Effect of hydration pretreatment on tunnel etching behaviour of aluminium foil
Source abstract
Abstract
Abstract Hydrous oxide films composed of pseudoboehmite and bayerite have been fabricated on the aluminium surfaces by hydration pretreatment in hot distilled water and ammonia solutions, respectively. After tunnel etching process, the specific surface area of aluminium foil with hydrous oxide film has been significantly improved, compared with that of aluminium foil with thermal oxide film. This effect can be attributed to the role that the hydrous oxide film contains plenty of water channels and defects, which allow the chloride ions to penetrate the film easily and reach the aluminium surface, thereby nucleating pits.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Concrete Corrosion and Durability · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. A scanning electron microscope study of etched aluminium foil for electrolytic capacitors10.1149/1.2408057 ↗
2. Electrochemical tunnel etching of aluminium10.1149/1.2115495 ↗
3. Growth rates of aluminium etch tunnels10.1149/1.2095356 ↗
4. Electrochemical study of the pitting corrosion of aluminium and its alloys—II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion10.1016/0013-4686(89)87119-1 ↗
5. Aluminium pitting in chloride solutions: morphology and pit growth kinetics10.1016/0010-938X(90)90112-I ↗
6. Insight into the pitting corrosion behavior of aluminium alloys10.1016/0010-938X(92)90130-U ↗
7. The electrode kinetics of pit initiation on aluminium10.1016/0010-938X(94)00150-5 ↗
8. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
9. Pit nucleation behavior of aluminium foil for electrolytic capacitors during early stage of DC etching10.1016/S0010-938X(99)00117-1 ↗
10. Sequence of steps in the pitting of aluminium by chloride ions10.1016/S0010-938X(02)00231-7 ↗
11. Electrochemical etching model in aluminium foil for capacitor10.1016/j.corsci.2008.02.017 ↗
12. Initial stages of the anodic etching of aluminium foils studied by atomic force microscopy10.1016/S0010-938X(98)00128-0 ↗
13. On the fundamentals of etching high-purity aluminium foil for capacitor use10.1149/1.2425556 ↗
14. Electrochemical aspects of pitting corrosion10.1016/S0010-938X(67)80073-8 ↗
15. Improvements in the etching of hard aluminium electrolytic capacitor foil10.1149/1.2407775 ↗
16. Tunnel morphology in anodic etching of aluminium10.1149/1.1837730 ↗
17. The effect of aluminium ions on the DC etching of aluminium foil10.1023/B:JACH.0000040439.04947.f4 ↗
18. Tunnel morphology of aluminium foil etched by a two-step DC etching method10.1016/j.corsci.2008.08.031 ↗
19. Effect of sulfuric acid on pit propagation behaviour of aluminium under AC etch process10.1016/j.corsci.2009.06.021 ↗
20. Effect of trace elements on electrochemical properties and corrosion of aluminium alloy AA310210.1016/S0010-938X(03)00159-8 ↗
21. Growth of etch pits formed during sonoelectrochemical etching of aluminium10.1016/j.electacta.2005.04.070 ↗
22. Effects of pretreatment on the aluminium etch pit formation10.1016/j.corsci.2009.02.028 ↗
23. The formation of films on aluminium immersed in water10.1039/tf9575301020 ↗
24. An investigation of the reaction between aluminium and water10.1149/1.2427728 ↗
25. Aluminium+water reaction10.1039/tf9696500561 ↗
26. The growth of hydrous oxide films on aluminium10.1149/1.2401679 ↗
27. Boiling water and silane pre-treatment of aluminium alloys for durable adhesive bonding10.1016/S0143-7496(99)00046-9 ↗
28. Superhydrophobic property of the perpendicular nanosheet film by hot water treatment of the metal aluminium10.2109/jcersj2.117.299 ↗
29. Anodizing of aluminium covered with hydroxide I. Formation of hydroxide and composite oxide films10.4139/sfj1950.38.67 ↗
30. On the mechanism of the passivity of aluminium and aluminium alloys10.1016/0022-0728(93)80186-L ↗
31. The protectivity of aluminium and its alloys with transition metals10.1007/s100080050019 ↗
32. Some physical and dielectric properties of hydrous alumina films10.1149/1.2407826 ↗
33. Wernick · 1972
34. Metal dissolution kinetics in aluminium etch tunnels10.1149/1.1394026 ↗
35. Activation of aluminium in chloride containing solutions10.1016/0013-4686(88)85035-7 ↗
36. Salt film formation during corrosion of aluminium10.1016/0013-4686(84)87098-X ↗
37. Kinetic model for aluminium dissolution in corrosion pits10.1149/1.1635386 ↗
38. Pit growth behaviour of aluminium under galvanostatic control10.1016/j.corsci.2011.06.024 ↗
39. Observations of the early stages of the pitting corrosion of aluminium10.1149/1.2085577 ↗
40. Initial events during the passivation of rapidly dissolving aluminium surfaces10.1149/1.2054945 ↗
41. Evolution of microscopic surface topography during passivation of aluminium10.1149/1.2054944 ↗
42. Evaluation of corrosion behavior of coated metals with AC impedance measurements10.5006/1.3577363 ↗