journal article·2020-09-01

Perspective on “Transgranular Stress Corrosion Cracking of High-Pressure Pipelines in Contact with Solutions of Near Neutral pH,” R.N. Parkins, W.K. Blanchard Jr., B.S. Delanty, Corrosion 50, 5 (1994): p. 394-408

Narasi Sridhar

Corrosion· Volume 76· Issue 9
Publisher page

Abstract

Abstract: This paper provides a perspective on the stress corrosion cracking (SCC) of buried pipelines based on a paper by R.N. Parkins, et al., and associated works. The paper by Parkins, et al., included an identification of factors controlling near-neutral pH SCC (NNPHSCC) and a probabilistic approach to evaluating multiple cracks. Considerable research since the publication of the paper has shed light on the mechanisms of NNPHSCC and the various contributing factors. However, a probabilistic framework advanced by this paper is still a work in progress. This perspective describes the progress that has been made and the gaps still remaining in this area.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Science and Engineering, The Ohio State University, Watts Hall, 2014 College, Columbus, OH 43210-1178

References (38)

Show source-provided references
1. Beavers · Corrosion · 2014 · 70 · 310.5006/0998 ↗
2. “Overview of Intergranular SCC Research Activities,”10.55274/R0010136 ↗
3. Sutcliffe · Corrosion · 1972 · 28 · 31310.5006/0010-9312-28.8.313 ↗
4. Parkins · Corrosion · 1994 · 50 · 39410.5006/1.3294348 ↗
5. Liu · Corros. Sci. · 2012 · 55 · 5410.1016/j.corsci.2011.10.002 ↗
6. Fessler · 1976
7. Parkins · Corrosion · 1987 · 43 · 13010.5006/1.3583125 ↗
8. Parkins · Corrosion · 1988 · 44 · 57210.5006/1.3583979 ↗
9. Parkins · Corrosion · 1990 · 46 · 17810.5006/1.3585089 ↗
10. Parkins · Corrosion · 1990 · 46 · 48510.5006/1.3585136 ↗
11. Parkins · Corrosion · 1993 · 49 · 95110.5006/1.3316023 ↗
12. Leis · Fatig. Fract. Eng. Mater. Struct. · 1998 · 21 · 58310.1046/j.1460-2695.1998.00049.x ↗
13. “Predicting the Growth of Low- and High-pH SCC on Gas Transmission Pipelines Based on Operating Conditions,”
14. “Long-Term Environmental Monitoring of Near-Neutral and High-pH SCC Sites and the Basis of an Improved SCC Site Selection Model,”
15. “Exploratory Study of the Relationship Between History of Pressure Fluctuations and Severity of Near-Neutral-pH Stress-Corrosion-Cracking,”
16. Asher · Corrosion · 2007 · 63 · 93210.5006/1.3278311 ↗
17. Li · Electrochim. Acta · 2007 · 52 · 811110.1016/j.electacta.2007.07.015 ↗
18. “Integrity Management of Stress Corrosion Cracking in Gas Pipeline High Consequence Areas,”
19. “Development of Guidelines for Identification of SCC Sites and Estimation of Re-inspection Intervals for SCC Direct Assessment,”
20. Lu · Corros. Sci. · 2010 · 52 · 178710.1016/j.corsci.2010.02.020 ↗
21. Song · Corrosion · 2010 · 66 · 095004-0110.5006/1.3490309 ↗
22. Zhang · Corros. Sci. · 2010 · 52 · 96010.1016/j.corsci.2009.11.019 ↗
23. Liu · J. Mater. Eng. Perform. · 2011 · 20 · 124210.1007/s11665-010-9770-6 ↗
24. Tang · Corros. Sci. · 2011 · 53 · 292710.1016/j.corsci.2011.05.032 ↗
25. “Investigation on the Dormancy of Stress Corrosion Cracking (SCC) Cracks,”
26. Chen · Corrosion · 2016 · 72 · 96210.5006/1967 ↗
27. Maocheng · Corros. Sci. · 2016 · 110 · 2310.1016/j.corsci.2016.04.006 ↗
28. Eslami · Corros. Sci. · 2011 · 53 · 231810.1016/j.corsci.2011.03.017 ↗
29. Cheng · Int. J. Hydrogen Energy · 2007 · 32 · 126910.1016/j.ijhydene.2006.07.018 ↗
30. Parkins · Corrosion · 2003 · 59 · 25810.5006/1.3277559 ↗
31. Fu · Appl. Mech. Mater. · 2014 · 529 · 11710.4028/www.scientific.net/AMM.529.117 ↗
32. Scully · J. Electrochem. Soc. · 1988 · 135 · 133710.1149/1.2095978 ↗
33. Scully · Corrosion · 1987 · 44 · 17610.5006/1.3583922 ↗
34. Thodla · Corrosion · 2020 · 76 · 29910.5006/3240 ↗
35. Kobayashi · Corrosion · 2018 · 74 · 50910.5006/2669 ↗
36. Yoshino · Corrosion · 1986 · 42 · 22210.5006/1.3586000 ↗
37. “Effect of Ni on Sulfide Stress Corrosion Cracking in Low Alloy Steels,”10.5006/C1986-86167 ↗