Abstract
Corrosion behaviour of low alloy (LASS) and plain carbon (PCSS) structural steels exposed in different types of climatic conditions and nature of rust formed on their surfaces have been studied after 2 years of exposures. The test sites were chosen to represent four types of environments who strongly influence the corrosion of metals and alloys. They include (a) humid–saline, (b) humid–saline–urban (c) humid–industrial and (d) plain dry–urban environments. Mass loss, Raman spectroscopy, scanning electron microscopy and electrochemical impedance spectroscopic studies have been performed to study the corrosion behaviour and characterise the nature of rusts formed on these steels. Mass loss measurement technique has been used to determine the loss of thickness of steels during their atmospheric and salt spray exposures. Results indicate that the corrosion rate of steels is strongly influenced by the climatic conditions prevailing at the exposure sites. The presence of SO2 and salinity in the environments change the structure and protective properties of rust formed on the steels’ surface. Electrochemical impedance and cyclic polarisation studies of the steels in simulated environments have been performed to understand the mechanism of corrosion in different climatic conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Schwartz · Werkst. Korros. · 1965 · 16 · 20810.1002/maco.19650160306 ↗
2. Keller · Werkst. Korros. · 1971 · 20 · 3210.1002/maco.19710220105 ↗
3. Hiller · Werkst. Korros. · 1966 · 17 · 94310.1002/maco.19660171104 ↗
4. Yamashita · Corros. Eng. · 2000 · 49 · 15910.3323/jcorr1991.49.159 ↗
5. Dillmann · Corros. Sci. · 2004 · 46 · 140110.1016/j.corsci.2003.09.027 ↗
6. Yamashita · Corros. Sci. · 1994 · 36 · 28310.1016/0010-938X(94)90158-9 ↗
7. Antunes · Materia · 2003 · 8 · 27
8. Ambler · J. Appl. Chem. · 1955 · 5 · 43710.1002/jctb.5010050901 ↗
9. Moszynki · J. Appl. Chem. · 1960 · 10 · 211
10. Practice for conducting atmospheric corrosion metals, ASTM G50-76, 1992.
11. Practice for preparing, cleaning and evaluating corrosion test specimens, ASTMG1-90.
12. Singh · Corrosion · 2003 · 59 · 102910.5006/1.3277521 ↗
13. Practice for operating salt spray (fog) testing, ASTM B-117, 1994.
14. M.W. Simpson, Van der Linde, D.C. Mc Cune, H.E. Townsend, Licence plate cosmetic corrosion tests automotive coated steel sheet CORROSION/98, paper No. 553 (Houston, TX, NACE 1998).
15. Singh · Corrosion · 2002 · 58 · 97110.5006/1.3280787 ↗
16. Fujiwara · Corros. Eng. · 2000 · 49 · 14510.3323/jcorr1991.49.88 ↗
17. Yamashita · Corros. Eng. · 2000 · 49 · 133
18. Ishikawa · Corros. Sci. · 1999 · 41 · 166510.1016/S0010-938X(98)00198-X ↗
19. Misawa · Corros. Sci. · 1974 · 4 · 27910.1016/S0010-938X(74)80037-5 ↗
20. Niemegeers · J. Appl. Phys. · 1997 · 81 · 288110.1063/1.363946 ↗
21. Boucherit · Mater. Sci. Forum · 1989 · 51 · 44
22. Materials Transactions10.2320/matertrans1989.37.67 ↗
23. Thierry · J. Electrochem. Soc. · 1988 · 135 · 30510.1149/1.2095605 ↗
24. Thibean · Appl. Spectrosc. · 1978 · 32 · 53210.1366/000370278774330739 ↗
25. Dunnwald · Corros. Sci. · 1989 · 29 · 116710.1016/0010-938X(89)90052-8 ↗
26. Ohtsuka · Corrosion · 1986 · 42 · 47610.5006/1.3583054 ↗
27. J. Gui, T.M. Devine, in: Proceedings of the 12th International Corrosion Congress, NACE International, Houston, 1993, p. 2052.
28. Kustova · Puyz. Chem. Min. · 1992 · 18 · 379
29. Cornell · 1996
30. Wang · Mater. Chem. Phys. · 1997 · 47 · 110.1016/S0254-0584(97)80019-3 ↗
31. Zhang · Mater. Protect. · 1989 · 22 · 15
32. Rosenfel’D · Dokl. Akad. Nauk. SSSR · 1954 · 99 · 137
33. Armstrong · J. Electroanal. Chem. · 1976 · 72 · 25710.1016/S0022-0728(76)80312-9 ↗
34. Schwertmann · Clay. Clay Mater. · 1983 · 31 · 27710.1346/CCMN.1983.0310405 ↗