Abstract In this study, the corrosion susceptibility of aluminum matrix composites reinforced with artificially oxidized SiO 2 and sol–gel Fe/TiO 2 coated silicon carbide particles (SiC p ) has been investigated. Corrosion behavior of the composites, fabricated by the liquid metal infiltration technique, was established in chloride containing alkaline environments by cyclic polarization (CP) and electrochemical impedance spectroscopy (EIS) techniques. It has been found that, sol–gel coating of SiC particles with Fe/TiO 2 has a detrimental effect on the corrosion characteristics of A380–SiC metal matrix composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Control of the interface in SiC/Al composites10.1016/S1359-6462(99)00227-4 ↗
2. Review reinforcement coatings and interfaces in aluminum metal matrix composites10.1023/A:1004674822751 ↗
3. The melt structural characteristics concerning the interfacial reaction in SiC(p)/Al composites10.1007/PL00021120 ↗
4. SEM observations on the porosity activities during corrosion of Al-Si-Mg/SiCp metal matrix composites
5. Control of the interface reaction between silicon carbide and iron10.1016/S0254-0584(02)00521-7 ↗
6. Microstructure and interface structure studies of SiCp-reinforced Al (6061) metal-matrix composites10.1016/S0921-5093(98)00686-8 ↗
7. M.S. Yaghmaee, G. Kaptay, On the stability range of SiC in ternary liquid Al-Si-Mg alloy, Materials Worlds Proceeding of Hungarian Materials Science Society II (2001) 3, http://materialworld.fw.hu.
8. The influence of silicon carbide reinforcement on the pitting behaviour of aluminium10.1016/0010-938X(96)00098-4 ↗
9. Effect of limited matrix-reinforcement interfacial reactions on enhancing the mechanical properties of aluminum-silicon carbide composites10.1016/S1359-6454(01)00221-X ↗
10. Effect of reinforcement coating on corrosion behavior of AA6061/SiC/20p composite in high relative humidity environments10.5006/1.3287828 ↗
11. Sol-gel coatings as active barriers to protect ceramic reinforcement in aluminum matrix composites10.1002/adem.200300519 ↗
12. Preparation and characterization of TiO2 thin films by the sol-gel process10.1023/A:1012989012840 ↗
13. Production of Al based composite reinforced with SnO2 coated SiC particles10.1177/0021998307082174 ↗
14. Oxidation barriers on SiC particles for use in aluminium matrix composites manufactured by casting route: mechanisms of interfacial protection10.1023/A:1020612819045 ↗
15. An investigation of the effect of SiC reinforcement coating on the wettability of Al/SiC system10.1177/0021998308092217 ↗
16. Squeeze casting of Ni coated SiC particle reinforced Al based composite10.1177/0021998308092195 ↗
17. The effect of ceramic coatings on the wettability of Al-SiC composites
18. A comparison of aluminium-based metal-matrix composites reinforced with coated and uncoated particulate silicon carbide10.1016/S0266-3538(99)00151-7 ↗
19. Corrosion of metal matrix composites
20. Lucas · 1993
21. Corrosion of aluminum and aluminum alloys
22. Shreir · 1979
23. Corrosion susceptibilities of Al–Cu/TiC MMCs fabricated by conventional hot pressing
24. Corrosion behavior of an artificially aged (T6) Al–Si–Mg based metal matrix composite10.1177/0021998305057434 ↗
25. The effect of SiCp reinforcement on the corrosion behaviour of Al based metal matrix composites10.1515/CORRREV.2006.24.1-2.27 ↗
26. The mechanical response of Al–Si–Mg/SiCp composite: influence of porosity10.1016/S0921-5093(03)00461-1 ↗
27. Interfacial reaction of Al matrix composites reinforced with TiO2-coated SiC particles during remelting10.1016/j.matlet.2003.10.024 ↗
28. Dynamics of light-induced water cleavage in colloidal systems10.1021/ja00406a004 ↗
29. AR coatings applied from metal-organic derived liquid precursors10.1364/AO.18.003133 ↗
30. Microstructures and age hardenabilitiy of Al–5%Si–0.2%Mg based composites reinforced with particulate SiC10.1016/S0266-3538(97)00049-3 ↗
31. Bonding and wetting in non-reactive metal:SiC systems: weak or strong interfaces?10.1016/S0921-5093(99)00274-9 ↗
32. The incorporation of ceramic particles in molten aluminium and the relationship to contact angle data10.1016/S0921-5093(98)01102-2 ↗
33. ASTM G1-90, ASTM International, USA, 15–20, 03.02, 2001.
34. ASTM G5-94, ASTM International, USA, 58–69, 03.02, 2001.
35. On the behaviour of enhanced mixing in metalceramic interfaces10.1016/S0168-583X(00)00577-2 ↗
36. Thermal properties of materials
37. Tafel’s law in pitting corrosion and crevice corrosion susceptibility10.1016/j.corsci.2005.05.043 ↗