Production of High Purity Magnesium Alloys by Melt Purification with Zr
Source abstract
Abstract
Abstract The efficacy of Zr in removing Fe from molten Mg‐X binary alloys was studied experimentally and using calculated phase diagrams. Zr is effective in reducing the Fe content from the Mg melt for Mg‐X binary alloys, X = Y, Si, Sn, Ca, Sr, Ce, Gd, Nd, Li, La, Mn, and Zn. Purification occurs by the precipitation from the melt of Fe rich precipitates, and the settling of the precipitates to the bottom of the melt. Any desired Fe content down to 1 ppm can be achieved by appropriate melt treatment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. 10.1016/j.corsci.2011.06.03010.1016/j.corsci.2011.06.030 ↗
2. 10.1016/j.mseb.2010.12.01710.1016/j.mseb.2010.12.017 ↗
3. 10.1533/9780857091413.2.11710.1533/9780857091413.2.117 ↗
4. 10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
5. 10.1002/adem.20031040510.1002/adem.200310405 ↗
6. 10.1002/adem.20060022110.1002/adem.200600221 ↗
7. 10.1016/j.corsci.2011.09.00410.1016/j.corsci.2011.09.004 ↗
8. 10.1016/j.corsci.2011.10.01410.1016/j.corsci.2011.10.014 ↗
9. T.Marker in:The sixth triennial International Fire and Cabin Safety Research Conference Atlantic City 2010 http://www.fire.tc.faa.gov/2010Conference/conference.asp.
10. T.Marker in:International aircraft materials fire test working group meeting Bremen 2010 http://www.fire.tc.faa.gov/meetings/meetings.asp.
11. 10.4028/www.scientific.net/MSF.419-422.69710.4028/www.scientific.net/MSF.419-422.697 ↗
12. 10.1016/j.corsci.2008.12.01510.1016/j.corsci.2008.12.015 ↗
13. 10.1016/j.msea.2003.08.06010.1016/j.msea.2003.08.060 ↗
14. 10.1016/S1471-5317(02)00008-110.1016/S1471-5317(02)00008-1 ↗
15. 10.1179/imr.1993.38.3.13810.1179/imr.1993.38.3.138 ↗
16. Froats A. · 1987
17. 10.1016/j.corsci.2007.11.00510.1016/j.corsci.2007.11.005 ↗
18. 10.1016/j.electacta.2008.06.00110.1016/j.electacta.2008.06.001 ↗
19. 10.1016/j.corsci.2008.03.00310.1016/j.corsci.2008.03.003 ↗
20. 10.1016/S1003-6326(09)60284-310.1016/S1003-6326(09)60284-3 ↗
21. 10.1016/j.msea.2003.11.01710.1016/j.msea.2003.11.017 ↗
22. 10.1016/S1003-6326(09)60275-210.1016/S1003-6326(09)60275-2 ↗
23. Emley E. F. · 1966
24. 10.1016/j.jallcom.2009.02.07310.1016/j.jallcom.2009.02.073 ↗
25. 10.1016/j.msea.2008.12.00410.1016/j.msea.2008.12.004 ↗
26. 10.5006/1.358315110.5006/1.3583151 ↗
27. Roberts C. S. · 1960
28. 10.1179/02670830422501231410.1179/026708304225012314 ↗
29. Hildebrand Z. · 2004 · 241
30. 10.1016/j.scriptamat.2005.11.00210.1016/j.scriptamat.2005.11.002 ↗
31. 10.1179/02670830322501084910.1179/026708303225010849 ↗
32. Qian M. · 2003 · 209
33. Qian M. · 2003 · 215
34. 10.1016/S1471-5317(01)00009-810.1016/S1471-5317(01)00009-8 ↗
35. 10.1002/adem.20070015710.1002/adem.200700157 ↗
36. 10.1179/136404607X24056210.1179/136404607X240562 ↗
37. 10.1007/s11661-005-0030-610.1007/s11661-005-0030-6 ↗
38. Prasad A. · Flammability of Mg‐X Binary Alloys · 2012
39. http://www.computherm.com/pandat.html.
40. Zhixia Q. · Corrosion of a Mg planar flow casting containing 20 ppm Fe · 2012
41. 10.1016/j.corsci.2010.03.00210.1016/j.corsci.2010.03.002 ↗
42. 10.1002/zaac.1960303050310.1002/zaac.19603030503 ↗