High-temperature corrosion resistance of SiO 2 -forming materials

Kazuya Kurokawa, Toto Sudiro, Tomonori Sano, Shoji Kyo, Osamu Ishibashi, Masaharu Nakamori

Corrosion Reviews· Volume 36· Issue 1
Publisher page

Abstract

Abstract An increasing demand for electricity and preserving the environment has become a great driving force for the development of advanced boilers for coal-fired plants to improve their plant efficiency by raising the operating temperature. To achieve this purpose, the development of materials that possess a high mechanical strength and excellent resistance against corrosion at high temperatures is required. Considering such situation, the high-temperature corrosion behavior of SiO 2 -forming materials such as CrSi 2 -Ni and CoNiCrAlY-Si alloys in atmospheres containing NaCl and Na 2 SO 4 is introduced. The SiO 2 scale plays a significant role in suppressing the inward diffusion of sulfur and chlorine, resulting in the remarkable suppression of the formation of sulfide and chloride at the scale/substrate interface and inside of the substrate. Based on such results, it is emphasized that SiO 2 -forming materials show outstanding corrosion resistance against atmospheres containing NaCl and Na 2 SO 4 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · nanoparticles nucleation surface interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Institute of Tomakomai College , Tomakomai 059-1275 , Japan

Research Center for Physics , Indonesian Institute of Sciences , Tangerang Selatan 15310 , Indonesia

Mitsubishi Heavy Industry Ltd. , Takasago 676-8686 , Japan

Kansai Electric Co., Inc. , Amagasaki 661-0974 , Japan

Osaka Fuji Corporation , Takaishi 592-0001 , Japan

High Temperature Corrosion and Protection Technosearch Co., Ltd. , Takasago 676-0082 , Japan

References (36)

Show source-provided references
1. Bender R, Schütze M. The role of alloying elements in commercial alloys for corrosion resistance in oxidizing-chloridizing atmospheres. Part I: Literature evaluation and thermodynamic calculations on phase stabilities. Mater Corros 2003; 54: 567–586.10.1002/maco.200390129 ↗
2. Cawley JD, Boyce RS. A solution of the diffusion equation for double oxidation in dry oxygen including lazy exchange between network and interstitial oxygen. Philos Mag A 1988; 58: 589–601.10.1080/01418618808209939 ↗
3. Glushko PI, Postogvard GI, Pugachev NS, Dudnik SF, Podtykan VP. Structure of scale on molybdenum disilicide. Zashchita Metallov (Engl Trans) 1977; 13: 222–224.
4. Goebel JA, Pettit FS. Na2SO4-induced accelerated oxidation (hot corrosion) of nickel. Metall Trans 1970; 1: 1943–1954.10.1007/BF02642794 ↗
5. Goebel JA, Pettit FS, Goward GW. Mechanisms for the hot corrosion of nickel-base alloys. Metall Trans 1973; 4: 261–278.10.1007/BF02649626 ↗
6. Grabke HJ. High temperature corrosion in complex, multi-reactant gaseous environments. In: Norton JF, editor. High temperature materials corrosion in coal gasification atmospheres. London: Elsevier Applied Science Publishers Ltd., 1984: 59–82.
7. Hashimoto T, Tanaka Y, Hokano M, Hirasaki D. Latest technology of highly efficient coal-fired thermal power plants and future prospects. Tech Rev (Mitsubishi Heavy Ind Ltd) 2008; 45: 11–14.
8. Hendry A, Lees DJ. Corrosion of austenitic steels in molten sulphate deposits. Corros Sci 1980; 20: 383–404.10.1016/0010-938X(80)90007-4 ↗
9. International Energy Outlook 2010: DEO/EIA-0484(2010), US Energy Information Administration (EIA), 2010.
10. Kalen JD, Boyce RS, Cawley JD. Oxygen tracer diffusion in vitreous silica. J Am Ceram Soc 1991; 74: 203–209.10.1111/j.1151-2916.1991.tb07318.x ↗
11. Kofstad P. High temperature corrosion. London: Elsevier Applied Science Publishers Ltd., 1988.
12. Lee WH, Lin RY. Oxidation, sulfidation and hot corrosion of intermetallic compound Fe3Al at 605°C and 800°C. Mater Chem Phys 1999; 58: 231–242.10.1016/S0254-0584(98)00280-6 ↗
13. Li YS, Niu Y, Spiegel M. High temperature interaction of Al/Si-modified Fe-Cr alloys with KCl. Corros Sci 2007; 49: 1799–1815.10.1016/j.corsci.2006.10.019 ↗
14. Mayoral MC, Andrés JM, Belzunce J, Higuera V. Study of sulphidation and chlorination on oxidized SS310 and plasma-sprayed Ni-Cr coatings as simulation of hot corrosion in fouling and slagging in combustion. Corros Sci 2006; 48: 1319–1336.10.1016/j.corsci.2005.06.004 ↗
15. Peng X, Liu K, Pan W-P, Riley JT. High-temperature corrosion of A210-C carbon steel in simulated coal-combustion atmospheres. Oxid Met 2003; 60:117–135.10.1023/A:1024621514635 ↗
16. Pettit F. Hot corrosion of metals and alloys. Oxid Met 2011; 76: 1–21.10.1007/s11085-011-9254-6 ↗
17. Rapp RA. Chemistry and electrochemistry of hot corrosion of metals. Mater Sci Eng 1987; 87: 319–327.10.1016/0025-5416(87)90394-6 ↗
18. Rapp RA. Hot corrosion of materials: a fluxing mechanism? Corros Sci 2002; 44: 209–221.10.1016/S0010-938X(01)00057-9 ↗
19. Sano T, Sudiro T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. High-temperature corrosion of Cr-Si-Ni alloys in atmospheres containing salt gases (in Japanese), Report of the 123rd Committee on Heat-Resisting Materials and Alloys, Japan Society for the Promotion of Science 2011; 52: 105–111.
20. Singh H, Puri D, Prakash S. An overview of Na2SO4 and or V2O5 induced hot corrosion of Fe- and Ni based superalloys. Rev Adv Mater Sci 2007; 16: 27–50.
21. Stringer J. Hot corrosion of high-temperature alloys. Annu Rev Mater Sci 1977; 7: 477–509.10.1146/annurev.ms.07.080177.002401 ↗
22. Stroosnijder MF, Quadakkers WJ. Review of high temperature corrosion of metals and alloys in sulphidizing/oxidizing environments I. Corrosion of metals. High Temp Tech 1986a; 4: 83–96.10.1080/02619180.1986.11753321 ↗
23. Stroosnijder MF, Quadakkers WJ. Review of high temperature corrosion of metals and alloys in sulphidizing/oxidizing environments II. Corrosion of alloys. High Temp Tech 1986b; 4: 141–151.10.1080/02619180.1986.11753329 ↗
24. Sudiro T, Sano T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. The influence of Cr addition on the high temperature corrosion of CoNiCrAlY alloys. Adv Appl Plasma Sci 2009; 7: 295–298.
25. Sudiro T, Sano T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K: High temperature corrosion of CoNiCrAlY-Si alloys in an air-Na2SO4-NaCl gas atmosphere. Mater Trans 2011a; 52: 433–438.10.2320/matertrans.MBW201026 ↗
26. Sudiro T, Sano T, Yamauchi A, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. High temperature corrosion behavior of Si-containing alloys in the gas phase of air-(Na2SO4 + 25.7 mass% NaCl). Mater Sci Forum 2011b; 696: 272–277.10.4028/www.scientific.net/MSF.696.272 ↗
27. Sudiro T, SanoT, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. High temperature corrosion of CoNiCrAlY-Si alloys in the liquid phase of Na2SO4-NaCl. Maters Trans 2012a; 53: 920–925.10.2320/matertrans.MBW201105 ↗
28. Sudiro T, Sano T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. The influence of CoNiCrAlY addition on the high temperature corrosion behavior of CrSi2 alloy in an air-Na2SO4-NaCl gas atmosphere. Maters Trans 2012b; 53: 1627–1632.10.2320/matertrans.MAW201210 ↗
29. Sudiro T, Sano T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. High temperature corrosion behavior of Si-containing alloys in the liquid phase of Na2SO4 + 25.7 mass% NaCl. Defect Diffus Forum 2012c; 323–325: 353–358.10.4028/www.scientific.net/DDF.323-325.353 ↗
30. Sudiro T, Sano T, Kyo S, Ishibashi O, Nakamori M, Kurokawa K. A comparative study of high temperature corrosion of Al2O3, SiO2 and Al2O3-SiO2 forming alloys in a Na2SO4-NaCl atmosphere. In: Proc. 8th International Symposium on High-Temperature Corrosion and Protection on Materials; Paper No. 71 in CD-ROM, 2012d: 1–8.10.1007/s11085-013-9398-7 ↗
31. Uusitalo MA, Vuoristo PMJ, Mäntylä TA. High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits. Corros Sci 2004; 46: 1311–1331.10.1016/j.corsci.2003.09.026 ↗
32. Viswanathan R, Bakker W. Materials for ultra supercritical coal power plants—boiler materials: Part 1. J Mater Eng Perform 2001a; 10: 81–95.10.1361/105994901770345394 ↗
33. Viswanathan R, Bakker W. Materials for ultra supercritical coal power plants—turbine materials: Part II. J Mater Eng Perform 2001b; 10: 96–101.10.1361/105994901770345402 ↗
34. Wirkus CD, Wilder DR. High-temperature oxidation of molybdenum disilicide. J Am Ceram Soc 1966; 49: 173–177.10.1111/j.1151-2916.1966.tb13227.x ↗
35. Yamauchi A, Suzuki Y, Sakaguchi N, Watanabe S, Kurokawa K. Microstructure and analysis of oxide scales formed on Cr-Si-Ni compacts in air and H2O-containing atmosphere. Corros Sci 2010; 52: 2098–2103.10.1016/j.corsci.2010.02.007 ↗
36. Young DJ. High temperature oxidation and corrosion of metals. Amsterdam: Elsevier Corrosion Series, 2008.