Abstract Passive films play an important role in corrosion and stress corrosion cracking of titanium. Correlation between passive film-induced stress and film mechanical properties on α-Ti in methanol solution with varying water content was investigated. Film-induced stress in the methanol solution was measured by the flow stress differential method, and thin film fracture properties were determined by nanoindentation. For small amounts of water (⩽0.15%), both film-induced tensile stress and film fracture load were higher. However, the film-induced tensile stress and fracture load decreased significantly in more dilute solutions. Thus, water reduces Ti SCC susceptibility in methanol solution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Effect of “pure” methanol on the cracking of titanium10.5006/0010-9312-25.2.87 ↗
2. Stress–corrosion cracking of titanium alloys
3. The stress–corrosion of Ti and Ti-8Al-1Mo-1V in methanol vapour10.1016/S0010-938X(68)80194-5 ↗
4. Stress–corrosion of Ti–8Al–1Mo–1V in methanol+HCl solutions10.1016/0010-938X(69)80006-5 ↗
5. Methanol cracking of Ti-8Al-1Mo-1V10.1016/S0010-938X(70)80014-2 ↗
6. The intergranular stress corrosion cracking of Ti 155 in methanol/HCl at room temperature10.1016/0010-938X(93)90046-J ↗
7. Stress corrosion crack propagation in Ti–13V–11Cr–3Al alloy in methanolic solutions
8. The stress corrosion cracking and hydrogen embrittlement of titanium in methanol–hydrochloric acid solutions10.1016/0010-938X(93)90102-M ↗
9. The stress corrosion cracking and hydrogen embrittlement of titanium in methanol–iodine solutions10.1016/0010-938X(93)90103-N ↗
10. Correlation between passive film-induced stress and stress corrosion cracking of α-Ti in a methanol solution at various potentials10.1016/S0921-5093(02)00529-4 ↗
11. Stress corrosion cracking caused by passive film-induced tensile stress10.5006/1.3294396 ↗
12. Stress corrosion cracking relation with dezincification layer-induced stress10.1007/s11661-001-0221-8 ↗
13. The correspondence between susceptibility to SCC of brass and corrosion-induced tensile stress with various pH values10.1016/S0010-938X(02)00055-0 ↗
14. The in-situ TEM observation of corrosion facilitating dislocation emission, multiplication and motion for brass10.1016/0956-716X(95)90851-A ↗
15. In-situ TEM observation of dissolution-enhanced dislocation emission, motion and the nucleation of SCC for Ti-24Al-11Nb alloy in methanol10.1016/S1359-6462(96)00368-5 ↗
16. In-situ transmission electron microscopic observation of corrosion-enhanced dislocation emission and crack initiation of stress corrosion10.5006/1.3280556 ↗
17. Passivity breakdown and stress corrosion cracking of stainless steel10.1016/j.corsci.2006.05.031 ↗
18. The stress corrosion of ti alloys in methanolic solutions10.1016/S0010-938X(68)80008-3 ↗
19. Passivity breakdown and stress corrosion cracking of α-brass in sodium nitrate solutions10.1016/j.corsci.2010.09.025 ↗
20. Passivity breakdown and stress corrosion cracking of α-brass in sodium nitrite solutions10.1016/j.corsci.2004.08.020 ↗
21. Film breakdown and anodic dissolution during stress corrosion cracking of carbon steel in bioethanol10.1149/1.3269927 ↗
22. Effects of hydrogen and tensile stress on the breakdown of passive films on type 304 stainless steel10.1016/S0013-4686(00)00661-7 ↗
23. Mechanism of pit nucleation by electrical breakdown of the passive film10.1016/S0010-938X(01)00113-5 ↗
24. Pre-strain enhances film rupture to promote SCC of brass in Mattsson’s solution – a proposal for a film-rupture-induced SCC mechanism10.1016/j.corsci.2012.11.043 ↗
25. Thin-film fracture during nanoindentation of a titanium oxide film–titanium system10.1557/JMR.2001.0362 ↗
26. Using nanoindentation techniques for the characterization of coated systems: a critique10.1016/0257-8972(93)90226-E ↗
27. Hardness measurement at penetration depths as small as 20nm10.1080/01418618308234914 ↗
28. In situ imaging of LiN load indents into GaAs10.1557/JMR.1995.2162 ↗
29. Non-linear deformation mechanisms during nanoindentation10.1016/S1359-6454(98)00024-X ↗
30. Continuous microindentation of passivating surfaces10.1557/JMR.1993.0685 ↗
31. Displacement burst and hydrogen effect during loading and holding in nanoindentation of an iron single crystal10.1016/j.scriptamat.2005.06.042 ↗
32. The role of dislocation walls for nanoindentation to shallow depths10.1016/j.ijplas.2008.02.003 ↗
33. Hydrogen effects on dislocation activity in austenitic stainless steel10.1016/j.actamat.2006.02.007 ↗
34. Recent developments in the study of hydrogen embrittlement: hydrogen effect on dislocation nucleation10.1016/j.actamat.2010.05.057 ↗
35. Improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
36. Plastic properties of thin films on substrates as measured by submicron indentation hardness and substrate curvature techniques10.1557/JMR.1986.0845 ↗
37. Structural and mechanical characteristics of anodic oxide films on titanium10.5006/1.3290378 ↗
38. The injection of plasticity by millinewton contacts10.1016/0956-7151(94)00351-H ↗
39. The anodic polarization of titanium in halide solutions10.1016/0010-938X(64)90041-1 ↗
40. Kinetic Monte Carlo simulations of the partial oxidation of methanol on oxygen-covered Cu(110)10.1016/j.susc.2006.06.020 ↗
41. The adsorption of methanol on NiOx/Ni{110}10.1016/0009-2614(94)01270-9 ↗
42. Anodic oxidation of anhydrous methanol10.1149/1.2132939 ↗
43. Some specific features of the catalytic role of UPD foreign metal adatoms and water on the anodic oxidation of absolute methanol on Pt10.1016/0022-0728(87)80255-3 ↗
44. Electrolytic behaviour of non-aqueous systems in methanol10.1016/0013-4686(72)90024-2 ↗
45. The oxidation of metals at high temperatures
46. Stress generation during anodic oxidation of titanium and aluminum10.1016/0010-938X(93)90009-6 ↗
47. A novel method to measure the residual stress in a corrosion film formed on metallic substrates10.1016/j.corsci.2012.11.004 ↗
48. Measurement of thin film mechanical properties using nanoindentation10.1557/S0883769400041634 ↗
49. Indentation induced film fracture in hard film–soft substrate systems10.1023/A:1024979030155 ↗
50. Hydrogen effects on stainless steel passive film fracture studied by nanoindentation10.1016/j.corsci.2011.05.025 ↗
51. Mechanical measurements of passive film fracture on an austenitic stainless steel10.1007/s11661-003-0240-8 ↗
52. Contact stresses between an elastic cylinder and a layered elastic solid10.1115/1.3451940 ↗
53. Barsoum · Fundam. Ceram. · 200310.1887/0750309024 ↗
54. Yield strength predictions from the plastic zone around nanocontacts10.1016/S1359-6454(98)00301-2 ↗
55. The effect of water on passivity and pitting of titanium in solutions of methanol and hydrogen chloride10.1149/1.2408339 ↗
56. Stress–corrosion cracking of Ti-6A1-4V alloy in methanol