mater Res 2011; 173: 18-23.
25. 25) Zhang XJ, Zhang XY, Zhu BS, Qian C. Effect of nano ZrO2 on flexural strength and surface hardness of polymethylmethacrylate. Shanghai Kou Qiang Yi Xue 2011; 20: 358-363.
26. 26) Bengisu M, Inal OT. Whisker toughening of ceramics: toughening mechanisms, fabrication, and composite properties. Annu Rev Mater Sci 1994; 24: 83-124.10.1146/annurev.ms.24.080194.000503 ↗
27. 27) Koh YH, Kim HW, Kim HE. Mechanical properties and oxidation resistance of Si3N4-SiC nanocomposites. Scripta Mater 2001; 44: 2069-2073.10.1016/S1359-6462(01)00885-5 ↗
28. 28) Xu HHK, Sun L, Weir MD, Takagi SK, Chow LC, Hockey B. Effects of incorporating nanosized calcium phosphate particles on properties of whisker-reinforced dental composites. J Biomed Mater Res Part B (Appl Biomater) 2007; 81: 116-125.
29. 29) Koh YH, Kim HW, Kim HE. Microstructural evolution and mechanical properties of Si3N4-SiC (nanoparticle)-Si3N4 (whisker) composites. J Mater Res 2000; 15: 364-368.10.1557/JMR.2000.0057 ↗
30. 30) Qu M, Meth JS, Blackman GS, Cohen GM, Sharp KG, Van Vliet KJ. Tailoring and probing particle-polymer interactions in PMMA/silica nanocomposites. Soft Matter 2011; 7: 8401-8408.10.1039/c1sm05668a ↗