Evaluation of Glass Coatings with Various Silica Content Corrosion in a 0.5 M HCl Water Solution
Source abstract
Abstract
Two enamel coatings with a high and a low silica content were prepared on 35CrMo steels via vacuum firing. Their corrosion behavior in a 0.5 M HCl solution including corrosion kinetics, microstructures and electrochemistry performance were studied in comparison with uncoated steels. The results show that catastrophic corrosion occurred for uncoated steels while enamel coatings significantly decreased the corrosion rate. Enamel coatings with a high silica content exhibited the best corrosion resistance against hydrochloric acid due to their highly connected silicate network, which inhibited the leaching process of alkali metals in the acid solution. The corrosion inhibition efficiency for enamel containing a high silica content reached a maximum of 94.3%.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tubular Goods Research Institute of CNPC, Xi’an 710077, China
State Key Laboratory of Performance and Structural Safety for Petroleum Tubular Goods and Equipment Materials, Xi’an 710077, China
CNPC Bomco Drilling & Production Equipment Co. LTD., Guanghan 618300, China
Shenyang National Laboratory for Materials Science, Northeastern University, Shenyang 110819, China
Funding
Minghui Chen · Hang Wang
References (47)
Show source-provided references
1. Evaluating the mechanical behavior of electrochemically borided low-carbon steel10.1016/j.surfcoat.2019.125177 ↗
2. The combination of strength and cryogenic impact toughness in low carbon 5Mn-5Ni steel10.1016/j.jallcom.2020.155484 ↗
3. Corrosion inhibition of mild steel in hydrochloric acid solution by a mercapto-triazole compound10.1016/S0254-0584(02)00123-2 ↗
4. The corrosion inhibition of mild steel in acidic media by a new triazole derivative10.1016/S0010-938X(98)00153-X ↗
5. Corrosion inhibition of mild steel in acidic solution by Tagetes erecta (Marigold flower) extract as a green inhibitor10.1016/j.corsci.2014.04.036 ↗
6. Computational, MD simulation, SEM/EDX and experimental studies for understanding adsorption of benzimidazole derivatives as corrosion inhibitors in 1.0 M HCl solution10.1016/j.jallcom.2020.155842 ↗
7. New Epoxy sugar based glucose derivatives as eco-friendly corrosion inhibitors for the carbon steel in 1.0 M HCl: Experimental and theoretical investigations10.1016/j.jallcom.2020.154949 ↗
8. Nanoflower like SnO2-TiO2 nanotubes composite photoelectrode for efficient photocathodic protection of 304 stainless steel10.1016/j.apsusc.2018.06.307 ↗
9. Corrosion protection of new composite polymer coating for carbon steel in sulfuric acid medium by electrochemical methods10.1080/01694243.2018.1478611 ↗
10. Influence of fluid flow on the performance of polyethylene glycol as a green corrosion inhibitor10.1080/01694243.2020.1715672 ↗
11. Corrosion inhibition of carbon steel in sulfuric acid by bicyclic isoxazolidines10.1108/00035590410560930 ↗
12. Cyclic nitrones as novel organic corrosion inhibitors for carbon steel in acidic media10.1108/00035590510595148 ↗
13. Evaluation of Lavandula mairei extract as green inhibitor for mild steel corrosion in 1 M HCl solution. Experimental and theoretical approach10.1016/j.molliq.2020.113493 ↗
14. Oxidation protection of mild steel by zirconia sol-gel coatings10.1016/S0167-577X(01)00311-1 ↗
15. The corrosion behavior of the SnO2-coated mild steel in HCl solution at different temperature10.1080/01694243.2020.1807240 ↗
16. Preparation of sol-gel SiO2 coatings on steel and their corrosion resistance
17. Understanding of failure mechanisms of the oxide scales formed on nanocrystalline coatings with different Al content during cyclic oxidation10.1016/j.actamat.2020.116576 ↗
18. Self-healing metal-enamel composite coating and its protection for TiAl alloy against oxidation under thermal shock in NaCl solution10.1016/j.corsci.2020.108526 ↗
19. Corrosion of enamel with and without CaF2 in molten aluminum at 750 °C10.1016/j.corsci.2018.12.016 ↗
20. Corrosion of SiO2-B2O3-Al2O3-CaF2-R2O (R = Na and K) enamels with different content of ZrO2 in H2SO4 and NaOH solutions10.1016/j.ceramint.2019.04.232 ↗
21. Protection mechanism of enamel-alumina composite coatings on a Cr-rich nickel-based superalloy against high-temperature oxidation10.1016/j.surfcoat.2015.11.026 ↗
22. Chemical stability of titanium enamel coatings10.1007/s10717-012-9461-x ↗
23. Effect of alkali metal oxides on the properties of titanium containing glass enamels10.1007/s10717-007-0061-0 ↗
24. Low-melting chemically resistant enamel for steel kitchenware10.1023/A:1023886032228 ↗
25. Increasing corrosion resistance of titanium enamel coatings by modifying the slip10.1007/BF00677711 ↗
26. Origin and consequences of silicate glass passivation by surface layers10.1038/ncomms7360 ↗
27. Insight into silicate-glass corrosion mechanisms10.1038/nmat2301 ↗
28. Nanometre-scale evidence for interfacial dissolution-reprecipitation control of silicate glass corrosion10.1038/nmat4172 ↗
29. Micro-alloys precipitation in NiO- and CoO-bearing enamel coatings and their effect on adherence of enamel/steel10.1111/ijag.12284 ↗
30. Pattern Formation in Silicate Glass Corrosion Zones10.1111/ijag.12046 ↗
31. Aqueous corrosion of borosilicate glass under acidic conditions: A new corrosion mechanism10.1016/j.jnoncrysol.2010.04.033 ↗
32. Role and properties of the gel formed during nuclear glass alteration: Importance of gel formation conditions10.1016/S0022-3115(01)00573-6 ↗
33. Nuclear glass durability: New insight into alteration layer properties10.1021/jp205477q ↗
34. Angeli, F., Delaye, J.M., Schuller, S., Pinet, O., Rebiscoul, D., Gin, S., and Peuget, S. (2014). Open scientific questions about nuclear glass corrosion. Proceedings of the 2nd International Summer School on Nuclear Glass Wasteform: Structure, Properties and Long-Term Behavior, France, 23–27 September 2014, Elsevier Science.
35. Inhibitory effect of Gentiana olivieri extracts on the corrosion of mild steel in 0.5 M HCl: Electrochemical and phytochemical evaluation10.1016/j.arabjc.2016.06.008 ↗
36. Green approach to corrosion inhibition of mild steel in two acidic solutions by the extract of Punica granatum peel and main constituents10.1016/j.matchemphys.2011.10.027 ↗
37. A new corrosion inhibitor for copper protection10.1016/j.corsci.2014.03.004 ↗
38. Crystal-orientation-dependent corrosion behaviour of single crystals of a pure Mg and Mg-Al and Mg-Cu solid solutions10.1016/j.corsci.2016.03.019 ↗
39. CPE analysis by local electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.128 ↗
40. Performance and computational studies of two soluble pyran derivatives as corrosion inhibitors for mild steel in HCl10.1016/j.molstruc.2019.06.070 ↗
41. Corrosion inhibition of indole-3-acetic acid on mild steel in 0.5 M HCl10.1016/j.colsurfa.2007.12.009 ↗
42. Raman spectroscopic investigation of the structure of silicate glasses (II). Soda-alkaline earth-alumina ternary and quaternary glasses10.1016/0022-3093(77)90009-6 ↗
43. Combined Raman and SEM study on CaF2 formed on/in enamel by APF treatments10.1159/000261579 ↗
44. Raman spectroscopic investigation of the structure of silicate glasses. I. The binary alkali silicates10.1063/1.431671 ↗
45. Probing hydrogen-bonding interactions of water molecules adsorbed on silica, sodium calcium silicate, and calcium aluminosilicate glasses10.1021/acs.jpcc.8b04233 ↗
46. Characterization of surface structures of dealkalized soda lime silica glass using X-ray photoelectron, specular reflection infrared, attenuated total reflection infrared and sum frequency generation spectroscopies10.1016/j.jnoncrysol.2017.08.009 ↗
47. Analysis of water and hydroxyl species in soda lime glass surfaces using attenuated total reflection (ATR)-IR spectroscopy10.1111/jace.13856 ↗