Microstructure Characterization and Mechanical Properties of Linear Friction Welded Ti‐6Al‐4V Alloy
Source abstract
Abstract
In this work, Ti-6Al-4V alloy was jointed by linear friction welding (LFW). A sound weld of thickness about 65–115 μm was obtained under the present processing parameters. The weld consisted of a superfine α + β microstructure, which is associated with the quick heating and cooling processes involved in LFW. This superfine microstructure contributes to the higher hardnesses of weld (422 ± 11Hv0.2) than that of parent Ti-6Al-4V (302 ± 20 Hv0.2). The tensile properties of weld are comparable to or higher than those of parent Ti-6Al-4V.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
2. 10.1016/j.scriptamat.2004.11.00910.1016/j.scriptamat.2004.11.009 ↗
3. P. Threadgill Linear Friction Weld.TWI Knowledge Summary The Welding Institute UK Available online at http://eurostir.co.uk/j32k/protected/band_3/ksplt001. html.
4. 10.1016/S0043-1648(98)00145-810.1016/S0043-1648(98)00145-8 ↗
5. 10.1016/S0921-5093(99)00449-910.1016/S0921-5093(99)00449-9 ↗
6. 10.1016/S0921-5093(00)01036-410.1016/S0921-5093(00)01036-4 ↗
7. 10.1007/s11661-005-0335-510.1007/s11661-005-0335-5 ↗
8. Ma T. J. · Rare Met. Mater. Eng. · 2006 · 35 · 233
9. Z. H. Cheng Titanium and Its Alloy Chemical Industry Press Beijing 2005.