journal article·2018-07

Effect of surface abrasion on pitting corrosion of Al-Li alloy

Jianhua Liu, Kuo Zhao, Mei Yu, Songmei Li

Corrosion Science· Volume 138
Publisher page

Abstract

Abstract The effects of surface abrasion on microstructure and pitting corrosion of 2297 Al-Li alloy were investigated. Statistical analysis reveals that surface abrasion alters surface roughness and induces partial dissolution of intermetallic particles. A smoother surface finish reduces the population density and the average size of AlCuMnFe particles, due to enhanced dissolution of AlCuMnFe particles. All abraded samples undergo pitting corrosion, and surface layer dissolution (except pitting) is not observed. Smoother surface has lower pitting susceptibility and better corrosion resistance than the rougher surface. The intermetallic particles significantly affect pitting corrosion of 2297 Al-Li alloy, while surface roughness has small influence.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Modelling of anisotropy for Al-Li 2099 T83 extrusions and effect of precipitate density10.1016/j.msea.2016.07.081 ↗
2. The passive film characteristics of several plastic deformation 2099 Al-Li alloy10.1016/j.jallcom.2015.12.051 ↗
3. Effect of precipitates on mechanical properties of AA219510.1016/j.jallcom.2016.01.229 ↗
4. Microstructures and properties of 2099 Al-Li alloy10.1016/j.matchar.2013.07.015 ↗
5. Influence of Mg and Li content on the microstructure evolution of AlCuLi alloys during long-term ageing10.1016/j.actamat.2016.09.036 ↗
6. Effect of aging treatment on the exfoliation corrosion and stress corrosion cracking behaviors of 2195 Al-Li alloy10.1016/j.matdes.2014.11.007 ↗
7. Localised corrosion in AA 2099-T83 aluminium-lithium alloy: the role of grain orientation10.1016/j.corsci.2016.02.018 ↗
8. SVET, SKP and EIS study of the corrosion behaviour of High strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
9. Identification of the metallurgical parameters explaining the corrosion susceptibility in a 2050 aluminium alloy10.1016/j.corsci.2015.10.020 ↗
10. Metastable pitting characteristics of aluminium alloys measured using current transients during potentiostatic polarisation10.1016/j.electacta.2012.01.090 ↗
11. The effect of chromate on the pitting susceptibility of AA7075-T651 studied using potentiostatic transients10.1016/j.corsci.2014.01.012 ↗
12. Pitting corrosion of naturally aged AA 7075 aluminum alloys with bimodal grain size10.1016/j.corsci.2016.09.013 ↗
13. Origins of Pitting Corrosion10.1179/147842204225016859 ↗
14. New processes for passive metal surfaces
15. Erosion-Corrosion of stainless steel under impingement by a fluid jet10.1016/j.corsci.2006.05.012 ↗
16. Effect of altered surface layer on localized corrosion of aluminum alloy 202410.1149/2.1541706jes ↗
17. Effect of surface roughness on breakdown behavior of Al-Zn-Mg-Cu alloy10.1149/2.1131409jes ↗
18. Near-Surface deformed layers on rolled aluminum alloys10.1007/s11661-010-0538-2 ↗
19. Influence of heat treatment and surface conditioning on filiform corrosion of aluminium alloys AA3005 and AA575410.1016/S0010-938X(01)00019-1 ↗
20. Characterization of electrochemically active surface layers on rolled commercial alloys AA8006 and AA5182 aluminum10.1149/1.1417554 ↗
21. Electrochemical behavior of the active surface layer on rolled aluminum alloy sheet10.1149/1.1635828 ↗
22. Effect of surface machining on the corrosion behaviour of 316 austenitic stainless steel in simulated PWR Water10.1016/j.corsci.2017.06.019 ↗
23. Sequence of corrosion attack of machining induced flow zone produced on some Al alloys that leads to Rapid intergranular penetration10.1179/mst.1998.14.2.151 ↗
24. Surface integrity analysis on high speed end milling of 7075 aluminum alloy10.4028/www.scientific.net/AMR.426.321 ↗
25. Microstructure evolution in abrasion-induced surface layer on an Al-Zn-Mg-Cu alloy10.1016/j.matchar.2014.10.009 ↗
26. On the first breakdown in AA7075-T610.1016/j.corsci.2007.02.001 ↗
27. The corrosion behaviour of machined AA7150-T651 aluminium alloy10.1016/j.corsci.2017.07.008 ↗
28. Correlations between intergranular stress corrosion cracking, grain-boundary microchemistry, and grain-boundary electrochemistry for Al–Zn–Mg–Cu alloys10.1016/j.corsci.2010.08.024 ↗
29. Effect of heat treatments on the tensile strength and SCC-resistance of AA7050 in an alkaline saline solution10.1016/j.corsci.2005.11.009 ↗
30. Localized corrosion of a 2219 aluminium alloy exposed to a 3.5% NaCl solution10.1016/j.corsci.2010.04.035 ↗
31. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
32. corrosion of AA2024-T3 part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
33. Quantifying the strain-induced dissolution of precipitates in Al alloy microstructures using nuclear magnetic resonance10.1016/j.actamat.2009.07.060 ↗
34. Formation of nanograined structure and decomposition of supersaturated solid solution during High pressure torsion of Al–Zn and Al–Mg alloys10.1016/j.actamat.2004.06.006 ↗
35. Cyclic hardening and softening of Al-2.9% Cu-2.2% Mg-0.6% Mn alloy10.1007/BF01151848 ↗
36. Strain-Induced dissolution of Cu-Mg co-clusters and dynamic recrystallization near a fatigue crack tip of an underaged Al-Cu-Mg alloy during cyclic loading at ambient temperature10.1016/j.scriptamat.2011.03.012 ↗
37. The effect of quench rate and overageing temper on the corrosion behaviour of AA705010.1016/j.corsci.2013.10.010 ↗
38. Mechanistic aspects of electrochemical corrosion of aluminum alloy in ethylene glycol-water solution10.1016/j.electacta.2008.06.043 ↗
39. Investigation of erosion–corrosion of 3003 aluminum alloy in ethylene glycol–water solution by impingement jet system10.1016/j.corsci.2008.10.026 ↗
40. Impedance studies of the passive film on aluminium10.1016/j.corsci.2005.05.058 ↗
41. Combined Anodic/Cathodic transient currents within nucleating pits on Al-Fe alloy surfaces10.1016/j.corsci.2010.11.008 ↗
42. Detection and analysis of anodic current transients associated with nanoscale β-Phase precipitates on an Al–Mg microelectrode10.1016/j.corsci.2015.03.001 ↗
43. Determining the probability of stable pit initiation on aluminium alloys using potentiostatic electrochemical measurements10.1016/j.corsci.2004.09.021 ↗
44. Nucleation of corrosion pits on stainless steel10.1080/09500839208229274 ↗
45. Aspects of the effects of electrolyte composition on the occurrence of metastable pitting on stainless steel10.1016/0010-938X(94)90041-8 ↗
46. The aspect ratio of surface grooves and metastable pitting of stainless steel10.1016/S0010-938X(01)00039-7 ↗
47. Surface roughness and the metastable pitting of stainless steel in chloride solutions10.5006/1.3293603 ↗
48. Surface roughness and the corrosion resistance of 21Cr ferritic stainless steel10.1016/j.corsci.2012.06.031 ↗
49. Corrosion behaviour and mechanism of New aerospace Al-Zn-Mg alloy friction stir welded joints and the effects of secondary Al3ScxZr1-x nanoparticles10.1016/j.corsci.2014.10.036 ↗
50. Intergranular corrosion of spark plasma sintering assembled bimodal grain sized AA7075 aluminum alloys10.1016/j.corsci.2016.02.034 ↗
51. A study of corrosion and pitting initiation of AA2024-T3 using atomic force microscopy10.1149/1.1471546 ↗
52. The effect of precipitate size on the yield strength-pitting corrosion correlation in Al-Cu-Mg alloys10.1016/j.actamat.2010.07.010 ↗
53. Localized corrosion in AA2099-T83 aluminum–lithium alloy: the role of intermetallic particles10.1016/j.matchemphys.2015.05.037 ↗
54. Continuous and discontinuous localized corrosion of a 2xxx aluminium–copper–lithium alloy in sodium chloride solution10.1016/j.jallcom.2015.10.185 ↗
55. Role of nanostructure in pitting of Al–Cu–Mg alloys10.1016/j.electacta.2010.02.001 ↗
56. Metastable pitting corrosion of stainless steel and the transition of stability
57. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗