Electrochemical reactivity, surface composition and corrosion mechanisms of the complex metallic alloy Al3Mg2

Ming Liu, Patrik Schmutz, Sandrine Zanna, Antoine Seyeux, Helene Ardelean, Guangling Song, Andrej Atrens, Philippe Marcus

Corrosion Science· Volume 52· Issue 2
Publisher page

Abstract

A corrosion mechanism is proposed for Al3Mg2, based on electrochemical tests, XPS, and depth profiling using XPS and ToF-SIMS. After short (∼2 min) solution exposure, the surface consists of a surface film above dealloying. The dealloying is attributed to selective Mg dissolution and the surface rearrangement of Al into islands, although the metallic Al could alternatively be formed by two reduction reactions. The surface film thickness was ∼10 nm. After exposure to ultra-pure water, the composition was AlMg1.3O0.2(OH)5.1 corresponding to Al(OH)3·1.1 Mg(OH)2·0.2MgO. After exposure to 0.01 M Na2SO4, the composition was AlMg0.2O0.4(OH)2.5 corresponding to Al(OH)3·0.1Al2O3·0.2MgO. Longer exposure produced a thicker surface film, more pronounced metallic Al islands and more MgH2. Three possibilities are identified for MgH2 formation. Al(OH)3 formation is attributed to a precipitation reaction. Bulk nanoporous Al3Mg2 formation is predicted to be possible by Mg dealloying of Mg17Al12. © 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nanoporous metals and alloys · Nanomaterials for catalytic reactions · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Recent insights into the mechanism of magnesium corrosion and research suggestions10.1002/adem.200600221 ↗
2. Recent progress in corrosion and protection of magnesium alloys10.1002/adem.200500013 ↗
3. Understanding magnesium corrosion – a framework for improved alloy performance10.1002/adem.200310405 ↗
4. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
5. ToF-SIMS depth profile of the surface film on pure magnesium formed by immersion in pure water and the identification of magnesium hydride10.1016/j.corsci.2009.06.002 ↗
6. A first quantitative XPS study of the surface films formed, by exposure to water, on Mg and on the Mg–Al intermetallics: Al3Mg2 and Mg17Al1210.1016/j.corsci.2009.02.017 ↗
7. The effect of crystallographic orientation on the active corrosion of pure magnesium10.1016/j.scriptamat.2007.10.027 ↗
8. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
9. Fractography of stress corrosion cracking of Mg–Al alloys10.1007/s11661-008-9475-8 ↗
10. Characterisation of stress corrosion cracking (SCC) of Mg–Al alloys10.1016/j.msea.2007.11.064 ↗
11. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
12. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
13. On the corrosion of binary magnesium-rare earth alloys10.1016/j.corsci.2008.12.012 ↗
14. The effect of alloy composition on the microstructure and tensile properties of binary Mg-rare earth alloys10.1016/j.intermet.2008.12.009 ↗
15. Corrosion behaviour of Mg-alloy AZ91E with atypical alloying additions10.1016/j.jallcom.2008.03.128 ↗
16. Influence of dichromate ions on corrosion of pure aluminum and AA2024-T 3 in NaCl solution studied by AFM scratching10.1149/1.1392659 ↗
17. Corrosion study of AA2024-T 3 by scanning Kelvin probe force microscopy and in situ atomic force microscopy scratching10.1149/1.1838634 ↗
18. Localized corrosion of 2024 T 351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
19. Heat treatment of cold spray coatings to form protective intermetallic layers10.1016/j.scriptamat.2009.03.002 ↗
20. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
21. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
22. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
23. Influence of heat treatment and microstructure on the corrosion of magnesium alloy Mg-10Gd-3Y–0.4Zr10.1007/s10800-008-9739-4 ↗
24. Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE4110.1016/j.corsci.2008.08.023 ↗
25. Influence of the beta-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
26. Corrosion of AZ91 in 1N NaCl and the mechanism of magnesium corrosion10.1002/adem.200800005 ↗
27. Influence of homogenization annealing of AZ91 on mechanical properties and corrosion behavior10.1002/adem.200700234 ↗
28. Influence of microstructure on corrosion of As-cast ZE4110.1002/adem.200700246 ↗
29. Electrochemical behavior of magnesium alloys AZ91D, AZCe2, and AZLa1 in chloride and sulfate solutions10.1007/s10800-007-9433-y ↗
30. Comparison of the corrosion behaviour in 5% NaCl solution of Mg alloys NZ30K and AZ91D10.1007/s10800-007-9426-x ↗
31. Effects of Zn additions on the grain boundary precipitation and corrosion of Al-508310.1016/S1359-6462(99)00349-8 ↗
32. Role of Mg in the stress corrosion cracking of an Al–Mg alloy10.1007/s11661-001-0148-0 ↗
33. Stress corrosion cracking of sensitized AA5083 (Al–4.5Mg–1.0Mn)10.1007/s11661-001-1036-3 ↗
34. Samson · 1969 · 65
35. The Samson phase, beta-Mg2Al3, revisited10.1524/zkri.2007.222.6.259 ↗
36. Structurally complex alloy phases10.1016/j.jnoncrysol.2003.11.029 ↗
37. Initial surface film on magnesium metal: a characterization by X-ray photoelectron spectroscopy (XPS) and photocurrent spectroscopy (PCS)10.1016/j.electacta.2007.03.019 ↗
38. The electrochemical behaviour of the Al8Mg5 intermetallic compound10.1016/0010-938X(83)90033-1 ↗
39. Influence of Mg on the corrosion of Al10.1116/1.582129 ↗
40. Electron beam induced oxidation of Al–Mg alloy surfaces10.1016/S0169-4332(02)00217-9 ↗
41. The negative difference effect and unipositive Mg10.1002/adem.200600275 ↗
42. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
43. The electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
44. Pourbaix · 1974
45. Film-induced cleavage of Ag–Au alloys10.1007/s11661-008-9714-z ↗
46. Stress corrosion cracking of noble metals and their alloys in solutions containing cations of the noble metal: review of observations relevant to competing models of SCC10.1016/j.corsci.2008.06.011 ↗
47. De-alloying of type 316 stainless steel in hot, concentrated sodium hydroxide solution10.1016/j.corsci.2004.01.011 ↗
48. Progress in testing the film-induced cleavage model of stress corrosion cracking
49. Stress-corrosion cracking of alpha-brass without copper oxidation10.1149/1.2221049 ↗
50. M. Saito, G. S. Smith, R. C. Newman, Testing the film-induced cleavage model of stress-corrosion cracking in: International Conference to Mark the 20th Anniversary of the UMIST Corrosion-and-Protection-Centre: Advances in Corrosion and Protection, Pergamon-Elsevier Science Ltd., Manchester, United Kingdom, 1992, pp. 411–417.10.1016/0010-938X(93)90174-F ↗
51. Brittle-fracture of an Au/Ag alloy induced by a surface-film10.1007/BF02656821 ↗
52. Role of intermetallic phases in localized corrosion of AA508310.1016/j.electacta.2006.12.072 ↗
53. C. Zhao, Z. Qi, X. Wang, Z. Zhang, Fabrication and characterization of monolithic nanoporous copper through chemical dealloying of Mg–Cu alloys, Corrosion Science. doi: 10.1016/j.corsci.2009.05.043.10.1016/j.corsci.2009.05.043 ↗
54. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
55. Uhlig · 1985
56. Evolution of nanoporosity in dealloying10.1038/35068529 ↗
57. An atomistic description of dealloying10.1149/1.1784820 ↗
58. Jones · 1996
59. Al–Mg (aluminum–magnesium)10.1361/105497198770341815 ↗
60. Calculations of electron inelastic mean free paths. II. Data for 27 elements over the 50–2000eV range10.1002/sia.740171304 ↗
61. Hartree–Slater subshell photoionization cross-sections at 1254 and 1487eV10.1016/0368-2048(76)80015-1 ↗
62. XPS study of the major minerals in bauxite: Gibbsite, bayerite and (pseudo-)boehmite10.1016/j.jcis.2005.09.054 ↗
63. Oxidation of magnesium10.1002/sia.1346 ↗
64. Implications of specimen preparation and of surface contamination for the measurement of the grain boundary carbon concentration of steels using X-ray microanalysis in an UHV FESTEM10.1002/(SICI)1096-9918(200001)29:1<23::AID-SIA689>3.0.CO;2-Y ↗
65. Atomic weights of the elements: review 2000 (IUPAC technical report)10.1351/pac200375060683 ↗
66. The potential–pH diagram of the magnesium–water system10.1016/S0022-0728(74)80298-6 ↗
67. Potentiostatic study of the magnesium electrode in aqueous solution10.1016/S0022-0728(70)80201-7 ↗
68. An XPS investigation of the oxidation/corrosion of melt-spun Mg10.1016/S0169-4332(99)00593-0 ↗
69. X-ray photoelectron spectroscopic studies of PbO surfaces bombarded with He+, Ne+, Ar+, Xe+ and Kr+10.1016/0039-6028(76)90390-3 ↗
70. Hoffmann · 1983 · 141
71. The initial interaction of water vapour with Mg–Al alloy surfaces at room temperature10.1016/0039-6028(94)90003-5 ↗
72. Interaction of hydrogen with the [beta]-Al3Mg2 complex metallic alloy: experimental reliability of theoretical predictions10.1016/j.jallcom.2008.05.029 ↗
73. Hydrogen absorption properties of the -Mg17Al12 phase and its Al-richer domain10.1016/j.jallcom.2006.12.055 ↗
74. Structure catalysis and atomic reactions on the nano-scale: a systematic approach to metal hydrides for hydrogen storage10.1007/s003390100783 ↗
75. Hydriding behavior of Mg–Al and leached Mg–Al compounds prepared by high-energy ball-milling10.1016/S0925-8388(99)00612-X ↗
76. Fabrication of nanoporous palladium by dealloying and its thermal coarsening10.1016/j.jallcom.2008.12.078 ↗
77. Preparation of nanoporous Ni and Ni–Cu by dealloying of rolled Ni–Mn and Ni–Cu–Mn alloys, Journal of Alloys and Compounds10.1016/j.jallcom.2009.06.031 ↗