journal article·2025-06

New insights from crystallography into the effect of boundaries on hydrogen embrittlement susceptibility of a 1000 MPa grade heavy gauge high-strength low-alloy steel

Rui Zhong, Jingxiao Zhao, Zhenjia Xie, Peng Han, Hua Wang, Jingliang Wang, Chengjia Shang

Corrosion Science· Volume 249
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Hydrogen trapping at dislocations, carbides, copper precipitates and grain boundaries in a dual precipitating low-carbon martensitic steel10.1016/j.scriptamat.2022.114934 ↗
2. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
3. Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels10.1016/j.ijhydene.2011.10.099 ↗
4. Hydrogen embrittlement of hardened low-carbon sheet steel10.2355/isijinternational.50.294 ↗
5. Evaluation of susceptibility of high strength steels to delayed fracture by using cyclic corrosion test and slow strain rate test10.1016/j.corsci.2010.02.005 ↗
6. The nature and consequences of coherent transformations in steel10.2355/isijinternational.43.410 ↗
7. The effect of prior austenite grain size on hydrogen embrittlement of Co-containing 18Ni 300 maraging steel10.1016/j.ijhydene.2019.05.074 ↗
8. Effects of hydrogen pressure and prior austenite grain size on the hydrogen embrittlement characteristics of a press-hardened martensitic steel10.1016/j.ijhydene.2021.05.005 ↗
9. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
10. Influence of band microstructure on carbide precipitation behavior and toughness of 1 GPa-grade ultra-heavy gauge low-alloy steel10.1007/s12613-023-2597-6 ↗
11. Absorption of hydrogen in high-strength low-alloy steel during tensile deformation in gaseous hydrogen10.2355/isijinternational.50.1496 ↗
12. Crystallographic features of lath martensite in low-carbon steel10.1016/j.actamat.2005.11.001 ↗
13. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
14. Strengthening steel by austenite grain refinement
15. The effect of structure on the deformation of as-quenched and tempered martensite in an Fe-0.2 pct C alloy10.1007/BF02644037 ↗
16. Effect of transformation substructure on the strength and toughness of Fe− Mn alloys10.1007/BF03037855 ↗
17. Effect of microstructural refinement on the toughness of low carbon martensitic steel10.1016/j.scriptamat.2007.10.053 ↗
18. New insights from crystallography into the effect of refining prior austenite grain size on transformation phenomenon and consequent mechanical properties of ultra-high strength low alloy steel10.1016/j.msea.2018.12.057 ↗
19. Analysis of impact toughness scatter in simulated coarse-grained HAZ of E550 grade offshore engineering steel from the aspect of crystallographic structure10.1016/j.matchar.2018.03.037 ↗
20. Influence of refined hierarchical martensitic microstructures on yield strength and impact toughness of ultra-high strength stainless steel10.1016/j.jmst.2020.04.001 ↗
21. Stress–strain behavior of ferrite and bainite with nano-precipitation in low carbon steels10.1016/j.actamat.2014.10.010 ↗
22. Microstructure and strength of nickel at large strains10.1016/S1359-6454(00)00082-3 ↗
23. On coherent transformations in steel10.1016/j.actamat.2004.08.011 ↗
24. Effect of boundaries on toughness in high-strength low-alloy steels from the view of crystallographic misorientation10.1016/j.matlet.2019.126841 ↗
25. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
26. Distribution feature of specific misorientation angle in a bainitic steel10.1016/j.matchar.2021.110874 ↗
27. New insights from crystallography into the effect of Ni content on ductile-brittle transition temperature of 1000 MPa grade high-strength low-alloy steel10.1016/j.jmrt.2024.09.072 ↗
28. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
29. Machine learning guided automatic recognition of crystal boundaries in bainitic/martensitic alloy and relationship between boundary types and ductile-to-brittle transition behavior10.1016/j.jmst.2020.12.024 ↗
30. Grain boundaries and interfaces in slip transfer10.1016/j.cossms.2014.05.003 ↗
31. Characterization of the stretch flangeabitity of high-strength bainitic steel: the significance of variant pairs
32. Effect of double-quenching on the hardness and toughness of a wear-resistant steel
33. Hydrogen embrittlement behavior of 13Cr-5Ni-2Mo supermartensitic stainless steel10.1016/j.corsci.2020.109046 ↗
34. Influence of vanadium on the hydrogen embrittlement of aluminized ultra-high strength press hardening steel10.1016/j.msea.2018.08.027 ↗
35. Effect of plastic deformation on hydrogen diffusion behavior of martensitic steel in hydrogen absorption environment10.2320/matertrans.M2019042 ↗
36. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
37. A combined thermal desorption spectroscopy and internal friction study on the interaction of hydrogen with microstructural defects and the influence of carbon distribution10.1016/j.actamat.2022.118374 ↗
38. Effects of transformation temperature on variant pairing of bainitic ferrite in low carbon steel10.1016/j.actamat.2011.12.018 ↗
39. On estimation of a probability density function and mode10.1214/aoms/1177704472 ↗
40. Multiple slip in bicrystal deformation10.1016/0001-6160(57)90044-5 ↗
41. Grain boundary effect on diffusion of hydrogen in pure aluminum10.2320/matertrans1989.32.1109 ↗
42. Effect of microstructure refinement on hydrogen-induced damage behavior of low alloy high strength steel for flexible riser10.1016/j.msea.2019.138278 ↗
43. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure10.1080/09500830500482316 ↗
44. Analysis of hydrogen atom transport in a two-phase alloy10.1016/0921-5093(94)90488-X ↗
45. Study on hydrogen segregation at individual grain boundaries in pure nickel by scanning Kelvin probe force microscopy10.1016/j.matlet.2021.130528 ↗
46. Experimental study on the diffusion of hydrogen along individual grain boundaries in nickel10.1016/j.elecom.2018.05.012 ↗
47. First-principles study on the interaction of H interstitials with grain boundaries in α- and γ-Fe10.1103/PhysRevB.84.144121 ↗
48. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
49. Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel10.1016/j.corsci.2018.04.041 ↗
50. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗
51. Dual role of nanosized NbC precipitates in hydrogen embrittlement susceptibility of lath martensitic steel10.1016/j.corsci.2019.108345 ↗
52. Synergistic effects of Ta and Mo on the hydrogen embrittlement resistance in ultra-high strength hot stamping steel10.1016/j.msea.2023.144956 ↗
53. Hydrogen interaction with multiple traps: can it be used to mitigate embrittlement?10.1016/j.ijhydene.2011.05.027 ↗
54. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
55. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
56. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
57. Effect of nano Nb and V carbides on the hydrogen interaction in tempered martensitic steels10.1016/j.ijhydene.2021.10.051 ↗
58. Prior austenite grain size and tempering effects on the dislocation density of low-C Nb–Ti microalloyed lath martensite10.1016/j.scriptamat.2015.05.036 ↗
59. Effect of initial dislocation density on hydrogen accumulation behavior in martensitic steel10.1016/j.scriptamat.2019.11.051 ↗
60. Control of hydrogen-induced failure in metastable austenite by grain size refinement10.1016/j.mtla.2019.100514 ↗