Abstract
Abstract Maximizing lithium (Li) utilization is crucial for enhancing the long‐term stability of Li‐based batteries. In anode‐free Li batteries (AFLBs), although the initial formation of solid electrolyte interphase (SEI) is beneficial on limiting further reaction between Li and electrolyte, large volume change of Li metal anode (LMA) during cycling often leads to continuous breakdown and re‐formation of SEI and formation of inactive Li, hindering its efficiency. In this study, a novel strategy is presented to protect Li metal by applying a floatable protection layer (FPL) on a copper substrate, enabling large Li particles to be primarily deposited below FPL, but SEI to be primarily formed above FPL. This approach effectively minimizes the direct contact between electrolyte and freshly deposited Li, therefore mitigating the continuous side reactions and early failure of AFLBs. As a result, Li consumption is minimized, and the overall stability of the battery is significantly enhanced. Further development of this approach can also be used to improve the performance of other Li‐based batteries for large‐scale applications.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Energy and Environment Directorate Pacific Northwest National Laboratory Richland WA 99354 USA
Funding
Vehicle Technologies Office · U.S. Department of Energy · Office of Energy Efficiency and Renewable Energy
References (28)
Show source-provided references
1. 10.1016/j.chempr.2018.05.00210.1016/j.chempr.2018.05.002 ↗
2. 10.1038/s41560-024-01624-510.1038/s41560-024-01624-5 ↗
3. 10.1149/1945-7111/abe08910.1149/1945-7111/abe089 ↗
4. 10.1021/acsenergylett.3c0180810.1021/acsenergylett.3c01808 ↗
5. 10.1016/j.ensm.2020.07.00410.1016/j.ensm.2020.07.004 ↗
6. 10.1002/adfm.20160235310.1002/adfm.201602353 ↗
7. 10.1038/s41560-019-0428-910.1038/s41560-019-0428-9 ↗
8. 10.1002/batt.20240050510.1002/batt.202400505 ↗
9. 10.1038/s43246-022-00273-z10.1038/s43246-022-00273-z ↗
10. 10.1016/j.jechem.2024.04.03310.1016/j.jechem.2024.04.033 ↗
11. 10.1149/2.0641814jes10.1149/2.0641814jes ↗
12. 10.1038/s41467-021-21683-610.1038/s41467-021-21683-6 ↗
13. 10.1002/aenm.20170209710.1002/aenm.201702097 ↗
14. 10.1016/j.ensm.2022.10.05210.1016/j.ensm.2022.10.052 ↗
15. 10.1002/adma.20220940410.1002/adma.202209404 ↗
16. 10.1016/j.cej.2024.14954710.1016/j.cej.2024.149547 ↗
17. 10.1016/j.mtener.2022.10119910.1016/j.mtener.2022.101199 ↗
18. 10.1002/adfm.20241164810.1002/adfm.202411648 ↗
19. 10.1021/acsnano.4c0450710.1021/acsnano.4c04507 ↗
20. 10.1016/j.nanoen.2024.10983610.1016/j.nanoen.2024.109836 ↗
21. 10.1038/s41467-023-41778-610.1038/s41467-023-41778-6 ↗
22. 10.1038/s41560-021-00917-310.1038/s41560-021-00917-3 ↗
23. 10.1016/j.matt.2019.05.01610.1016/j.matt.2019.05.016 ↗
24. 10.1038/nnano.2014.15210.1038/nnano.2014.152 ↗
25. 10.1149/1.141494610.1149/1.1414946 ↗
26. 10.1002/batt.20180010910.1002/batt.201800109 ↗
27. 10.1002/adma.20170610210.1002/adma.201706102 ↗
28. 10.1021/acsenergylett.3c0180810.1021/acsenergylett.3c01808 ↗