Low‐Temperature and High‐Strain Rate Superplastic Zirconia
Source abstract
Abstract
A superplastic ceramic with a strain rate comparable to metals based on 3% Y2O3‐doped tetragonal zirconia (3YTZ) was synthesized at relatively low temperature, based on the doping with MgO and TiO2. The desirable material properties result from both a refined preparation procedure for the zirconia, and from enhanced cation lattice diffusion due to the MgO and TiO2 doping.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 10.1111/j.1551-2916.1986.tb00026.x10.1111/j.1551-2916.1986.tb00026.x ↗
2. Wakai F. · Jpn. J. Appl. Phys. · 1989 · 2 · 57
3. 10.1016/0956-7151(90)90185-J10.1016/0956-7151(90)90185-J ↗
4. 10.1016/0956-7151(94)00307-410.1016/0956-7151(94)00307-4 ↗
5. 10.1016/0956-7151(94)00320-H10.1016/0956-7151(94)00320-H ↗
6. 10.1016/S1359-6454(97)00251-610.1016/S1359-6454(97)00251-6 ↗
7. 10.1111/j.1151-2916.1998.tb02695.x10.1111/j.1151-2916.1998.tb02695.x ↗
8. 10.2320/matertrans1989.39.110810.2320/matertrans1989.39.1108 ↗
9. 10.1246/nikkashi.1999.49710.1246/nikkashi.1999.497 ↗
10. 10.1038/3509502510.1038/35095025 ↗
11. 10.1246/bcsj.55.42010.1246/bcsj.55.420 ↗
12. 10.4028/www.scientific.net/MSF.304-306.45110.4028/www.scientific.net/MSF.304-306.451 ↗
13. 10.1111/j.1151-2916.1989.tb05945.x10.1111/j.1151-2916.1989.tb05945.x ↗
14. 10.1111/j.1151-2916.2001.tb00973.x10.1111/j.1151-2916.2001.tb00973.x ↗
15. 10.1111/j.1151-2916.1972.tb11224.x10.1111/j.1151-2916.1972.tb11224.x ↗
16. 10.1111/j.1151-2916.1991.tb06808.x10.1111/j.1151-2916.1991.tb06808.x ↗
17. 10.1016/S1359-6454(01)00407-410.1016/S1359-6454(01)00407-4 ↗