Role of CaCO3 in Retarding UV- and Thermally Induced Degradation of PVC Compounds
Source abstract
Abstract
This study provides an in-depth investigation of the influence of calcium carbonate (CaCO3) filler on the mechanical performance and aging resistance of polyvinyl chloride (PVC)-based composites. PVC/CaCO3 composites containing 2.5, 5, and 7.5 wt% of CaCO3 were subjected to accelerated aging under combined ultraviolet (UV) irradiation and thermal stress for up to 1248 h. The key mechanical properties of specimens —tensile strength and elongation at break—were measured before and after aging. Changes in surface morphology, coloration, hydrophobicity, and chemical composition were characterized using scanning electron microscopy (SEM-EDS), X-ray spectroscopy, atomic force microscopy (AFM), contact angle measurements, and carbonyl index calculation to quantify relationships between the structural and physical properties of the specimens and aging conditions. The results reveal a significant correlation between filler content and the mechanical behavior of aged specimens, highlighting the potential of CaCO3 reinforcement not only to improve the retention of mechanical properties but also to increase the service life of PVC-based insulation compounds.
Source: crossref · Quality: baseline
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratoire de Technologies Avancées en Génie Electrique, (LATAGE), Université Mouloud Mammeri de Tizi-Ouzou, BP 17 RP, Tizi-Ouzou 15000, Algeria
Advanced High Voltage Engineering Center, School of Engineering, Cardiff University, Queen’s Buildings, The Parade, Cardiff CF24 3AA, UK
Department of Chemical Engineering, Engineering Faculty, Istanbul University-Cerrahpasa, Istanbul 34320, Turkey
Laboratoire de Physique et Chimie Quantique (LPCQ), Université Mouloud Mammeri de Tizi-Ouzou, BP 17 RP, Tizi-Ouzou 15000, Algeria
References (40)
Show source-provided references
1. Popoola, P.A.I., Ogbonna, V.E., Popoola, O.M., and Ajayi, O.O. (2025). Polymer Micro and Nanocomposites for High Voltage Insulation: Properties and Applications, Elsevier.
2. Factors affecting the ageing of polymer composite: A state of art10.1016/j.polymdegradstab.2024.110670 ↗
3. Clay-reinforced PVC composites and nanocomposites10.1016/j.heliyon.2024.e29196 ↗
4. Ashby, M.F., Shercliff, H., and Cebon, D. (2018). Materials: Engineering, Science, Processing and Design, Butterworth-Heinemann.
5. Gibson, R.F. (2016). Principles of Composite Material Mechanics, CRC Press. [4th ed.].10.1201/b19626 ↗
6. Joint physicochemical effects of UV-B irradiation on microplastics formation: The case of poly(vinyl chloride) and poly(methyl methacrylate)10.1016/j.polymdegradstab.2025.111366 ↗
7. Different photodegradation processes of {PVC} with different average degrees of polymerization10.1002/app.25389 ↗
8. The photodegradation processes and mechanisms of polyvinyl chloride and polyethylene terephthalate microplastic in aquatic environments: Important role of clay minerals10.1016/j.watres.2021.117879 ↗
9. Photodegradation of plasticized poly(vinyl chloride) stabilized by different types of thermal stabilizers10.1002/pen.21868 ↗
10. Maraveas, C., Kyrtopoulos, I.V., Arvanitis, K.G., and Bartzanas, T. (2024). The Aging of Polymers under Electromagnetic Radiation. Polymers, 16.10.3390/polym16050689 ↗
11. Amraoui, S., Hedir, A., Moudoud, M., Haddad, A., Durmus, A., and Clark, D. (2025, January 14–17). Dielectric Properties of PVC/Al2O3 Nanocomposite Under the Influence of Thermal Aging. Proceedings of the 2025 IEEE Conference on Electrical Insulation and Dielectric Phenomena (CEIDP), Manchester, UK.10.1109/CEIDP61707.2025.11218532 ↗
12. Solek, C., Crespo-Sánchez, J., del Toro, S., Ayllón, J., Frigione, M., Camacho, A.M., Rodríguez-Hernández, J., and Rodríguez-Prieto, A. (2026). Degradation and Long-Term Response Evaluation of Polymeric Components Produced by Additive Manufacturing. J. Manuf. Mater. Process., 10.10.3390/jmmp10030102 ↗
13. Effect of The Incorporation of Micro and Nanoparticles of Calcium Carbonate in Poly (Vinyl Chloride) Matrix for Industrial Application10.1590/1980-5373-mr-2018-0870 ↗
14. Assessment of the potential industrial applications of calcium carbonate derived from mineral carbonation of alkaline waste material
15. Amraoui, S., Hedir, A., Moudoud, M., Durmus, A., Rondot, S., Haddad, A.M., and Clark, D. (2025). Assessment of Long-Term Thermal Aging Effects on PVC/Al2O3 Nanocomposites Through Electrical, SEM and FTIR Characterizations. Energies, 18.10.3390/en18226034 ↗
16. Nait Larbi, S., Moudoud, M., Hedir, A., Lamrous, O., Durmus, A., Clark, D., and Slimani, F. (2025). Characterization of PVC/CaCO3 Nanocomposites Aged Under the Combined Effects of Temperature and UV-Radiation. Materials, 18.10.3390/ma18174001 ↗
17. Effect of calcium carbonate particle size and content on the thermal properties of PVC foamed layer used for coated textiles10.55730/1300-0527.3514 ↗
18. Thermal Stabilities of Poly (Vinyl Chloride)/Calcium Carbonate (PVC/CaCO3) Composites10.1080/00222340600962650 ↗
19. The Mechanism for Inorganic Fillers Accelerating and Inhibiting the UV Irradiation Aging Behaviors of Rigid Poly(vinyl chloride)10.1002/app.34396 ↗
20. (2024). Plastics—Methods of Exposure to Laboratory Light Sources—Part 1: General Guidance and Requirements (Standard No. ISO 4892-1:2024).
21. (2023). Standard Practice for Operating Fluorescent Ultraviolet (UV) Lamp Apparatus for Exposure of Nonmetallic Materials (Standard No. ASTM G154-23).
22. (2019). Plastics—Determination of Tensile Properties Part 1: General Principles, Published (Edition 3) (Standard No. ISO 527-1: 2019). Available online: https://www.iso.org/standard/527-1.
23. Recent advances in oxidative degradation of plastics10.1039/D4CS00407H ↗
24. Mechanical Characterization of Polymer Nanocomposite Films: Influence of Force Regimes and Nano Silica Reinforcement10.1002/pc.30072 ↗
25. Li, H., Su, X., Gong, G., Shao, A., and Zheng, Y. (2025). Macro-Microscopic Characterization and Long-Term Performance Prediction of Polyvinyl Chloride Under Hydrothermal Aging Based on Creep Behavior Analysis. Polymers, 17.10.3390/polym17172320 ↗
26. Structural Changes Undergone During Thermal Aging and/or Processing of Unstabilized, Dry-blend and Rigid PVC, Investigated by FTIR-ATR and Curve Fitting10.18280/acsm.430109 ↗
27. Quantifying the impact of surface roughness on contact angle dynamics under varying conditions10.1038/s41598-025-01127-7 ↗
28. Quantifying time-dependent structural and mechanical properties of UV-aged LDPE power cables insulations10.55730/1300-0527.3407 ↗
29. Physical Ageing of Insulating Polystyrene from Dielectric Properties Measurements and Structural Analysis10.1088/2053-1591/ab316f ↗
30. Effects of CaCO3 surface modification and water spraying on the weathering properties of PBAT/CaCO3 films10.1016/j.polymertesting.2021.107334 ↗
31. Effect of filler addition and weathering conditions on the performance of PVC/CaCO3 composites10.1002/pc.23396 ↗
32. Assessment of UV-Aging of Crosslinked Polyethylene Cable Insulation by Electrical Measurements10.1149/2162-8777/ada79e ↗
33. Influence mechanism of mechanical properties and crack formation of CaCO3/PVC composites based on cohesion model10.1016/j.mtcomm.2022.103747 ↗
34. Interfacial structures and mechanical properties of PVC composites reinforced by CaCO3 with different particle sizes and surface treatments10.1002/pi.1932 ↗
35. Biçer, Z., Yaman, B.C., Çeliksöz, Ö., and Tepe, H. (2024). Surface roughness of different types of resin composites after artificial aging procedures: An in vitro study. BMC Oral Health, 24.10.1186/s12903-024-04669-w ↗
36. Ultraviolet radiation aging impact on physicochemical properties of crosslinked polyethylene cable insulation10.1002/app.48575 ↗
37. Partial discharges impact on the electrical properties of low-density polyethylene power cable insulation10.1088/2631-8695/ae7ed0 ↗
38. Temperature Dependence of Degradation of Colored Oxo-Biodegradable Low-Density Polyethylene Films under Accelerated Thermal Aging10.4028/www.scientific.net/MSF.890.82 ↗
39. The effects of unmodified vermiculite on photooxidation of polyamide 11 nanocomposites under accelerated UV test Available to Purchase10.1063/1.5045910 ↗
40. Gardi, S., Giannone, L., Sarti, G., and Sarti, G. (2024). Surface Chalking upon Weathering of Dark-Colored PVC Articles and Relevant Stabilizers. Polymers, 16.10.20944/preprints202403.0319.v1 ↗