Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel

Motomichi Koyama, Eiji Akiyama, Kaneaki Tsuzaki

Corrosion Science· Volume 59
Publisher page

Abstract

Abstract The hydrogen embrittlement of a Fe–18Mn–0.6C austenitic steel (wt.%) was examined using tensile tests under hydrogen charging at various current densities. The tensile properties deteriorated due to the occurrence of intergranular fracture above a specific current density. The work hardening behavior was not affected by the hydrogen charging, indicating that the embrittlement was independent of the change in behavior of slip deformation, martensitic transformation, and twinning deformation. The relationship between the fracture stresses for the intergranular fracture and the diffusible hydrogen content of the austenitic steel was approximated to the power law similarly to ferritic high strength steels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. O. Kwon, Development of high performance high manganese TWIP steels in POSCO, in: Proceedings of HMnS, CD-ROM, 2011.
2. The development of a Fe–Mn–C austenitic steel for automobile applications10.1051/metal:2006142 ↗
3. Strain hardening in Hadfield manganese steel10.1007/BF02817271 ↗
4. Strain hardening behavior in a Fe–18Mn–0.6C–1.5Al TWIP steel10.1016/j.msea.2009.08.028 ↗
5. Dislocation twin substructure evolution during strain hardening of an Fe–22wt.% Mn–0.6wt.% C TWIP steel observed by electron channeling contrast imaging
6. Effect of hydrogen on fracture of austenitic Fe–Mn–Al steel10.2355/isijinternational.34.211 ↗
7. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5Al–0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
8. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
9. High Mn TWIP steels for automotive applications, new trends and developments
10. R.T. Van Tol, L. Zhao, J. Sietsma, Effect of strain on the deformation mechanism in austenitic Mn-based TWIP steels, in: Proceedings of HMnS, CD-ROM, 2011.
11. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
12. Hydrogen transport during deformation in Nickel: Part 1. Single crystal nickel10.1007/BF02643863 ↗
13. Hydrogen transport by dislocations10.1007/BF02644079 ↗
14. Hydrogen-induced strain localization and failure of austenitic stainless-steels at high hydrogen concentrations10.1016/0956-7151(91)90211-I ↗
15. Hydrogen effects on phase-transformations in austenitic stainless-steels10.1007/BF02403244 ↗
16. TEM investigation of hydrogen-induced deformation twinning and associated martensitic phases in 304-type stainless-steel10.1007/BF00566284 ↗
17. Hydrogen-induced twinning in <001>Hadfield steel single crystals10.1016/j.scriptamat.2010.08.029 ↗
18. Solute segregation and hydrogen-induced intergranular fracture in an alloy steel10.1007/BF02644295 ↗
19. First-principles study on the grain boundary embrittlement of metals by solute segregation: Part II. Metal (Fe, Al, Cu)-hydrogen (H) systems10.1007/s11661-010-0380-6 ↗
20. Hydrogen in trapping states innocuous to environmental degradation of high strength steel10.2355/isijinternational.43.520 ↗
21. Localized deformation due to Portevin–Le Chatelier effect in 18Mn–0.6C TWIP austenitic steel10.2355/isijinternational.47.1804 ↗
22. The influence of plastic instabilities on the mechanical properties of a high-manganese austenitic FeMnC steel10.3139/146.101693 ↗
23. Microstructural dependence of Fe-high Mn tensile behavior10.1007/BF02643961 ↗
24. Effect of martensitic phase transformation and deformation twinning on mechanical properties of Fe–Mn–Si–Al steels10.1179/mst.1998.14.12.1213 ↗
25. Work hardening associated with ε-martensitic transformation, deformation twinning and dynamic strain aging in Fe–17Mn–0.6C and Fe–17Mn–0.8C TWIP steels10.1016/j.msea.2011.06.011 ↗
26. The effect of hydrogen on the yield and flow stress of an austenitic stainless steel
27. Effect of hydrogen on crack propagation behavior and microstructures around cracks in austenitic stainless steels10.2355/tetsutohagane1955.64.6_769 ↗
28. Hydrogen degradation of a boron bearing steel with 1050 and 1300MPa strength levels10.1016/j.scriptamat.2004.10.023 ↗
29. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗