journal article·2006-03

Tensile Deformation Behaviour of the Titanium Alloy with Hard Elastic Coating

W. Ziaja, J. Sieniawski

Advanced Engineering Materials· Volume 8· Issue 3
Publisher page

Abstract

Various surface engineering techniques are used to modify the surface layer of the Ti alloys to improve their tribological properties. The life of the coating can be increased by introducing intermediate hardened surface layer reducing plastic deformation of substrate material. In this paper, the tensile behaviour of Ti alloy with hard elastic coating was investigated to enable tailoring the resistance to plastic deformation and increase load bearing capacity and fatigue resistance.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Mechanical stress and fatigue analysis · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. 10.1016/S0921-5093(98)00841-710.1016/S0921-5093(98)00841-7 ↗
2. 10.1016/S0257-8972(03)00429-810.1016/S0257-8972(03)00429-8 ↗
3. 10.1016/S0301-679X(98)00015-210.1016/S0301-679X(98)00015-2 ↗
4. 10.1016/S0142-1123(01)00015-910.1016/S0142-1123(01)00015-9 ↗
5. 10.1016/j.ijfatigue.2003.08.00910.1016/j.ijfatigue.2003.08.009 ↗
6. 10.1016/S0257-8972(99)00005-510.1016/S0257-8972(99)00005-5 ↗
7. 10.1016/j.surfcoat.2003.10.09010.1016/j.surfcoat.2003.10.090 ↗
8. ADINA – Theory and Modeling Guide. ADINA R&D Inc. Watertown MA 2004.
9. 10.1016/j.cma.2004.02.01510.1016/j.cma.2004.02.015 ↗
10. 10.1016/S0142-1123(01)00150-510.1016/S0142-1123(01)00150-5 ↗
11. 10.1016/0040-6090(95)06990-910.1016/0040-6090(95)06990-9 ↗
12. 10.1016/0040-6090(95)06921-610.1016/0040-6090(95)06921-6 ↗
13. 10.1016/S0040-6090(96)09029-310.1016/S0040-6090(96)09029-3 ↗