A Combined Electromagnetic Levitation Melting, Counter‐Gravity Casting, and Mold Preheating Furnace for Producing TiAl Alloy
Source abstract
Abstract
In this work, the authors describe the development of TiAl castings over a wide range of approaches. To overcome casting defects and cracks that appear in TiAl castings, a novel furnace is designed and constructed. The design combines induction skull melting, counter‐gravity casting, and mold heating, which facilitates both filling and microstructure formation via a controllable process. This aim is to improve shaping capabilities and microstructural control for TiAl castings. Melting and casting experiments on TiAl alloys with a nominal composition corresponding to Ti–48Al–2Cr–2Nb (at%) are carried out and discussed. X‐ray examinations indicate that the shaping of the TiAl components dose not contain macro casting defects, validating the advantages of this technique. The results are of interest to researchers devoted to technical innovations and modifications for TiAl casting at the industrial scale.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Energetic Materials and Combustion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University Xi'an 710072 Shaanxi China
Funding
National Natural Science Foundation of China · Aeronautical Science Foundation of China
References (30)
Show source-provided references
1. 10.1016/j.pnsc.2016.01.01410.1016/j.pnsc.2016.01.014 ↗
2. 10.1002/adem.20160073510.1002/adem.201600735 ↗
3. 10.1016/j.intermet.2005.10.01910.1016/j.intermet.2005.10.019 ↗
4. 10.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO;2-U10.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO;2-U ↗
5. 10.1016/j.paerosci.2012.04.00110.1016/j.paerosci.2012.04.001 ↗
6. 10.1016/j.pmatsci.2016.01.00110.1016/j.pmatsci.2016.01.001 ↗
7. 10.1016/j.intermet.2006.01.06410.1016/j.intermet.2006.01.064 ↗
8. 10.1016/j.intermet.2012.06.01210.1016/j.intermet.2012.06.012 ↗
9. 10.1002/adem.20080016410.1002/adem.200800164 ↗
10. Structural Aluminides for Elevated Temperatures(Eds: Y.W. Kim D. Morris R. Yang C. Leyens) TMS New Orleans Louisiana USA 2008.
11. 10.1016/j.intermet.2004.07.00710.1016/j.intermet.2004.07.007 ↗
12. 10.1002/adem.20120023110.1002/adem.201200231 ↗
13. 10.1179/02670830010150896410.1179/026708300101508964 ↗
14. Tetsui T. · Intermetallics · 2005 · 13 · 91710.1016/j.intermet.2004.12.012 ↗
15. 10.1002/adem.20031055910.1002/adem.200310559 ↗
16. 10.1016/j.matdes.2014.12.00610.1016/j.matdes.2014.12.006 ↗
17. 10.1016/j.actamat.2009.11.03210.1016/j.actamat.2009.11.032 ↗
18. Su Y. Q. · J. Alloys Compd · 2002 · 334 · 26110.1016/S0925-8388(01)01766-2 ↗
19. Godfrey B. · Mater. Sci. Eng. A · 1999 · 266 · 11510.1016/S0921-5093(99)00038-6 ↗
20. 10.1016/S0966-9795(98)00036-310.1016/S0966-9795(98)00036-3 ↗
21. 10.1016/S0921-5093(01)01584-210.1016/S0921-5093(01)01584-2 ↗
22. 10.1016/j.intermet.2010.11.02210.1016/j.intermet.2010.11.022 ↗
23. Gombert D. · Nucl. Technol · 2003 · 141 · 30110.13182/NT03-A3368 ↗
24. 10.1016/j.apm.2006.03.00310.1016/j.apm.2006.03.003 ↗
25. Campbell J. · 2015 · 82110.1016/B978-0-444-63509-9.00016-9 ↗
26. Shendye S. B. · Trans. Am. Foundry Soc · 2009 · 117 · 305
27. 10.1016/j.intermet.2015.03.01510.1016/j.intermet.2015.03.015 ↗
28. 10.1007/s11661-017-4209-410.1007/s11661-017-4209-4 ↗
29. 10.1016/S1359-6454(97)00127-410.1016/S1359-6454(97)00127-4 ↗
30. Greenberg B. A. · Intermetallics · 2000 · 8 · 84510.1016/S0966-9795(00)00008-X ↗