Durability degradation of tunnel-lining-shotcrete exposed to nitric acid: Neutralization and nitrate ion migration

Jiabin Wang, Zelong Mi, Ting Zhang, Dongjing Wang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Concrete Corrosion and Durability · Smart Materials for Construction · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Durability of dry-mix shotcrete using supplementary cementitious materials10.1016/j.conbuildmat.2018.09.107 ↗
2. Thomas · 2012
3. Properties of wet-mixed fiber reinforced shotcrete and fiber reinforced concrete with similar composition10.1016/j.cemconres.2004.05.033 ↗
4. Tomas Franzen, K.F. Garshol, N. Tomisawa. Sprayed concrete for final lining: ITA working group report, Tunneling and Underground Space Technology 16(2001) 295-309. DOI: http://dx.doi.org/10.1016/S0886-7798(01)00052-9.10.1016/S0886-7798(01)00052-9 ↗
5. Direct shear behavior of sulfate-exposed shotcrete: Experimental and modelling research10.1016/j.conbuildmat.2019.03.229 ↗
6. Durability of shotcrete for underground support – Review and update10.1016/j.conbuildmat.2018.12.151 ↗
7. SiyueHe
8. Comparative analysis of biogenic and chemical sulfuric acid attack on hardened cement paste using laser ablation-ICP-MS10.1016/j.cemconres.2016.05.003 ↗
9. Elisabeth Müller
10. Advances in concrete materials for sewer systems affected by microbial induced concrete corrosion: A review10.1016/j.watres.2018.01.043 ↗
11. Deterioration of compressive property of concrete under simulated acid rain environment10.1016/j.conbuildmat.2010.04.002 ↗
12. Deterioration mechanism of cementitious materials under acid rain attack10.1016/j.engfailanal.2012.08.007 ↗
13. Effect of acid attack on FRP-to-concrete bonded interfaces10.1016/j.conbuildmat.2017.06.140 ↗
14. Mechanical properties and durability of concrete specimens containing nano silica in sulfuric acid rain condition10.1016/j.conbuildmat.2018.01.137 ↗
15. Differential acid neutralisation analysis10.1016/S0008-8846(99)00127-1 ↗
16. Effect of nanomaterials additives on performance of concrete resistance against magnesium sulfate and acids10.1016/j.conbuildmat.2019.03.099 ↗
17. Microstructure and mechanical properties of accelerated sprayed concrete10.1617/s11527-015-0589-3 ↗
18. JungHeumYeon
19. Durability performance of brine-exposed shotcrete in salt lake environment10.1016/j.conbuildmat.2018.08.139 ↗
20. GB 50086-2015, Technical code for engineering of ground anchorages and shotcrete support, Ministry of Housing and Urban-Rural Development of PRC, 2015. (in Chinese).
21. GB/T 50081-2019, Standard for test methods of concrete physical and mechanical properties, Ministry of Housing and Urban-Rural Development of PRC and State Administration for Market Regulation, 2019. (in Chinese).
22. Mechanical properties, permeability and durability of accelerated shotcrete10.1016/j.conbuildmat.2015.07.148 ↗
23. Ditao Niu, Shaohui Zhang, Yan Wang, Mengshu Hong, Zhaoguang, Li, Effect of temperature on the strength, hydration products and microstructure of shotcrete blended with supplementary cementitious materials, Construction and Building Materials, 2020, 264: 120234. DOI: https://doi.org/10.1016/j.conbuildmat.2020.120234.10.1016/j.conbuildmat.2020.120234 ↗
24. The lamellar double-hydroxide (LDH) compound with composition 3CaO·Al2O3·Ca(NO3)2·10H2O
25. Huang Sijing, Huang Keke, Feng Liwen, Tong Hongpeng, Liu Lihong, Zhang Xuehua. Mass exchanges among feldspar, kaolinite and liilite and their influence on secondary porosity formation in clastic diagenesis – A case study on the Upper Paleozoic, Ordos Bsain and Xujiahe Formation, Western Sichuan Depression, Geochimica 38(5)(2009), 498-506. (in Chinese) DOI: http://dx.doi.org/ 10.19700/j.0379-1726.2009.05.009.
26. Study of deterioration of concrete exposed to different types of sulfate solutions under drying-wetting cycles10.1016/j.conbuildmat.2016.04.094 ↗