Ti-4Al-6Mo-2V-5Cr-2Zr alloy with different microstructures was prepared through two heat treatment processes (STA 1 and STA 2), and its corrosion fatigue behavior in a 3.5 % NaCl solution was investigated. STA 1 forms a hierarchical nanostructure (HN) containing coarse grain boundary α (GB α), primary α (α p ), and nanoscale secondary α (α s ) with significant elemental segregation. In contrast, STA 2 forms a lamellar structure (LM) composed of fine, needle-like α s with uniform element distribution. Results indicate that LM has better corrosion resistance, its passive film resistance (4.328 ×10 6 Ω·cm 2 ) is higher than that of HN (1.101 ×10 6 Ω·cm 2 , 6.9 nm). In a 3.5 % NaCl solution, STA 1 shows significant corrosion fatigue behavior, whereas STA 2 does not exhibit any signs of corrosion fatigue. The deformation in HN mainly occurs within the coarse α phase, and the high dislocation density can lead to localized stress concentrations, thereby damaging the passivation film and initiating corrosion fatigue cracks.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Fatigue and fracture mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. A review on heat treatment efficiency in metastable β titanium alloys: the role of treatment process and parameters10.1016/j.jmrt.2020.10.088 ↗
2. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
3. Review of corrosion fatigue in offshore structures: present status and challenges in the offshore wind sector10.1016/j.rser.2016.02.017 ↗
4. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
5. Trifunctional nanoprecipitates ductilize and toughen a strong laminated metastable titanium alloy10.1038/s41467-023-37155-y ↗
6. Enhanced mechanical properties of Ti-5Al-5Mo-5V-3Cr-1Zr by bimodal lamellar precipitate microstructures via two-step aging10.1016/j.msea.2021.142117 ↗
7. Effect of aging treatment on microstructure and tensile properties of Ti–4Al–6Mo–2V–5Cr–2Zr10.1016/j.jmrt.2022.12.058 ↗
8. Effect of solution treatment and aging on microstructure, tensile properties and creep behavior of a hot-rolled β high strength titanium alloy with a composition of Ti-3.5Al–5Mo–6V–3Cr–2Sn-0.5Fe-0.1B-0.1C10.1016/j.msea.2021.141728 ↗
9. Nb modified Ti-5553 alloy: effects of heating rate on mechanical properties, corrosion behavior, and crystallographic texture10.1016/j.jmrt.2023.02.138 ↗
10. Effect of 0.1wt% Nb on the microstructure and corrosion fatigue performance of high strength steels10.1016/j.corsci.2023.111242 ↗
11. Comparative study on mechanical and corrosion fatigue properties of high-strength bridge steels produced by TMCP and intercritical quenching & tempering process10.1016/j.msea.2022.143771 ↗
12. Experimental investigation on corrosion fatigue crack initiation and growth of heat-treated U75V rail steel10.1016/j.ijfatigue.2023.107973 ↗
13. A critical review on very high cycle corrosion fatigue: mechanisms, methods, materials, and models10.1016/j.jsse.2023.05.002 ↗
14. Unravelling the competitive effect of microstructural features on the fracture toughness and tensile properties of near beta titanium alloys10.1016/j.jmst.2021.04.032 ↗
15. A novel ultra-high strength titanium alloy via hierarchical α/α′ precipitation strengthening10.1016/j.msea.2022.142878 ↗
16. Morphology characteristics of α precipitates related to the crystal defects and the strain accommodation of variant selection in a metastable β titanium alloy10.1016/j.jmst.2021.01.090 ↗
17. Corrosion, fatigue and corrosion fatigue behaviour of metal implant materials, especially titanium alloys10.1016/j.ijfatigue.2009.09.009 ↗
18. Effects of the microstructural characteristics of a metastable β Ti alloy on its corrosion fatigue properties10.1016/j.ijfatigue.2013.04.010 ↗
19. Controlled nanoscale precipitation to enhance the mechanical and biological performances of a metastable β Ti-Nb-Sn alloy for orthopedic applications10.1016/j.matdes.2017.04.014 ↗
20. Effects of microstructure on high-cycle fatigue properties of Ti-4Al-6Mo-2V-5Cr-2Zr alloy10.1016/j.ijfatigue.2024.108223 ↗
21. Influence of microstructure on cyclic deformation response and micromechanics of Ti-55531 alloy10.1016/j.msea.2020.140505 ↗
22. Influence of ω phase precipitation on mechanical performance and corrosion resistance of Ti–Nb–Zr alloy10.1016/j.matdes.2016.09.026 ↗
23. Fatigue properties of a metastable β-type titanium alloy with reversible phase transformation10.1016/j.actbio.2007.09.009 ↗
24. Fatigue and corrosion resistance of low modulus Ti-35Nb-7Zr-5Ta-0.35O beta Ti alloy for orthopedic implant applications
25. The effect of heat treatment on corrosion behavior of selective laser melted Ti-5Al-5Mo-5V-3Cr-1Zr alloy10.1016/j.surfcoat.2022.128743 ↗
26. Designing the microstructural constituents of an additively manufactured near β Ti alloy for an enhanced mechanical and corrosion response10.1016/j.matdes.2022.110618 ↗
27. Effect of microstructure characteristic on mechanical properties and corrosion behavior of new high strength Ti-1300 beta titanium alloy10.1016/j.jallcom.2017.08.239 ↗
28. Effect of annealing temperatures on microstructural evolution and corrosion behavior of Ti-Mo titanium alloy in hydrochloric acid10.1016/j.corsci.2021.110079 ↗
29. Corrosion behavior of Ti–39Nb alloy for dentistry
30. Annealed microstructure dependent corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy10.1016/j.jmst.2020.05.058 ↗
31. A low-cost hierarchical nanostructured beta-titanium alloy with high strength10.1038/ncomms11176 ↗
32. A novel high-strength β-Ti alloy with hierarchical distribution of α-phase: the superior combination of strength and ductility10.1016/j.matdes.2019.107640 ↗
33. Very high-cycle fatigue behaviour of Ti-6Al-4V alloy under corrosive environment10.1111/ffe.12735 ↗
34. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
35. The role of multiple interfaces induced by hierarchical phase structures in the corrosion of low-cost titanium alloys10.1016/j.matdes.2024.113521 ↗
36. Effect of Zr content on microstructure, mechanical properties and corrosion behaviour in hydrochloric acid for as-cast Ti-Zr alloy10.1016/j.corsci.2024.112136 ↗
37. Metastable pitting corrosion behavior of laser powder bed fusion produced Ti-6Al-4V in Hank’s solution10.1016/j.corsci.2022.110333 ↗
38. The effect of fluoride ion on crevice corrosion of Ti-6Al-3Nb-2Zr-1Mo alloy in NaCl solution10.1016/j.corsci.2025.113287 ↗
39. Study on corrosion fatigue of Ti-6Al-4V alloy under hydrostatic pressure environment in 3.5 % NaCl solution10.1016/j.corsci.2025.112950 ↗
40. Corrosion and passivation behavior of laser powder bed fusion produced Ti-6Al-4V in static/dynamic NaCl solutions with different concentrations10.1016/j.corsci.2021.109728 ↗
41. Great enhancement in corrosion resistance of Ti alloy by Mo element regulating β grain boundary and microstructure10.1016/j.corsci.2025.113237 ↗
42. Understanding the effect of fluoride on corrosion behavior of pure titanium in different acids10.1016/j.corsci.2021.109812 ↗
43. Fluoride induced corrosion of Ti-45Nb in sulfuric acid solutions10.1016/j.corsci.2020.109232 ↗
44. Characterization of corrosion properties, structure and chemistry of titanium-implanted TiNi shape memory alloy10.1016/j.matchar.2023.113457 ↗
45. The anisotropy of corrosion and passive behavior in selective laser melted Ti-5Al-5Mo-5V-3Cr-1Zr alloy10.1016/j.matchar.2023.112954 ↗
46. Comparison of the corrosion behavior of pure titanium and its alloys in fluoride-containing sulfuric acid10.1016/j.corsci.2015.11.003 ↗
47. Synergistic effects of fluoride and chloride on general corrosion behavior of AISI 316 stainless steel and pure titanium in H2SO4 solutions10.1016/j.corsci.2017.10.028 ↗
48. The corrosion resistance and passive film compositions of 12% Cr and 15% Cr oxide dispersion strengthened steels in nitric acid media10.1016/j.corsci.2013.10.015 ↗
49. Microstructural influences on the high cycle fatigue life dispersion and damage mechanism in a metastable β titanium alloy10.1016/j.jmst.2020.07.018 ↗
50. Micromechanisms of crack initiation of a Ti-8Al-1Mo-1V alloy in the very high cycle fatigue regime10.1016/j.ijfatigue.2021.106314 ↗
51. Corrosion behavior of Ti-Mo alloys cold rolled and heat treated10.1016/j.jallcom.2011.03.045 ↗
52. Effect of surface mechanical attrition treatment on corrosion fatigue behavior of AZ31B magnesium alloy10.1016/j.ijfatigue.2019.06.031 ↗
53. Corrosion fatigue behavior of MRI-compatible Nb-60Ta-2Zr alloy in exposure to simulated physiological solution10.1016/j.ijfatigue.2021.106583 ↗
54. Corrosion fatigue behavior of Fe-16Mn-0.6C-1.68Al twinning-induced plasticity steel in simulated seawater10.1016/j.corsci.2021.109282 ↗
55. Composite structure of α phase in metastable β Ti alloys induced by lattice strain during β to α phase transformation10.1016/j.actamat.2017.04.051 ↗
56. Reply to comments on “composite structure of α phase in metastable β Ti alloys induced by lattice strain during β to α phase transformation” by prof. D. Banerjee10.1016/j.scriptamat.2017.08.010 ↗
57. Heterostructures enhance simultaneously strength and ductility of a commercial titanium alloy10.1016/j.actamat.2023.119182 ↗
58. Tuning the scale of α precipitates in β-titanium alloys for achieving high strength10.1016/j.scriptamat.2018.05.040 ↗
59. Influence of surface roughness on the corrosion behaviour of magnesium alloy10.1016/j.matdes.2010.12.016 ↗
60. Wear and corrosion behaviour of Ti–13Nb–13Zr and Ti–6Al–4V alloys in simulated physiological solution10.1016/j.corsci.2010.11.014 ↗
61. Stress corrosion characteristics of electron beam welded titanium alloys joints in NaCl solution10.1016/j.matchar.2022.112126 ↗
62. Effects of intermittent loading time and stress ratio on dwell fatigue behavior of titanium alloy Ti-6Al-4V ELI used in deep-sea submersibles10.1016/j.jmst.2020.10.063 ↗
63. Effect of annealing on the corrosion-fatigue strength and hot salt corrosion resistance of fine-grained titanium near-α alloy Ti-5Al-2V obtained using Rotary Swaging10.1016/j.jallcom.2024.175612 ↗
64. Micro-mechanisms and modelling of the corrosion fatigue behaviour of a maraging steel10.1016/j.corsci.2023.111769 ↗
65. Comparative study on corrosion fatigue behaviour of high strength low alloy steel and simulated HAZ microstructures in a simulated marine atmosphere10.1016/j.ijfatigue.2020.105666 ↗
66. Corrosion fatigue acoustic emission characteristics and evaluation of friction stir welding joints of AZ31 magnesium alloy in 3.5wt% NaCl solution10.1016/j.jmrt.2023.06.240 ↗