journal article·2022-12

Laser Cladding Fe/FeCr Coatings on Continuous Casting Cu Mold

Ma Zichao, Shen Yijie, Lou Hanyu, Liu Xinying, Gao Mingyu, Guan Weimian, Fang Youtong, Liu Jiabin, Dong Weiping

Advanced Engineering Materials· Volume 24· Issue 12
Publisher page

Abstract

The crystallizer is the key component controlling the solidification process and is mainly made of pure Cu. The poor wear resistance and oxidation resistance of pure Cu limit the working life of the Cu crystallizer. Herein, Fe/FeCr coatings are designed and successfully fabricated on the Cu substrate by laser cladding technique. The composition, microstructure, mechanical, and thermal properties of the Cu–Fe/FeCr composite are investigated. The coating is composed of a body‐centered cubic Fe–Cr alloy phase. The grains on the surface are equiaxed grains with an average diameter of 2 μm. The coating exhibits a tensile strength 3 times of Cu substrate and well elongation thanks to the fine‐grain structure. The interface between coating and substrate is metallic bonding and possesses a shear strength of as high as 200 MPa. The coating shows obvious advantages in wear resistance and antioxidation at high temperatures in comparison to Cu substrate. The laser cladding Cu–Fe/FeCr composite is promising to prolong crystallizer life for continuous casting.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering Zhejiang University Hangzhou 310027 China

College of Engineering Zhejiang Normal University Jinhua 321004 China

College of Electrical Engineering Zhejiang University Hangzhou 310027 China

Key Laboratory of Urban Rail Transit Intelligent Operation and Maintenance Technology & Equipment of Zhejiang Province Zhejiang Normal University Jinhua 321004 China

Funding

National Natural Science Foundation of China

References (27)

Show source-provided references
1. 10.1016/j.engfailanal.2013.11.00410.1016/j.engfailanal.2013.11.004 ↗
2. 10.1002/srin.20170031210.1002/srin.201700312 ↗
3. 10.1007/s00339-022-05274-w10.1007/s00339-022-05274-w ↗
4. 10.1007/s11665-020-05376-710.1007/s11665-020-05376-7 ↗
5. 10.3365/KJMM.2020.58.4.24710.3365/KJMM.2020.58.4.247 ↗
6. Gao M. · Metals · 2021 · 31 · 1121
7. 10.1016/j.surfcoat.2019.12533110.1016/j.surfcoat.2019.125331 ↗
8. 10.1016/j.jmrt.2020.07.01010.1016/j.jmrt.2020.07.010 ↗
9. 10.1016/j.apsusc.2011.09.10110.1016/j.apsusc.2011.09.101 ↗
10. Zhang J. · Mater. Rev. · 2014 · 28 · 68
11. Dobrzanski L. A. · Mater. Perform. Charact. · 2019 · 8 · 109110.1520/MPC20190203 ↗
12. Wang R. · Mater. Rev. · 2021 · 35 · 19142
13. 10.3390/pr906099310.3390/pr9060993 ↗
14. 10.3390/ma1002016010.3390/ma10020160 ↗
15. 10.1557/jmr.2019.5710.1557/jmr.2019.57 ↗
16. 10.1016/j.surfcoat.2013.05.03610.1016/j.surfcoat.2013.05.036 ↗
17. 10.1007/s11085-010-9215-510.1007/s11085-010-9215-5 ↗
18. 10.1080/21663831.2021.196852410.1080/21663831.2021.1968524 ↗
19. 10.1016/j.ijleo.2019.16331610.1016/j.ijleo.2019.163316 ↗
20. 10.1007/s10765-022-02991-510.1007/s10765-022-02991-5 ↗
21. Shao T. M. · Acta Metall. Sin. · 2001 · 37 · 1040
22. Gao Y. · Hot Working Technol. · 2017 · 46 · 246
23. 10.1016/j.jallcom.2021.15913410.1016/j.jallcom.2021.159134 ↗
24. 10.1016/j.msea.2020.13893710.1016/j.msea.2020.138937 ↗
25. 10.1063/1.172144810.1063/1.1721448 ↗
26. 10.1016/j.surfcoat.2008.06.16310.1016/j.surfcoat.2008.06.163 ↗
27. 10.1016/j.jallcom.2020.15840510.1016/j.jallcom.2020.158405 ↗