journal article·2021-11

Effect of pre-oxidation on hot corrosion resistance of HR3C stainless steel in sulfate salt with or without Fe2O3

Zheng Yu, Jintao Lu, Minghui Chen, Jinlong Wang, Fuhui Wang

Corrosion Science· Volume 192
Publisher page

Abstract

Abstract HR3C steel exhibits high oxidation resistance in air at 700 °C owing to the formation of a dense chromia scale. In the presence of sulfate salt deposition (Na2SO4:K2SO4 = 1:1), hot corrosion occurs. It leads to the dissolution and re-precipitation of Cr2O3 platelets and severe internal corrosion. Pre-oxidation can notably enhance corrosion resistance with almost no internal corrosion zone. When the deposited sulfate salt contains Fe2O3 (Na2SO4:K2SO4:Fe2O3 = 1:1:1), HR3C steel suffers even severer hot corrosion. Its scale spalls off easily and internal corrosion develops deep into the steel. Meanwhile, pre-oxidation played almost no positive effect on corrosion in sulfate salt containing Fe2O3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Clean coal technology development in China10.1016/j.enpol.2009.06.003 ↗
2. The fossil fuel power plants technology
3. Microstructure and long-term creep properties of 9–12% Cr steels10.1016/j.ijpvp.2007.06.010 ↗
4. Long-term creep deformation characteristics of advanced ferritic steels for USC power plants10.1016/j.ijpvp.2006.09.005 ↗
5. High-efficiency coal-fired power plants development and perspectives10.1016/j.energy.2005.05.025 ↗
6. U.S. program on materials technology for ultra-supercritical coal power plants10.1361/10599490524039 ↗
7. Materials for boilers operating under supercritical steam conditions
8. Investigation on high temperature corrosion characteristic of Super304H, TP347H, and HR3C steel in an ultra‐supercritical coal‐fired boiler10.1002/fuce.202000031 ↗
9. N. Komai, M. Igarashi, Y. Minami, H. Mimura, F. Masuyama, M. Prager, P.R. Boyles, Field test results of newly developed austenitic steels in the eddystone unit no.1 boiler, in : Proceedings of the. Vessel. Pip. Conf. Eighth Int. Conf. Creep Fatigue Elev. Temp. CREEP8, 2007 ASME Press, 2008.10.1115/CREEP2007-26760 ↗
10. Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass10.1016/j.fuel.2013.04.005 ↗
11. Fireside corrosion behaviors of super304H and HR3C in coal ash/gas environment with different SO2 contents at 650 °C10.1007/s11665-017-3051-6 ↗
12. Influence of dissolved oxygen concentration and exposure temperature on the steam oxidation behaviour of HR3C10.1080/1478422X.2019.1611248 ↗
13. Effect of aging process on steam oxidation behaviour of austenitic steels Super 304H and HR3C10.1016/j.ijpvp.2021.104344 ↗
14. Environmental degradation of boiler components
15. Effect of SO2 in flue gas on coal ash hot corrosion of Inconel 740 alloy – a high temperature electrochemical sensor study10.1016/j.corsci.2013.07.012 ↗
16. Rates of fireside corrosion of superheater and reheater tubes: making sense of available data10.1179/1878641314Y.0000000030 ↗
17. New austenitic steels for the advanced USC power plants
18. Fireside corrosion of superheater materials in coal/biomass co-fired advanced power plants10.1007/s11085-013-9394-y ↗
19. Chemical and structural properties of the system Fe2O3-Cr2O310.1007/BF01151237 ↗
20. A theoretical investigation of alpha- Fe2O3-Cr2O3 solid solutions10.1039/B815907F ↗
21. Effects of silicon and water vapour on corrosion of Fe–20Cr and Fe–20Cr–20Ni alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
22. Mechanochemical-molten salt synthesis of α-Al2O3 platelets10.1016/j.ceramint.2015.03.095 ↗
23. Size control of α-Al2O3 platelets synthesized in molten Na2SO4 flux10.1111/j.1551-2916.2004.00533.x ↗
24. Synthesis of α-alumina platelets from γ-alumina with and without microwaves10.1016/j.msea.2007.02.041 ↗
25. Growth habit of rutile and α-Al2O3 crystals10.1016/S0022-0248(99)00419-4 ↗
26. Effects of sulphate deposits on corrosion behaviour of Ni-base alloys in wet CO2 gas at 750 °C10.1016/j.corsci.2020.109227 ↗
27. Investigation into the failure mechanism of chromia scale thermally grown on an austenitic stainless steel in pure steam10.1016/j.corsci.2016.03.021 ↗
28. Hot corrosion behaviour of a Ni+CrAlYSiN composite coating in Na2SO4–25wt% NaCl melt10.1016/j.apsusc.2012.12.012 ↗
29. Hot corrosion behaviour of plasma sprayed YSZ/Al2O3 dispersed NiCrAlY coatings on Inconel-718 superalloy10.1016/j.surfcoat.2009.07.026 ↗
30. Impacts of applied stresses on high temperature corrosion behavior of HR3C in molten salt10.1007/s11085-014-9522-3 ↗
31. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
32. Effects of chromate and vanadate anions on the hot corrosion of preoxidized Ni by a thin fused Na2SO4 film at 900 °C10.1149/1.2086437 ↗
33. Hot corrosion of materials: fundamental studies10.1007/BF03222665 ↗
34. Hot corrosion of materials: a fluxing mechanism10.1016/S0010-938X(01)00057-9 ↗
35. Chapter 8 - corrosion by sulphur
36. Thermodynamic analysis of phase diagrams of binary solid solutions of ascending and minimum types: Na2SO4-Ag2SO4, Ag2SO4-K2SO4, Na2SO4-K2SO410.1139/v89-223 ↗
37. Crystal chemistry of the system Na2SO4-K2SO4-K2CrO4-Na2CrO4 of the glaserite phase
38. Growth mechanism of Cr2O3 scales: oxygen and chromium diffusion, oxidation kinetics and effect of yttrium10.1016/0921-5093(96)10173-8 ↗
39. Understanding of failure mechanisms of the oxide scales formed on nanocrystalline coatings with different Al content during cyclic oxidation10.1016/j.actamat.2020.116576 ↗